S7035 a ni
| Availability: | |
|---|---|
| Quantity: | |
HNBR compound hi rubber material bik a ni a, oil leh ozone resistance a nei a, hydraulic hose siamnaah pawh hman a ni nasa hle. Hydraulic hose hi piping system, liquid pressure transfer nana hman a ni a, industrial equipment, automotive, leh aerospace-ah te hman tlanglawn tak a ni. A hnuaia tarlan te hian hydraulic hose-a HNBR compound hman dan tur chu product characteristics, application fields leh advantages lam aangin kan rawn tarlang dawn a ni.
A hmasa berah chuan HNBR compound te hian oil resistance tha tak an nei a. Hydraulic system-ah chuan hydraulic oil hi hnathawhna atana hman tlanglawn tak a ni a, hydraulic hose erawh chuan pressure sang leh temperature sang tak hnathawhna hmun a tuar a ngai thung. HNBR compound hian oil resistance tha tak a pe a, hydraulic oil nena inzawm hian hun rei tak chhung chu an physical property leh service life te chu an vawng reng thei bawk. Hei hian HNBR compound te hi hydraulic hose siamna atana hmanraw tha ber pakhat a siam a ni.
Pahnihnaah chuan HNBR compound te hian ozone resistance tha tak an nei bawk. Ozone hi boruak tichhetu tlanglawn tak a ni a, awlsam takin rubber materials te chu a upa thei a, a chhe thei bawk. Mahse, HNBR compound te hi ozone attack lakah a tangkai hle a, hydraulic hose te service life pawh a ti rei hle. Hei hian HNBR compound te hi pawn lam boruak leh hnathawhna hmuna ozone concentration sang takah hman lar tak a siam a ni.
HNBR compound hi hmanraw hrang hrangah hman a ni. A hmasa berah chuan industrial equipment-a hydraulic system-ah te hman a ni tlangpui a, chu chu metallurgical equipment, plastic machinery leh machine tools te hi a ni. Heng hmanrua te hi pressure sang leh temperature sang tak hmanga hnathawhna hmuna tuar thei tura mamawh an ni fo a, HNBR compound te hian oil laka invenna leh ozone laka an mamawh chu an phuhruk a ni. Pahnihnaah chuan HNBR compound hi automotive industry-ah pawh hman a ni nasa hle. Automobile siamnaah hian hydraulic hose hi automotive hydraulic system-a fluid pressure thawn chhuahna atana thil pawimawh tak a ni a, chu chu braking system, suspension system leh steering system te hi a ni. HNBR compound te oil leh ozone resistance vang hian automotive hydraulic hose siamna atana hmanraw duh ber pakhat a ni. Hei bakah hian HNBR compound hi aerospace sector-a hydraulic system-ah pawh hman theih a ni a, aircraft leh spacecraft-ah te pawh hman theih a ni.
Hydraulic hose-a HNBR compound hman hian a hnuaia hlawkna te hi a nei a ni. A hmasa berah chuan wear resistance leh heat resistance sang tak a nei a, temperature sang leh pressure sang tak hnathawhna hmunah pawh a physical property leh service life te chu a vawng reng thei bawk. Pahnihnaah chuan HNBR compound hian anti-aging performance tha tak a nei a, ultraviolet rays, oxidation leh ozone erosion te a do thei a, hydraulic hose service life pawh a ti rei thei bawk. Hei bakah hian HNBR compound hian compression set rate hniam tak leh sealing performance tha tak a nei bawk a, hei hian hydraulic system hnathawh dan pangngai a tichiang thei a ni.
A tawi zawngin, HNBR compound hi rubber material bik, oil resistance leh ozone resistance nei angin hydraulic hose siamnaah hman a ni nasa hle. Oil resistance tha tak leh ozone resistance tha tak a neih avangin hydraulic hose siamna atana hmanraw tha ber pawl a ni. Industrial equipment, automotive leh aerospace-ah te chuan HNBR compound te hian hydraulic system te hnathawh dan pangngaia kalpui theih nan pressure sang, temperature sang leh boruak khirh tak tak mamawh a phuhruk a ni.
Tin, HNBR compound te hian chemical resistance tha tak an nei bawk. Acid, alkalis, solvent leh chemical dangte a do thei a, chemical environment hrang hranga hydraulic hose te chu a nghetin a rintlak hle. Hei hian HNBR compound te hi chemical, petroleum leh damdawi siamna lama hydraulic system-ah hman lar tak a siam a ni.
Tin, HNBR compound te hian elasticity leh tensile property tha tak an nei a, pressure sang leh chakna sang tak hnathawhna hmunah pawh an tuar thei bawk. A chakna sang tak leh a chhe thei lo avangin hydraulic hose hian hun rei tak hman leh duty cycle tam tak a tuar thei a, hei hian hydraulic system rintlak leh nghetna a ti sang hle.
Hydraulic hose siamna kawngah pawh HNBR compound hian processing performance tha tak a nei bawk. Hydraulic hose chi hrang hrang leh a lian leh te mamawh ang zela extrusion, calendering leh injection molding hmanga siam theih a ni. Chutih rual chuan HNBR compound te hi thil dang nen pawh inzawmkhawmin hydraulic hose structure complex zawk siam theih a ni bawk.