| Umubare: | |
Incamake y'ibicuruzwa: Amavuta-Yimbaraga-Zirwanya Hagati-Yuzuye HNBR Synthetic Rubber
Hagati ya Saturation HNBR Synthetic Rubber yakozwe kugirango itange imikorere idasanzwe mumavuta agaragara hamwe ninganda zikomeye cyane. Hamwe na 34% bya acrylonitrile, iyi hydrogène nitrile reberi (HNBR) itanga amavuta arwanya imbaraga mugihe ikomeza guhinduka kandi ikaramba, bigatuma iba nziza kuri kashe, gasketi, nibigize ibintu bikora nabi.
Ibyingenzi byingenzi bya tekiniki:
- Ibirimo Acrylonitrile: 34% - Gukoresha uburyo bwiza bwo kurwanya amavuta hamwe nubushyuhe buke.
- Ubukonje bwa Mooney (ML 1 + 4 @ 125 ° C): 70-90 - Iremeza uburyo bwiza bwo gutunganya no gusohora.
- Agaciro ka Iyode Agaciro: 11-22 - Yerekana ubwuzuzanye buciriritse bugamije kongera imiti no kurwanya gusaza.
- Gukomera: Urwego ruhinduka (urugero, 60-90 Inkombe A) kugirango uhuze ibyifuzo bitandukanye.
Ibyiza byo gukora:
- Kurwanya Amavuta & Ibikomoka kuri peteroli: Irwanya guhura igihe kinini namavuta, amavuta, hamwe na hydrocarubone (byageragejwe kuri ASTM D471).
- Imbaraga Zirenze: Zigumana ubusugire bwimiterere munsi yumutwaro uremereye hamwe nigitutu gikabije.
- Ubushyuhe bwumuriro: Ikora neza mubushyuhe kuva kuri -30 ° C kugeza kuri + 150 ° C (-22 ° F kugeza + 302 ° F).
- Kurwanya Abrasion: Byiza kubikorwa byambara cyane nka kashe izunguruka na sisitemu ya hydraulic.
Porogaramu:
- Amavuta na gaze: Ikidodo cya pompe, valve, nibikoresho byo hasi.
- Imodoka: Ibikoresho bya lisansi, O-impeta, n'umukandara wigihe.
- Imashini zinganda: Igipapuro, amacupa, nibice byabugenewe byo gutunganya imiti.
Kuki Hitamo HNBR?
- Guhindura uburyo bwihariye: Ubudozi bukomeye, ubwiza, nurwego rwuzuye kubyo ukeneye byihariye.
- Ubwiza buhoraho: Bujyanye na ISO 9001 na ASTM.
- Ubuzima Bwagutse bwa Serivisi: Kugabanya igihe cyo kugabanuka mumavuta akomeye yibidukikije.