GA-32×0 Silicone rababa si wozãna le mɔ gbadza nu (silica si me dzudzɔ le) (HCR) .

Dɔwɔwɔ: sɔ na wɔwɔ ƒomevi ɖesiaɖe sheath, nuɖanuwo, gakotoku, gaƒoɖokuibandand nu bubu siwo bɔ.
Nu veviwo: kabakaba dɔyɔyɔ duƒuƒu, ŋusẽ gã, processability nyuitɔ kekeake,to RoHS, REACH, kple LFGB ƒe kpeɖodzinana.
 
Shanghai Herchy Rubber Co., Ltd nye dɔwɔƒe xɔŋkɔ aɖe si wɔa silicone rababa ƒe nuwɔna deŋgɔwo. Míewɔa dɔ tɔxɛ le silicone rababa ƒe kuxiwo gbɔ kpɔnu vovovo siwo wozãna le mɔ gbadza nu siwo wowɔ ɖe ɖoɖo nu be woakpɔ wò nuhiahiã tɔxɛwo gbɔ la nana me. Míetsɔa mɔ̃ɖaŋununya deŋgɔ siwo wowɔna kple eŋutinunyalawo ƒe ƒuƒoƒo aɖe tsɔa silicone rababa siwo wɔa dɔ nyuie wu siwo nɔa anyi didina, siwo te ŋu trɔna bɔbɔe, eye wosɔna ɖe dɔwɔƒea ƒe dzidzenu kɔkɔtɔwo kekeake nu la naa amewo. Ðo wò adzɔnuwo ƒe nudidiwo ɖe mí egbea, eye míana egbɔkpɔnu nyuitɔ kekeake na wò dɔbiagbalẽvi.
  • GA-32×0 ƒe ƒuƒoƒo

  • Herchy ƒe ame

Nusiwo wotsɔ wɔe:
Nusiwo li:
Agbɔsɔsɔ:

GA-32 × 0 Taɖodzinu Gbãtɔ Silicone Rubber (Fumed Silica) Adzɔnuwo Numeɖeɖe


Wotrɔ asi le GA-32 × 0 Taɖodzinu Gbãtɔ Silicone Rubber, si Shanghai Herchy Rubber Co., Ltd wɔ, be wòakpɔ dɔwɔƒewo ƒe nuhiahiã vovovowo gbɔ. Esi wòxɔ dzesi vovovowo, siwo dome GA-3230 va ɖo GA-3280 hã le, enaa dɔwɔwɔ si woate ŋu azã le mɔ vovovowo nu le dɔwɔwɔ vovovowo me. Silicone rababa sia si wɔa dɔ nyuie la nyo ŋutɔ na nutrenu, gasket, kple nusiwo xea mɔ na dzoxɔxɔ le dɔwɔƒe vovovowo abe ʋuwo, elektrɔnikmɔ̃wo, kple xɔtutu ene me.


Silica silicone rababa sia si me dzo le la ɖea asitɔtrɔ le nɔnɔmewo ŋu nyuie ŋutɔ eye wònɔa anyi didina, si wɔe be wòsɔ na dzoxɔxɔ gã kple dzoxɔxɔ sue siaa. Enaa ŋusẽ ɖedzesi aɖe si woate ŋu aʋuʋu, didi, kple aɖatsi te ŋu, si wɔnɛ be wowɔa dɔ ɣeyiɣi didi le nɔnɔme sesẽwo gɔ̃ hã me. Wozãnɛ zi geɖe le dɔ siwo bia be woate ŋu atrɔ ɖe nɔnɔmewo ŋu eye ŋusẽ nanɔ wo ŋu siaa, abe silicone-nutrenuwo, silicone-gaskets, kple elastomeric-nu siwo wotsɔ wɔa nu ene.


Silicone rababa si me kɔ la li le sesẽme vovovowo me, tso 30 Shore A va ɖo 80 Shore A, si naa ŋutete wò be nàtia dzesi si sɔ wu na wò hiahiã tɔxɛwo. Esi woƒe kpekpeme kple eƒe tenɔnɔ ƒe ŋusẽ le vovovo ta la, woate ŋu atrɔ asi le GA-32×0 ƒe hatsotsoawo ŋu na dɔwɔƒewo kple asitsatsa ƒe dɔwɔwɔ vovovowo.


GA-32×0 ƒe hatsotso la nye esi woate ŋu azã le mɔ vovovowo nu ŋutɔ, si wɔe be wònye tiatia nyui aɖe na silicone rababa ƒe kuxiwo gbɔ kpɔnu siwo wowɔ ɖe ɖoɖo nu. Eɖanye be èhiã silicone rababa si te ŋu trɔna bɔbɔe na ʋu ƒe akpa aɖewo, elektrik ƒe akpa aɖewo, alo xɔtunuwo o, adzɔnu sia naa dɔwɔwɔ tɔxɛ aɖe le zazã vovovowo me.


Dodokpɔ: 1% le atike si daa gbe le ame ŋu (50% ƒe atike si wotsɔ DBPMH wɔe le silicone gum me), 175° x 5min x 15MPa.


Parameter Tabla


Nusiwo wowɔ ƒe nɔnɔmewo
Nu si wowɔ GA-3230 ƒe agbalẽa
GA-3240 ƒe agbalẽ GA-3250 ƒe agbalẽa GA-3260 ƒe agbalẽa GA-3270 ƒe agbalẽa GA-3280 ƒe agbalẽ
Dzedzeme Nusi me kɔ nyuie
Williamplasticity ƒe dɔwɔwɔ
140
180
210
240
280
310
Sesẽme (ƑutaA) .
30
40
50
60
70
80
Eƒe kpekpeme(g/cm3) . 1.08
1.11
1.14
1.17
1.20
1.22
Ŋusẽ si le lãme na ame (MPa) .

9
9.5
11
10.5
10.5
9
Elongation(%) ƒe didime . 900
700
650
600
450
350
Aɖatsi ƒe ŋusẽ (kN/m) . 18
22
25
30
30
30

Le GA-32 × 0 General Purpose Silicone Rubber series, èkpɔa egbɔkpɔnu siwo ŋu kakaɖedzi le, siwo woate ŋu atrɔ asi le na dɔwɔƒewo ƒe dɔ vovovowo. Eɖanye silicone rababa dim nèle hena ewɔwɔ, silicone rababa si ƒe ŋusẽ te ŋu ʋuʋuna ŋutɔ, alo rababa ƒe nusiwo te ŋu trɔna bɔbɔe hena nutrenu dim o, míaƒe nutovɛwo naa dɔwɔwɔ nyuitɔ kekeake le asi me.


Te ɖe mía ŋu egbea be míadzro wò dɔa ƒe nudidiwo me, eye míatrɔ asi le HCR silicone rababa si sɔ pɛpɛpɛ ŋu wòasɔ ɖe wò hiahiãwo nu.


Taɖodzinu Gbãtɔ Silicone Rubber kplɔ wo nɔewo ɖo

GA-32 × 0 Taɖodzinu Gbãtɔ Silicone Rubber Nɔnɔmewo


GA-32×0 General Purpose Silicone Rubber, si me fumed silica le, nye nusi woate ŋu azã le mɔ vovovowo nu si sɔ nyuie na dɔwɔƒewo ƒe dɔwɔwɔ vovovowo. Enaa dɔwɔwɔ deŋgɔ eye dɔwɔƒe siwo hiã elastomers siwo nɔa anyi didina eye woate ŋu atrɔ ɖe nɔnɔmewo ŋu la ka ɖe edzi. Nu vevi siwo na GA-32×0 nye tiatia si ŋu kakaɖedzi le la le ete.


Dɔwɔwɔ Siwo Woate Ŋu Azã le Mɔ Vovovowo Me

Wozãa GA-32×0 le silicone rababa ƒe nu vovovowo abe nutrenu, gasket, kple ametakpɔnu siwo wotsɔ blaa nu ene wɔwɔ me. Ewɔa dɔ nyuie ŋutɔ le dɔwɔƒewo abe ʋuwo, elektrɔnikmɔ̃wo, kple nuzazãwo wɔwɔ me, si wɔe be wònye tiatia si ame geɖe lɔ̃a zazã le dɔ siwo wozãna le mɔ gbadza nu.


Dɔdada Kabakaba ƒe Duƒuƒu

Silicone rababa sia ɖea ɣeyiɣi siwo wotsɔ daa dɔ kabakaba fiana, si naa ewɔwɔ ƒe ŋutete nyona ɖe edzi eye wòɖea ɣeyiɣi si woatsɔ awɔ dɔe dzi kpɔtɔna. Eɖanye silicone ƒe akpa aɖewo wɔm nèle na ʋu ƒe nutrenu alo elektrik-nu siwo xea mɔ na ʋu ƒe nutrenu o, GA-32×0 naa dɔyɔyɔ kabakaba be wòawɔ ɖe ewɔwɔ ƒe ɖoɖowɔɖi siwo wobia tso ame si ŋutɔ dzi.


Tensile Ŋusẽ si Kɔkɔ

GA-32 × 0 naa tensile ŋusẽ tɔxɛ aɖe, si kpɔa egbɔ be ewɔa dɔ ɣeyiɣi didi le dɔ sesẽwo me. Nɔnɔme sia na wòsɔ nyuie na akpa siwo toa mɔ̃wo ƒe nuteɖeamedzi me, abe nutrenu, gasket, kple ametakpɔnu ene.


Dɔwɔwɔ Nyuie Nyuie

Alesi eŋudɔwɔwɔ le bɔbɔe na GA-32×0 sɔ na aŋɔ ƒe nɔnɔme vovovowo. Eƒe sisi ƒe nɔnɔme ɖedzesiwo naa emetsonu siwo mewɔa tɔtrɔ o kple nusiwo le nyonyome deŋgɔ, siwo sɔ nyuie na nusiwo wowɔ ɖe ɖoɖo nu kple esiwo wowɔna le agbɔsɔsɔ gã me siaa.


Dukɔwo Dome Dzidzenuwo Dzi Wɔwɔ

GA-32×0 silicone rababa ɖo dukɔwo dome sedede ƒe dzidzenu veviwo abe RoHS, REACH, kple LFGB ƒe ɖaseɖigbalẽwo ene gbɔ. Ðaseɖigbalẽ siawo kpɔa egbɔ be nusi wotsɔ wɔe la le dedie be woazã le nuɖuɖu siwo sɔ na nuɖuɖu, atikewɔnuwo, kple nusiwo hiã be woawɔ ɖe seawo dzi pɛpɛpɛ me.


Aɖatsi ƒe Ŋusẽ si Dzi Ðe Edzi

GA-32×0 ɖea aɖatsiŋusẽ ɖedzesi aɖe fiana, si wɔnɛ be enɔa anyi eteƒe didina le nɔnɔme sesẽwo gɔ̃ hã me. Esɔ na dɔwɔƒewo ƒe nutrenu kple nu bubu siwo hiã be woanɔ te ɖe woƒe vuvu kple woƒe vuvu ɣesiaɣi nu koŋ.


Dzoxɔxɔ si bɔbɔ kple esi kɔkɔ ƒe tsitretsitsi nyuie

GA-32×0 te ŋu nɔa te ɖe dzoxɔxɔ si gbɔ eme nu ŋutɔ, eye wòléa eƒe xɔtuɖoɖo ƒe blibonyenye me ɖe asi le dzoxɔxɔ vovovowo me. Esia na wòsɔ nyuie be woazãe le dɔwo abe ʋu ƒe akpa aɖewo, yamenutomeyimɔ̃wo, kple elektrɔnikmɔ̃wo ene me, afisi dzoxɔxɔ gã kple esi mebɔ o ƒe liƒo le vevie ŋutɔ.


Dzeside Siwo Woate Ŋu Atrɔ Asi Le Na Hiahiã Tɔxɛwo

Le sesẽme ƒe dzesi vovovowo ta la, woate ŋu atrɔ asi le GA-32×0 ŋu wòasɔ ɖe wò hiahiã tɔxɛwo nu. Eɖanye elastomer falɛfalɛ dim nèle na nutrenu alo esi sesẽ wu na gasket o, woate ŋu atrɔ asi le silicone rababa sia ŋu wòasɔ ɖe wò nɔnɔme siwo tututu nèdi nu.


Shanghai Herchy Rubber Co., Ltd. nye silicone rababa kple elastomer nu bubuwo wɔwɔ kple wo dzrala xɔŋkɔ aɖe. Esi míetsɔa míaƒe susu ɖoa nuwo ƒe nyonyome deŋgɔ ŋu ta la, míesubɔa dɔwɔƒewo abe ʋuwo, yamenutomeyimɔ̃wo, atikewɔwɔ, kple nuzazãwo ene. Míaƒe ƒuƒoƒo si si nuteƒekpɔkpɔ le kpɔa egbɔ be adzɔnu ɖesiaɖe ɖoa nyonyome kple dɔwɔwɔ ƒe dzidzenu kɔkɔtɔwo gbɔ, si kpena ɖe míaƒe asisiwo ŋu be woaɖo woƒe taɖodzinuwo gbɔ kple egbɔkpɔnu siwo ŋu kakaɖedzi le. Eɖanye silicone ƒe atikewo, atike siwo wowɔ ɖe ɖoɖo nu, alo rababa ƒe hatsotso aɖe koŋ dim nèle o, míenaa egbɔkpɔnu siwo te ŋu trɔna bɔbɔe eye wosɔ ɖe wò dɔwɔƒea ƒe nuhiahiãwo nu.


Le Shanghai Herchy Rubber Co., Ltd., míeɖoe kplikpaa be míana nu nyuitɔ kekeake kple nu yeyewo dodo ɖe ŋgɔ, akpɔ egbɔ be míaƒe adzɔnuwo katã, siwo dome GA-32×0 hã le, ɖo wò nudidiwo tututu gbɔ eye míakpe ɖe ŋuwò nàdo wò dɔwɔƒea ɖe ŋgɔ.

Si do ŋgᴐ: 
Esi kplᴐe ɖo: 

NYAGBLƆÐI KABAWO

MÍAƑE NUWO ƑE NUWO

NYATAKAKA SIWO WOÐO BE WOAÐO BE WOAÐE KPƆKPƆ

Tsɔ kpe ɖe eŋu: No.33, Mɔdodo 159, Taiye Mɔ dzi, Fengxian Nutome, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nutata ƒe Gomenɔamesi     2023 Shanghai Herchy Rubber Co., Ltd. Nyatakakadzraɖoƒe ƒe Nɔnɔmetata |   Ameŋunyatakakawo Ŋuti Ðoɖo | Kpekpeɖeŋu To Leadong ƒe agbalẽ.