Compound Rubbers: Nneɛma a Ɛkɔ Akyiri, Mfaso, ne Nea Wɔde Di Dwuma

1. FKM Nnuru a Wɔde Yɛ Adwuma (FKM) .

Agyapadeɛ:

  • Ɔhyew a ɛtra so a ɛko tia (-20°C kosi +250°C).

  • Nneɛma soronko a ɛko tia ngo, pɛtro, nnuru a wɔde siw ano, acid, ne bases.

  • Ahoɔden a ɛkorɔn a ɛtwetwe (10-20 MPa), nhyɛso a ɛba fam a wɔde asi hɔ (<15% wɔ 150°C/70h).

  • Ogya a ɛmma ogya ntumi nhyew (UL94 V-0 rating) na ɛko tia ozone.

Mfaso a ɛwɔ so:

  • Wɔde nnuru a wɔde sa yare (sɛ nhwɛso no, bisphenol AF, peroxide) adi kan afra mu ama vulcanization a etu mpɔn.

  • Ɛkura dimensional stability wɔ aggressive nnuru a atwa yɛn ho ahyia.

  • FDA-compliant grades a ɛwɔ hɔ ma aduan/aduruyɛ mu nkitahodi.

Nnwuma a Wɔde Di Dwuma:

  • Ahunmu: Petrol nhyehyɛe O-rings, engine seals, ne diaphragms.

  • Kar: Turbocharger gaskets, transmission seals, ne petrol injectors.

  • Nnuru: Pɔmpɛ a wɔde kata so, valve nkongua, ne hose a wɔaboaboa ano.

2. HNBR Nnuru (HNBR) .

Agyapadeɛ:

  • Ɔhyew a ɛko tia kodu +150°C (ɛyɛ bere ne bere mu +175°C).

  • Ɛko tia ngo, amine, ne nsu a ɛwɔ nsu mu a ɛkorɔn.

  • Ahoɔden a ɛkorɔn a ɛtwetwe (15–35 MPa) ne ɔbrɛ a ɛko tia.

  • Mframa a ɛmma mframa nkɔ mu a ɛba fam.

Mfaso a ɛwɔ so:

  • Pre-vulcanized ma ɛtew bere a wɔde yɛ adwuma.

  • Ɛkura elasticity mu wɔ bere tenten a wɔde hyɛ nsɛm ho amanneɛbɔ a emu yɛ den mu.

  • Wɔde peroxide anaa sulphur ayɛ mu.

Nnwuma a Wɔde Di Dwuma:

  • Oil & Gas: Drilling packers, atɛkyɛ pɔmpɛ nsɔano, ne abura no ti afã horow.

  • Kar: Timing belt, pɛtro a wɔde gu mu, ne turbocharger hose.

  • Mfiridwuma: Hydraulic cylinder seals ne gearbox afã horow.

3. NBR Nnuru a Wɔde Yɛ Adwuma (NBR) .

Agyapadeɛ:

  • Ngo a ɛko tia a ɛkɔ fam (eye sen EPDM, ennu HNBR).

  • Ɔhyew a ɛwɔ hɔ: -40°C kosi +120°C.

  • Abrasion a ɛkorɔn a ɛko tia (ASTM D5963: 100–200 mm3 a ɛyera).

  • Resilience pa ne compression set resistance.

Mfaso a ɛwɔ so:

  • Ɛho ka sua a ɛma wotumi nwene nneɛma yiye.

  • Acrylonitrile dodow a wotumi sesa (18–50%) ma ngo a wɔahyɛ da ayɛ.

Nnwuma a Wɔde Di Dwuma:

  • Kar: Petrol hose, O-ring, ne transmission seals.

  • Mfiridwuma: Conveyor belts, printing rollers, ne hydraulic seals.

  • Nea ɔde di dwuma: Latex nsateaa ne agumadi nnwinnade.

4. EPDM Nneɛma a Wɔde Yɛ Adwuma (Ethylene Propylene Diene Monomer) .

Agyapadeɛ:

  • Ozone/wim tebea a ɛda nsow a ɛko tia ( nnɔnhwerew 5,000+ wɔ QUV sɔhwɛ mu).

  • Ɔhyew a ɛwɔ hɔ: -50°C kosi +150°C.

  • Dielectric ahoɔden a ɛkorɔn (20–30 kV/mm) ne nsuo a ɛrentumi nkɔ mu.

  • Mframa a ɛtumi fa mu a ɛba fam.

Mfaso a ɛwɔ so:

  • Wɔde nnuru a ekum ɔyare mmoawa ne UV stabilizers adi kan ayɛ.

  • Wosow damping a eye kyɛn so (adehwere factor: 0.1–0.3).

Nnwuma a Wɔde Di Dwuma:

  • Kar: Ɔpon ano nsɔano, radiator hose, ne engine mounts.

  • Adansi: Nhama a wɔde kata ɔdan atifi, atare a wɔde kata so, ne mfɛnsere mu gasket.

  • Electrical: Cable insulation ne ahoɔden a wɔde fa mu abɔso.

5. MPU Nneɛma a Wɔde Yɛ Adwuma (MPU) .

Agyapadeɛ:

  • Ahoɔden a ɛkorɔn a ɛtwetwe (20–60 MPa) ne elasticity (ɛkɔ 800% elongation).

  • Abrasion a ɛyɛ soronko a ɛko tia (ASTM D5963: 20–50 mm3 a ɛyera).

  • Ɔhyew a ɛwɔ hɔ: -40°C kosi +100°C (ɛkɔ +120°C a wɔde nneɛma a ɛma ɔhyew gyina so).

  • Ɛko tia nnuru a wɔde siw ano ne nsu mu nsu a ɛyɛ hyew.

Mfaso a ɛwɔ so:

  • Nneɛma a ɛyɛ den a wotumi sesa (Shore A 50–95).

  • Wobetumi anya bi wɔ cast, millable, anaa thermoplastic grades mu.

Nnwuma a Wɔde Di Dwuma:

  • Mfiridwuma: Ntwahonan, rollers, ne conveyor belts.

  • Kar: Bushings a wɔde sɛn so, shock absorbers, ne CV joint boots.

  • Aduruyɛ: Catheters, nnompe a wɔde hyɛ nipadua mu, ne nnompe a wɔde hyɛ nipadua mu.

6. ACM Nneɛma a Wɔde Yɛ Adwuma (ACM) .

Agyapadeɛ:

  • Ɔhyew a ɛkɔ so gyina ano kodu +150°C (ɛyɛ bere ne bere mu +175°C).

  • Nsu a wɔde fa nneɛma a ɛyɛ adwuma ankasa (ATF), ngo, ne ɔhyew a ɛko tia yiye.

  • Ozone a ɛkɔ fam ne wim tebea a ɛko tia.

  • Ahoɔden a ɛtwetwe ade: 7–15 MPa.

Mfaso a ɛwɔ so:

  • Wɔde amine anaa peroxide aduru a wɔde sa yare adi kan afra mu ma ayɛ yiye ntɛmntɛm.

  • Ɛkura dimensional stability mu wɔ ATF mmeaeɛ.

Nnwuma a Wɔde Di Dwuma:

  • Kar: Transmission seals, O-rings, ne pump diaphragms.

  • Power steering nhyehyɛe no afã horow.

  • Mfiridwuma: Pɔmpɛ nsɔano a wɔde yɛ nsɛm ho amanneɛbɔ a wɔde ngo ayɛ.

7. AEM Nneɛma a Wɔde Yɛ Adwuma (AEM) .

Agyapadeɛ:

  • Ɔhyew a ɛtrɛw (-40°C kosi +150°C).

  • Ngo, glycols, ne wim tebea a ɛko tia.

  • Ahoɔden a ɛkorɔn a ɛtwetwe (10-20 MPa) ne nhyɛso set resistance.

  • Mframa a ɛmma mframa nkɔ mu a ɛba fam.

Mfaso a ɛwɔ so:

  • Ɛma ɔhyew a ɛko tia ne sɛnea ɛyɛ mmerɛw no kari pɛ.

  • Ɛko tia nsu a ɛtwetwe ne onyin.

  • Wɔde peroxide anaa sulphur ayɛ mu.

Nnwuma a Wɔde Di Dwuma:

  • Kar: Radiator hose, coolant system no afã horow, ne mframa a wɔde fa mu hose.

  • Mfiridwuma: Conveyor belts a wɔde di nnuru ho dwuma ne pɔmpɛ diaphragms.

  • HVAC: Duct gaskets ne vibration isolators.


NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.