Njirimara:
Oké okpomọkụ na-eguzogide (-20 Celsius C ka + 250 Celsius C).
Ebe pụrụ iche iguzogide mmanụ, a na-emegharị, sons, acid, na ntọala.
Ike Tenza (10-20 MPA), obere mkpakọ dị ala (<15% na 150 Celsius C / 70H).
Ọkachaala ezumike (UL94 V-0 rating) na Ozone na-eguzogide.
Uru:
A na - agwakọta ya na ịracha (dịka, bisphenol af, peroxide) maka ngwangwa arụmọrụ nke ọma.
Na-ejigide nguzosi ike na gburugburu ime ihe ike.
Usoro akara aka FDA dị maka nri / ahụike.
Ngwa:
Aerospace: Mkpịsị ugodi O.-mgbaaka, akara aka, na diaphragms.
Automage: Turbocharger Gosket, akàrù na-enyefe, na mmanụ mmanụ.
Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na Na)
Njirimara:
Ngugide okpomoku rue 150 Celsius C (Intermitittent + 175 Celsius C).
Izogide mmanụ, amines, na mmiri hydraulic.
Ike tensile di elu (15-35 MPA) na ike ọgwụgwụ iguzogide.
Dị ala na gas.
Uru:
Na-emefu tupu oge nhazi.
Nọgide na-enwe ike na-enweghị ngbanwe n'okpuru mkpughe dị ogologo karịa na mgbasa ozi ọjọọ.
Dị na peroxide- ma ọ bụ sọlfọ gọọmenti.
Ngwa:
Mmanụ & gas: Achịcha Mbupu, apịtị kpụrụ, na ihe ndị dị na-acha.
Automagement: Oge elekere, usoro ihie mgbochi, na Turbocharger Hues.
Industrial: Sydraulic cylinder cylinder na mejupụtara Gearbox.
Njirimara:
Na-agbanwe agbanwe na-agbanwe agbanwe (dị mma karịa EPDM, ihe na-erughị HNBr).
Ọnọdụ okpomọkụ: -40 Celsius C ka + 120 Celsius C.
Nguzogide ala a na-eguzogide (ASTM D5963: 100-200 mM na mfu).
Ezigbo mma na mkpakọ na-esetịpụ nguzogide.
Uru:
Ọnụ ahịa - nke dị irè.
Ọdịnaya ọdịnaya acrnonomiintrile (18-50%) maka nguzozi mmanụ.
Ngwa:
Automative: Mmiri mmanụ, o-yiri akara.
Industrial: na-akpọ eriri eriri, na-ebipụta rollers, na akwara hydraulic.
Onye na-azụ ahịa: latex uwe na akụrụngwa egwuregwu.
Njirimara:
Ọnọdụ ikuku dị mma / elekere 5,000+ na nnwale QV).
Ọnọdụ okpomọkụ: -50 ° C ka + 150 Celsius C.
Ike Dielactric dị elu (20-30 kV / mm) na adịghị ike.
Dị ala gas.
Uru:
Ejiri antioxidants na usoro iwu UV.
Ezigbo oke mkpọtụ (ihe efu: 0.1-0.3).
Ngwa:
Automagive: Ọnụ ụzọ Ahịhịa, HADIATOR HOS, na injin n'Ugwu.
Ewu Ihe: Ime membranes, linters, na gasketk window.
Electrical: Nkpuru agha na eriri nnyefe.
Njirimara:
Ike tensile dị elu (20-60 MPA) na enweghị ike (ihe ruru 800%).
Nguzogide Aaghagide Aation (ASTM D5963: 20-50 mm Ụnwụ).
Ọnọdụ okpomọkụ: -40 Celsius C ka + 100 Celsius C (ruo na + 120 Celsius C na ndị ọrụ ọkụ).
Na-eguzogide mgbaze na hydrolysis.
Uru:
Hazie ihe siri ike (shere a 50-95).
Ọ dị na nkedo, millable, ma ọ bụ nke ahụ.
Ngwa:
Industriallọ ọrụ mmepụta: wiil, rollers, ma na-akpọ eriri eriri.
Automage: nkwusioru bus, ujo, na akpụkpọ ụkwụ CV.
Ahụike: catheters, ihe nkwado Orthopedic, na Shoresthetics.
Njirimara:
Nguzogide ọkụ na-aga n'ihu ruo + 150 Celsius C (Intermitittent + 175 Celsius C).
Ezigbo nguzogide mmiri na-ebugharị akpaka (ATF), mmanụ, na okpomọkụ.
Onerate ozone na iguzogide ihu igwe.
Ike tensile: 7-15 MPA.
Uru:
Na-agwakọta ya na ụdị abụba ma ọ bụ cuatives maka ịgwọ ngwa ngwa.
Na-edobe nguzosi ike na gburugburu atf.
Ngwa:
Automage: Ahịrị na-enye nkwado, o-yiri, na Reephragms.
Ihe eji eme ihe.
Industrial: Bọm Brans maka mgbasa ozi sitere na mmanụ.
Njirimara:
Ọnọdụ okpomọkụ dị obosara (-40 Celsius C ka + 150 Celsius C).
Iguzogide mmanu, glycols, na ihu igwe.
Ike tensile dị elu (10-20 MPA) na mkpakọ setịpụrụ iguzogide.
Dị ala na gas.
Uru:
Na-eme ka okpomọkụ na-eguzogide na mgbanwe.
Na-eguzogide ọgwụ na hydrolysis na ịka nká.
Dị na peroxide- ma ọ bụ sọlfọ gọọmenti.
Ngwa:
Automative: Radiator Hosis, usoro dị mma na-eme, na ikuku na-egwu ikuku.
Industrial: na-ebu eriri maka kemịkalụ kemịkalụ na Ruaphragms.
HVAC: Nkpuru na ndi na - ebu ibu.