Agbara-giga Epo-Resistant Alabọde-Saturation HNBR Sintetiki Roba

Akopọ Ọja: Agbara-giga Epo-Resistant Alabọde-Saturation HNBR Sintetiki

Roba Alabọde-Saturation HNBR Sintetiki Rubber ti wa ni iṣelọpọ lati fi iṣẹ iyasọtọ han ni ifihan epo ati awọn agbegbe ile-iṣẹ wahala giga. Pẹlu akoonu 34% acrylonitrile, roba nitrile nitrile hydrogenated (HNBR) nfunni ni aabo epo ti o ga julọ lakoko mimu irọrun ati agbara, ṣiṣe ni apẹrẹ fun awọn edidi, awọn gaskets, ati awọn paati ni awọn ipo iṣẹ lile.

Awọn pato Imọ-ẹrọ bọtini:
- Akoonu Acrylonitrile: 34% - Iṣapeye fun idiwọ epo iwọntunwọnsi ati irọrun iwọn otutu.
- Mooney Viscosity (ML 1 + 4 @ 125 ° C): 70-90 - Ṣe idaniloju ilana ti o dara julọ fun sisọ ati extrusion.
- Iye Gbigba Iodine: 11-22 - Ṣe afihan itẹlọrun alabọde ti iṣakoso fun imudara iduroṣinṣin kemikali ati resistance ti ogbo.
- Lile: Iwọn adijositabulu (fun apẹẹrẹ, 60-90 Shore A) lati pade awọn ibeere ohun elo lọpọlọpọ.
 
  • HNBR3418

  • HERCHY

Wiwa:
Iwọn:

Akopọ ọja: Agbara-giga Epo-Atako Alabọde-Saturation HNBR Sintetiki Roba


Rọba Sintetiki HNBR Alabọde-Saturation wa jẹ iṣẹ-ṣiṣe lati fi iṣẹ ṣiṣe alailẹgbẹ han ni awọn agbegbe ile-iṣẹ ti o ni wahala ti o ga. Pẹlu akoonu 34% acrylonitrile, roba nitrile nitrile hydrogenated (HNBR) nfunni ni aabo epo ti o ga julọ lakoko mimu irọrun ati agbara, ṣiṣe ni apẹrẹ fun awọn edidi, awọn gaskets, ati awọn paati ni awọn ipo iṣẹ lile.


Awọn Pataki Imọ-ẹrọ:  

- Akoonu Acrylonitrile: 34% - Iṣapeye fun idiwọ epo iwọntunwọnsi ati irọrun iwọn otutu.

- Mooney Viscosity (ML 1 + 4 @ 125 ° C): 70-90 - Ṣe idaniloju ilana ti o dara julọ fun sisọ ati extrusion.

- Iye Gbigba Iodine: 11-22 - Ṣe afihan itẹlọrun alabọde ti iṣakoso fun imudara iduroṣinṣin kemikali ati resistance ti ogbo.

- Lile: Iwọn adijositabulu (fun apẹẹrẹ, 60-90 Shore A) lati pade awọn ibeere ohun elo lọpọlọpọ.

Awọn anfani Iṣe:

- Epo ti o ga julọ & Resistance Epo: Ṣe idiwọ ifihan gigun si awọn epo, awọn girisi, ati awọn fifa hydrocarbon (idanwo fun ASTM D471).

- Agbara Fifẹ giga: Ṣetọju iduroṣinṣin igbekalẹ labẹ awọn ẹru agbara ati awọn igara to gaju.

- Iduroṣinṣin Ooru: Ṣiṣẹ ni igbẹkẹle ninu awọn iwọn otutu lati -30°C si +150°C (-22°F si +302°F).

- Abrasion Resistance: Apẹrẹ fun awọn ohun elo aṣọ-giga bi awọn edidi yiyi ati awọn ọna ẹrọ hydraulic.


Awọn ohun elo:  

- Epo & Gaasi: Awọn edidi fun awọn ifasoke, awọn falifu, ati ohun elo isalẹhole.

- Automotive: Awọn paati eto epo, Awọn oruka, ati awọn beliti akoko.

- Ẹrọ Ile-iṣẹ: Awọn gasket, awọn okun, ati awọn ẹya ti a ṣe apẹrẹ fun iṣelọpọ kemikali.


Kini idi ti Yan HNBR wa?  

- Awọn agbekalẹ isọdi: Lile telo, iki, ati awọn ipele itẹlọrun fun awọn iwulo kan pato.

- Didara Didara: Ni ibamu pẹlu ISO 9001 ati awọn iṣedede ASTM.

- Igbesi aye Iṣẹ ti o gbooro: Din akoko idinku ni awọn agbegbe ti o han epo pataki.


[Kan si wa fun awọn iwe data imọ-ẹrọ ati awọn ayẹwo lati ṣe idanwo iṣẹ ṣiṣe ninu ohun elo rẹ.]
Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. Maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.