GA-32 × 0 General chinangwa silicone rabha (fumed silica) (HCR)

Chishandiso: chakakodzera kugadzira marudzi ese esheath, kitchenware, chikwama, wachi uye zvimwe zvigadzirwa zvakajairika.
Akakosha maficha: kukurumidza kurapa kukurumidza, kusimba kwepamusoro, kugona kwakanakisa, kupfuudza huchokwadi hweRoHS, REACH, uye LFGB.
 
Shanghai Herchy Rubber Co., Ltd inotungamira kugadzira zvemhando yepamusoro silicone rabha zvigadzirwa. Isu tine hunyanzvi mukupa huwandu hwakasiyana-siyana-chinangwa silicone rabha mhinduro dzakagadzirirwa kuzadzisa zvaunoda chaizvo. Nehunyanzvi hwekugadzira tekinoroji uye timu yenyanzvi, tinoburitsa epamusoro performance silicone rubber akasimba, anochinjika, uye anosangana nepamusoro indasitiri zviyero. Titumire zvaunoda chigadzirwa nhasi, uye isu tinopa iyo yakanakira mhinduro yekushandisa kwako.
  • GA-32×0

  • Herchy

Material:
Kuwanikwa:
Huwandu:

GA-32 × 0 General Chinangwa Silicone Rubber (Fumed Silica) Chigadzirwa Tsanangudzo


GA-32 × 0 General Chinangwa Silicone Rubber, inogadzirwa neShanghai Herchy Rubber Co., Ltd, yakagadzirirwa kusangana neyakasiyana siyana yezvido zveindasitiri. Nemagiredhi akasiyana, kusanganisira GA-3230 kusvika GA-3280, inopa kuita kwakasiyana-siyana mumashandisirwo akasiyana. Iyi yakakwirira-inoshanda silicone rabha yakanakira kuvhara, gasketing, uye insulation mumaindasitiri akasiyana semotokari, zvemagetsi, uye kuvaka.


Iyi fumed silica silicone rabha inoratidza kuchinjika kwakanakisa uye kusimba, ichiita kuti ive yakakodzera kune ese ari maviri epamusoro- uye akaderera-tembiricha nharaunda. Inopa simba rakatanhamara rekusimba, kurebesa, uye kubvarura kuramba, kuve nechokwadi chekuita kwenguva refu kunyangwe pasi pemamiriro anodikanwa. Inowanzo shandiswa mumashandisirwo anoda zvese kuchinjika uye simba, senge silicone seals, silicone gaskets, uye elastomeric components.


Iyo translucent silicone rabha inowanikwa mumhando dzakasiyana dzekuoma, kubva pa30 Shore A kusvika 80 Shore A, ichikupa iwe kugona kusarudza giredhi rakanyatsokodzera kune zvaunoda chaizvo. Nekusiyana-siyana uye kusimba kwesimba, iyo GA-32 × 0 nhevedzano inogona kugadziridzwa kune akasiyana maindasitiri uye ekutengesa maapplication.


Iyo GA-32 × 0 yakatevedzana inoshanda zvakasiyana-siyana, zvichiita kuti ive sarudzo yakanaka kune tsika silicone rabha mhinduro. Kunyangwe iwe uchida inochinjika silicone rabha yezvikamu zvemotokari, zvikamu zvemagetsi, kana zvekuvakisa, chigadzirwa ichi chinopa mashandiro anoshamisa pane dzakasiyana siyana dzekushandisa.


Muedzo: 1% yekurapa mumiririri (50% paste yeDBPMH musilicone gum), 175 ° x 5min x 15MPa.


Parameter Tafura


Product parameters
Product GA-3230
GA-3240 GA-3250 GA-3260 GA-3270 GA-3280
Chitarisiko Translucent
Williamplasticity
140
180
210
240
280
310
Kuoma (ShoreA)
30
40
50
60
70
80
Density(g/cm3) 1.08
1.11
1.14
1.17
1.20
1.22
Tensilestrength (MPa)

9
9.5
11
10.5
10.5
9
Elongation(%) 900
700
650
600
450
350
Kusimba kwemisodzi (kN/m) 18
22
25
30
30
30

Iine GA-32 × 0 General Chinangwa Silicone Rubber akatevedzana, iwe unowana yakavimbika, inogoneka mhinduro dzeakasiyana maindasitiri ekushandisa. Kunyangwe iwe uchitsvaga silicone rabha yekugadzira, yakakwirira kubvambura simba silicone rabha, kana inochinjika rabha zvinhu zvekuisa chisimbiso, zvigadzirwa zvedu zvinopa kuita kwakanyanya mumusika.


Bata nesu nhasi kuti tikurukure zvaunoda purojekiti, uye isu tichagadzirisa iyo yakakwana HCR silicone rabha kuti ienderane nezvido zvako.


General Chinangwa Silicone Rubber series

GA-32 × 0 General Chinangwa Silicone Rubber Features


GA-32 × 0 General Chinangwa Silicone Rubha, ine fumed silica, chinhu chinosiyana-siyana chakanakira akasiyana siyana ekushandisa mumaindasitiri. Iyo inopa kuita kwepamusoro uye inovimbwa nemaindasitiri anoda anogara uye anochinjika elastomers. Pazasi pane akakosha maficha anoita GA-32 × 0 sarudzo yakavimbika.


Zvishandiso Zvakasiyana-siyana

GA-32 × 0 inoshandiswa mukugadzira zvakasiyana-siyana silicone rabha zvigadzirwa sezvisimbiso, gaskets, uye machira ekudzivirira. Inonyanya kushanda mumaindasitiri akaita semotokari, zvemagetsi, uye zvigadzirwa zvevatengi, zvichiita kuti ive sarudzo yakakurumbira yezvese-chinangwa kunyorera.


Kukurumidza Kurapa Speed

Iyi silicone rabha inoratidza kukurumidza kurapa nguva, inosimudzira kugadzirwa kwakanaka uye kuderedza nguva. Kunyangwe iwe uri kugadzira silicone zvikamu zvezvisimbiso zvemotokari kana magetsi ekuisa, GA-32 × 0 inopa nekukurumidza kurapwa kusangana nepamusoro-inodiwa masheti ekugadzira.


High Tensile Simba

GA-32 × 0 inopa yakasarudzika simba rekusimba, kuve nechokwadi chekugara kwenguva refu mukuita zvinoda maapplication. Ichi chivakwa chinoita kuti ive yakanaka kune zvikamu zvinosangana nekushushikana kwemagetsi, senge zvisimbiso, gaskets, uye zvivharo zvekudzivirira.


Yakanakisa Processing Performance

Iko kureruka kwekugadzirisa kunoita kuti GA-32 × 0 ikwane kune akasiyana mold dhizaini. Hunhu hwayo hwakatanhamara hwekuyerera hunoita kuti mhedzisiro inowirirana uye zvigadzirwa zvemhando yepamusoro, zvakakwana kune ese ari maviri tsika uye maitiro ekugadzira akawanda.


Kutevedza neInternational Standards

GA-32 × 0 silicone rabha inosangana neakakosha epasirese zviyero seRoHS, REACH, uye LFGB zvitupa. Izvi zvitupa zvinovimbisa kuti zvinhu zvacho zvakachengeteka kuti zvishandiswe mumagiredhi echikafu, zvishandiso zvekurapa, uye zvigadzirwa zvinoda kutevedzwa kwakasimba.


Kuwedzera Kusimba Kwemisodzi

GA-32 × 0 inoratidza inoshamisa simba rekubvarura, ichivimbisa kusimba kunyangwe mumamiriro ezvinhu akaoma. Inonyanya kukodzera zvisimbiso zvemabhizimisi uye zvimwe zvigadzirwa zvinoda kutsungirira nguva dzose kupfeka uye kubvarura.


Yakanaka Yakaderera uye Yakakwira Temperature Resistance

GA-32 × 0 inoshingirira zvakanyanya kune tembiricha yakanyanyisa, ichichengetedza kutendeseka kwayo mumhando dzakasiyana dzetembiricha. Izvi zvinoita kuti ive yakanakira kushandiswa mumashandisirwo akadai sezvikamu zvemotokari, aerospace, uye zvemagetsi, uko kugadzikana kwepamusoro uye kwakaderera-tembiricha kwakakosha.


Customizable Magiredhi kune Chaiyo Inodiwa

Iine akasiyana magiredhi ekuomarara, GA-32 × 0 inogona kugadzirwa kune zvaunoda chaizvo. Kunyangwe iwe uchitsvaga yakapfava elastomer yezvisimbiso kana giredhi yakasimba yemagaskets, iyi silicone rabha inogona kugadzirwa kuti isangane nezvako chaizvo.


Shanghai Herchy Rubber Co, Ltd inotungamira mugadziri uye mutengesi wesilicone rabha uye zvimwe zvigadzirwa elastomer. Nekutarisa pazvinhu zvemhando yepamusoro, tinoshandira maindasitiri akaita semotokari, ndege, zvekurapa, uye zvinhu zvevatengi. Chikwata chedu chine ruzivo chinoona kuti chigadzirwa chega chega chinosangana nemhando yepamusoro yemhando uye kuita, kubatsira vatengi vedu kuzadzisa zvinangwa zvavo nemhinduro dzakavimbika. Kunyangwe iwe uchitsvaga masikirwo esilicone, maumbirwo etsika, kana imwe giredhi rerabha, tinopa zvinochinjika uye zvakagadzirirwa mhinduro dzezvido zvebhizinesi rako.


KuShanghai Herchy Rubber Co., Ltd., takazvipira kuendesa hunyanzvi uye hutsva, kuve nechokwadi chekuti zvigadzirwa zvedu zvese, zvinosanganisira GA-32 × 0, zvinozadzisa zvaunoda chaizvo uye kubatsira kufambisa bhizinesi rako kumberi.

Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.