Khoom Muag Khoom: High-Strength Oil-Resistant Medium-Saturation HNBR Synthetic Rubber
Peb Qhov Nruab Nrab-Saturation HNBR Synthetic Rubber yog tsim los ua kom muaj kev ua tau zoo tshwj xeeb hauv cov roj-tshuaj thiab muaj kev ntxhov siab ntau hauv kev lag luam. Nrog rau 34% acrylonitrile cov ntsiab lus, cov roj hmab hydrogenated nitrile (HNBR) muaj cov roj ua haujlwm zoo dua thaum tswj kev yoog raws thiab ua haujlwm ntev, ua rau nws zoo tagnrho rau cov ntsaws ruaj ruaj, gaskets, thiab cov khoom siv hauv kev ua haujlwm hnyav.
Ntsiab Technical Specifications:
- Cov ntsiab lus Acrylonitrile: 34% - Optimized rau cov roj sib npaug thiab qhov kub thiab txias yooj yim.
- Mooney Viscosity (ML 1 + 4 @ 125 ° C): 70-90 - Ua kom cov txheej txheem zoo heev rau molding thiab extrusion.
- Iodine Absorption Tus nqi: 11-22 - Reflects tswj nruab nrab saturation rau txhim kho tshuaj stability thiab kev laus tsis kam.
- Hardness: Kho tau ntau yam (piv txwv li, 60-90 Shore A) kom tau raws li ntau hom kev thov.
Kev Ua Haujlwm Zoo:
- Superior Roj & Roj Resistance: Nrog rau lub sij hawm raug rau cov roj, roj, thiab hydrocarbon kua (kuaj ib ASTM D471).
- High Tensile Strength: Ua kom muaj kev ntseeg ruaj khov nyob rau hauv cov khoom siv hluav taws xob thiab kev kub ntxhov.
- Thermal Stability: Ua haujlwm zoo hauv qhov kub ntawm -30 ° C txog + 150 ° C (-22 ° F txog + 302 ° F).
- Abrasion Resistance: Zoo tagnrho rau cov ntaub ntawv hnav zoo li cov ntsaws ruaj ruaj thiab cov tshuab hydraulic.
Daim ntawv thov:
- Roj & Roj: Cov ntsaws ruaj ruaj rau cov twj, li qub, thiab cov khoom siv downhole.
- Automotive: Roj system Cheebtsam, O-rings, thiab siv sij hawm.
- Industrial Machinery: Gaskets, hoses, thiab kev cai-moulded qhov chaw rau kev ua tshuaj.
Vim Li Cas Xaiv Peb HNBR?
- Customizable Formulations: Tailor hardness, viscosity, thiab saturation qib rau cov kev xav tau tshwj xeeb.
- Kev Ua Tau Zoo: Ua raws li ISO 9001 thiab ASTM cov qauv.
- Kev Pab Cuam Ntxiv: Txo cov sij hawm poob qis hauv qhov chaw muaj roj tseem ceeb.