Princeps Fortitudo oleum repugnans Medium-Saturatio HNBR Saccharum Purgamentum

Product Overview: Princeps Fortitudo Olei Repugnans Medium-Saturationis HNBR Syntheticum Purgamentum

Nostrum Medium-Saturationis HNBR Syntheticum Rubber machinatur ad liberam eximiam observantiam in culturae ambitu oleo exposito et magno vis. Cum contento 34% acrylonitrili, haec hydrogenata globulus nitrile (HNBR) superiori olei resistentiam praebet, flexibilitatem et durabilitatem conservans, id facit specimen sigillis, gaskets et componentibus in conditionibus duris operantis.

Clavis Specificationum technicarum:
- Acrylonitrile Content: 34% - Optimized ad resistentiam olei libratam et flexibilitatem humilis temperaturae.
- Viscositas Mooney (ML 1+4 @125°C): 70-90 - Ensures processabilium excellentium formandi et extrusionis.
- Iodi Absorptionis Value: 11-22 - Medium satietatem reflexum moderatum ad incrementum chemicae stabilitatis et resistentiae senescentes.
- Hardness: Adjustable range (exempli, 60-90 Litus A) ut diversa applicatione occurrat.
 
  • HNBR3418

  • HERCHY

Availability:
Quantitas:

Product Overview


Nostrum Medium-Saturationis HNBR Syntheticum Purgamentum machinatur ad liberam eximiam observantiam in ambitu olei exposito et magno vis industriae. Cum contento 34% acrylonitrili, haec hydrogenata globulus nitrile (HNBR) superiori olei resistentiam praebet, flexibilitatem et durabilitatem conservans, id facit specimen sigillis, gaskets et componentibus in conditionibus duris operantis.


Key Specifications Technical:  

- Acrylonitrile Contentus: 34% - Optimized pro librata olei resistentia et humilis temperatura flexibilitas.

- Viscositas Mooney (ML 1+4 @125°C): 70-90 - Ensures processabilium excellentium formandi et extrusionis.

- Iodi Absorptionis Value: 11-22 - Medium satietatem reflexum moderatum ad incrementum chemicae stabilitatis et resistentiae senescentes.

- Hardness: Adjustable range (exempli, 60-90 Litus A) ut diversa applicatione occurrat.

Commodo euismod:

- Superior Oleum & Fuel Resistentia: Substantia diuturna expositionis oleorum, unctorum, humorum hydrocarbonis (probati per ASTM D471).

- Princeps tensile fortitudo: structuram conservat integritas sub oneribus dynamicis et pressionibus extremis.

- Stabilitas scelerisque: in temperaturis fideliter operatur ab -30°C ad +150°C (-22°F ad +302°F).

- Abrasio Resistentia: Specimen pro applicationibus altum induendi sicut sigilla rotanda et systemata hydraulica.


Applicationes:  

- Oleum & Gas: Sigilla soleatus, valvulae, et instrumentum deorsum.

- Automotiva: Fuel systematis componentium, o-annuli, et cingula leo.

- Machinaria Industrialis: Gaskets, hoses, et custo- mata partes chemicae processus.


Cur elige nostrum HNBR?  

- Formulae Mos: Scissor duritia, viscositas, et saturatio gradus ad certas necessitates.

- Consistent Quality: Compliant with ISO 9001 and ASTM standards.

- Fundo Service Vita: reduces downtime in critica oleum patere ambitibus.


[Continge nos ad technicas notitias et exempla ad probandum effectum in applicatione tua.]
Priora: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.