1. Xarunta FKM (FKM)

Guryaha:

  • Cadaadiska ugu daran caabbinta (-20 ° C illaa + 250 ° C).

  • Caawinta gaarka ah ee saliidaha, shidaalka, dareeraha, aashitada, iyo saldhigyada.

  • Awoodda sare ee mudaharaad (10-20 MPA), isku-dhafan oo hoos udhac ah (<15% 150 ° C / 70h).

  • Olol dib-u-dhac ah (Ul94 V-0 qiimeynta) iyo ozone-adkeysi.

Faa'iidooyinka:

  • Horudhacday (tusaale ahaan, bisphenol af, peroxide) si hufan u nugul.

  • Waxay sii jirtaa xasilloonida cabirka ee deegaannada kiimikada ee rabshadaha ah.

  • Darajooyinka FDA-ka-hogaanka ah ee loo heli karo cuntada / xiriirka caafimaadka.

Codsiyada:

  • Aerospace: Nidaamka shidaalka o-giraanta, shaabadaha mashiinka, iyo diaphragms.

  • Gawaarida: Ganacsiga turbogers-ka, xargaha gudbinta, iyo qudhayaasha shidaalka.

  • Kiimikada: daqiiqadaha matoorka, kuraasta valve, iyo tuubooyinka tuullada.

2. Xarunta Hnbr (HNBR)

Guryaha:

  • Cadaadiska kululaynta ilaa + 150 ° C (oo aan kala go 'lahayn + 175 ° C).

  • Iska caabin ka sareeya saliidaha, amines, iyo dareeraha hydralic.

  • Awoodda sare ee mudaharaad (15-35 MPA) iyo iska caabinta caabbinta daalka.

  • Qurux-darrooyinka hoose ee gaasaska.

Faa'iidooyinka:

  • Cudur ka hor ayaa loo kaxeeyey waqtiga la dhimay.

  • Waxay ku sii wadaysaa dhaxalka hoostiisa oo ka hooseeya soo-gaadhista saxaafadda adag.

  • Waxaa laga heli karaa fasalada Peroxide- ama shaashad-sulfur.

Codsiyada:

  • Shidaalka & gaaska: Xirmooyinka qodista, shaabadaha bamka dhoobada, iyo qaybaha waaweyn.

  • Gawaarida: suumanka waqtiga, nidaamyada duritaanka shidaalka, iyo tuubooyinka tufaaxeedka.

  • Warshadaha: Xirmooyinka dhululubo ee hydrauder iyo qalabka gaaska.

3. Xarunta NBR (NBR)

Guryaha:

  • Iska caabbinta saliida ee dhexdhexaad ah (ka fiican EPDM, wax ka yar HNBR).

  • Tusmaha heerkulka: -40 ° C illaa + 120 ° C.

  • Calaamadoonaanta sare (ASTM D5963: 100-200 mm³ khasaaro).

  • Adkeysiga wanaagsan iyo cadaadiska ayaa iska caabbinta.

Faa'iidooyinka:

  • Qiimaha wax ku oolka ah oo leh miro aad u wanaagsan.

  • Waxyaabaha loo yaqaan 'acrylonitrit acrylonitrile' (18-50%) si loogu caabbiyo saliida saliida.

Codsiyada:

  • Gawaarida: tuubooyinka shidaalka, o-giraanta, iyo shaashadda gudbinta.

  • Warshadaha: Suumanka Conveyor, Daabacaadda Rollers, iyo Xirmooyinka Hydralic.

  • Macmiilka: galoofyada cinjirka iyo qalabka isboortiga.

4. Xarunta EPDM (Ethylenene Propylene Dieneomer)

Guryaha:

  • Iska caabbinta cimilada / cimilada (5,000+ saacadood ee baaritaanka Quid).

  • Xaddiga heerkulka: -50 ° C illaa + 150 ° C.

  • Awoodda sare ee Dielectric (20-30 kV / mm) iyo biyo-mareenka.

  • Gaaska gaaska yar.

Faa'iidooyinka:

  • Lagu diyaariyey ka hortagga antioxidants iyo xasilayaasha UV.

  • Garabka wanaagsan ee gariirka (khasaaraha khasaaraha: 0.1-0.3).

Codsiyada:

  • Gawaarida: Xirmooyinka albaabka, tuubooyin hiitarka, iyo mashiinka ayaa kor u qaadaya.

  • Dhismaha: xuubka saqafka, saqafka saqafka, line line, iyo gaaska daaqadaha.

  • Korantada: Daaweynta Cable iyo Suumanka Gudbinta Awoodda.

5. Xarunta MPU (MPU)

Guryaha:

  • Awoodda sare ee Tensele (20-60 MPA) iyo dabacsanaan (ilaa 800% conongotion).

  • Caabudyaha Ka-Baxsan (ASTM D5963: 20-50 mm³ khasaaro).

  • XUQUUQDA: -40 ° C illaa + 100 ° C (illaa + 120 ° C oo leh kuleylka kuleylka).

  • U adkaysata solvents iyo hydrolysis.

Faa'iidooyinka:

  • Adag oo adag (xeebta ah 50-95).

  • Waxaa laga heli karaa dhiiga, malax, ama buundooyin heerkul ah.

Codsiyada:

  • Warshadaha: giraangiraha, rollers, iyo suumanka lagu gudbiyo.

  • Gawaarida: Caymiska lagu joojiyo, nasiino naxdin, iyo kabaha wadajirka ah ee CV.

  • Caafimaadka: Cadhogayaasha, geesaha orthopedic, iyo sabooliska.

6. Xarunta ACM (ACM)

Guryaha:

  • Caabbi karta kuleylka joogtada ah ilaa + 150 ° C (oo ay ku dhexeysaan + 175 ° C).

  • Caadid aad u fiican oo cabitaanno toos ah (ATF), saliido, iyo kuleyl.

  • Ozone dhexdhexaad ah iyo iska caabbinta cimilada.

  • Xoog maleh: 7-15 MPA.

Faa'iidooyinka:

  • Horudhacday oo ay ku dhacday daawooyinka amine ama aruuriyaha si dhakhso leh u daaweyn.

  • Waxay ku haysaa xasilloonida cabirrada ee deegaannada ATF.

Codsiyada:

  • Gawaarida: Shaatiyada gudbinta, o-giraanta, iyo xaashida diaphms.

  • Qaybaha nidaamka isteerinka awooda.

  • Warshadaha: shaabadaha matoorka ee warbaahinta saliida ku saleysan.

7. AEM Consult (AEM)

Guryaha:

  • Xanuun heerkul ballaaran (-40 ° C illaa + 150 ° C).

  • Caabbinta saliidaha, glcols, iyo cimilada.

  • Xoog sare oo sarreeya (10-20 MPA) iyo cadaadiska ayaa iska caabbinta.

  • Qurux-darrooyinka hoose ee gaasaska.

Faa'iidooyinka:

  • Isu dheellitirka iska caabinta kuleylka iyo dabacsanaanta.

  • U adkaysata hydrolysis iyo gabowga.

  • Waxaa laga heli karaa fasalada Peroxide- ama shaashad-sulfur.

Codsiyada:

  • Gawaarida: Riwaayadda kuleylka, qaybaha nidaamka qaboojiyaha, iyo tuubooyinka qaadashada hawada.

  • Warshadaha: Suumanka loo yaqaan 'gelts' loogu talagalay wax ka qabashada kiimikada iyo xaashida bamka.

  • HVAC: DIIWAAN GALING iyo ILAASHADA DHAQANKA.


Xiriir deg deg ah

Alaabadayadayada

Macluumaadka xiriirka

Ku dar: Maya.33, Lane 159, The Road, Degmada Fenyexian, Shanghai
Tel / whatsapp / skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai herrchy caag Co., Ltd. Hartemap |   Qaanuunka Arrimaha Khaaska ah | Taageer by Hondong.