SAIC® EPDM 626

SABIC EPDM 626 matsakaicin dankon wata ne, babban ethylene da ƙarancin abun ciki na ENB wanda aka samar ta hanyar polymerization na bayani ta amfani da mai kara kuzari na metallocene. Yana da matsakaicin rarraba nauyin kwayoyin halitta. Ana samun wannan samfurin a sigar pellet.
  • 626

  • SABIC

  • Bayanan Bayani na EPDM626

samuwa:
Yawan:

DARAJAR ARZIKI NA DUKIYA:

DUKIYA MATSALOLIN MATAKI RAKA'A HANYOYIN gwaji
KAYAN POLYMER


Dankowar Mooney


ML 1+4, 125 °C (1) 67
MU
Saukewa: ASTMD1646
Abubuwan Ethylene 69
wt.%
Saukewa: ASTMD3900
Abun ciki Ethylidene Norbornene (ENB). 2.8
wt.% Saukewa: ASTMD6047

HALAYE:

 SABIC EPDM 626 an ƙera shi don: ingantattun kaddarorin jiki, ingantaccen haɗawa da sarrafa niƙa, ingantaccen calenderability, mafi kyawun riƙe mai, rage furen magani a cikin mahadi.

AJIYA DA KIYAYE: SABIC EPDM 626 yakamata a adana shi a cikin marufinsa na asali a yanayin zafi a yanayin bushewa; gudanawar pellets na iya zama mummunan tasiri ta matsa lamba ko babban zafin jiki; ya kamata a guje wa fuskantar zafi, hasken ultraviolet da hasken rana kai tsaye. A ƙarƙashin yanayin ajiyar da ya dace, samfurin ya tsaya tsayin daka na tsawon watanni 24 daga ranar da aka yi. SABIC ba za ta tsawaita garantin sa ba lokacin da yanayin ajiya bai isa ba wanda zai iya haifar da lalacewa mai inganci kamar taurin pellet ko canjin launi wanda zai iya haifar da ƙarancin aikin samfur.

 DISCLAIMER Duk wani tallace-tallace ta SABIC, rassan sa da masu haɗin gwiwa (kowane mai siyarwa), ana yin shi ne kawai ƙarƙashin daidaitattun sharuɗɗan siyarwa (samuwa akan buƙata) sai dai in an yarda da haka a rubuce kuma aka sanya hannu a madadin mai siyarwa. Yayin da bayanin da ke ƙunshe a cikin ya ke bayar da gaskiya mai kyau, MAI SALLA BABU WARRANTI, BAYANI KO BAYYANA, HAR DA SAMUN SAUKI DA RASHIN DUKIYAR HANKALI, KUMA BAYA YIWA WANI ALHAKI, GASKIYA KO GASKIYA, GASKIYA, GASKIYA, GASKIYA, GASKIYA. DON NUFIN AMFANI KO MANUFAR WADANNAN KAyayyakin A kowace APPLICATIONS. Dole ne kowane abokin ciniki ya ƙayyade dacewar kayan mai siyarwa don amfanin abokin ciniki ta hanyar gwaji da bincike da ya dace. Babu wata sanarwa ta mai siyarwa game da yuwuwar amfani da kowane samfur, sabis ko ƙira da aka yi niyya, ko yakamata a fassara, don ba da kowace lasisi ƙarƙashin kowane haƙƙin mallaka ko wasu haƙƙin mallaka.


Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.