GA-32×0 Jɛnɛral pɔpɔshɔn silikon rɔba (fumed silika) (HCR)

Aplikeshɔn: fayn fɔ prodyuz ɔl kayn sheath, kitchenware, purse, watchbandand ɔda kɔvɛnshɔnal prodak dɛm.
Ki ficha dɛm: fast curing spid, ay trɛnk, ɛksɛlɛnt prɔsesabiliti,pas di ɔthɛntishɔn fɔ RoHS, REACH, ɛn LFGB.
 
Shanghai Herchy Rubber Co., Ltd na wan big manifakta fɔ ay kwaliti silikon rɔba prodak. Wi spɛshal fɔ gi bɔku bɔku jenɛral-pɔpɔs silikon rɔba sɔlvishɔn dɛn we dɛn kɔstɔmayz fɔ mit yu spɛshal nid dɛn. Wit advans prodakshɔn teknɔlɔji ɛn wan tim we gɛt ɛkspɛkt, wi de gi supia pefɔmɛns silikon rɔba dɛn we de te, we kin chenj, ɛn we mit di ays industri standad. Send wi yu prodak rikwaymɛnt tide, ɛn wi go gi yu di bɛst sɔlvishɔn fɔ yu aplikeshɔn.
  • GA-32 × 0. Di wan dɛn we de wok

  • Herchy bin de du am

Di tin dɛn we dɛn yuz: Di tin dɛn we
dɛn kin gɛt:
Kwantiti:

GA-32×0 Jɛnɛral Pɔpɔshɔn Silikɔn Rɔba (Fumed Silika) Prodakt Diskripshɔn


GA-32×0 Jɛnɛral Pɔpɔz Silikɔn Rɔba, we Shanghai Herchy Rɔba Kɔmni, Ltd mek, dɛn mek am fɔ mit bɔku bɔku industrial nid dɛn. Wit difrɛn gred dɛn, inklud GA-3230 to GA-3280, i de gi versatile pefɔmɛns akɔs difrɛn aplikeshɔn dɛn. Dis silikon rɔba we de wok fayn fayn wan fɔ sial, gasket, ɛn insuleshɔn na difrɛn industri dɛn lɛk motoka, ilɛktronik, ɛn kɔnstrɔkshɔn.


Dis fumed silika silikon rɔba de sho fayn fayn fleksibiliti ɛn durabiliti, we mek i fayn fɔ ɔl tu di ay ɛn lɔw tɛmpracha ɛnvayrɔmɛnt. I de gi ɔdasayz tɛnsiɛl trɛnk, elongation, ɛn tear resistans, mek shɔ se i de wok fɔ lɔng tɛm ivin ɔnda dimand kɔndishɔn dɛn. Dɛn kin yuz am fɔ du tin dɛn we nid fɔ chenj ɛn trɛnk, lɛk silikon sil, silikon gasket, ɛn ɛlastomɛrik kɔmpɔnɛnt dɛn.


Di translucent silikon rɔba de insay difrɛn hadnɛs lɛvɛl dɛn, we de frɔm 30 Shore A to 80 Shore A, we de gi yu di abiliti fɔ pik di gred we fit yu pas ɔl fɔ yu patikyula nid dɛn. Wit difrɛn density ɛn tɛnsiɛl trɛnk, di GA-32×0 siriɔs kin kɔstɔmayz fɔ difrɛn industrial ɛn kɔmɛshɔnal aplikeshɔn dɛn.


Di GA-32×0 siriɔs na ayli versatile, we mek am wan fayn chuk fɔ kɔstɔm silikon rɔba sɔlvishɔn. Ilɛksɛf yu nid fleksibul silikon rɔba fɔ motoka pat dɛn, ilɛktrik kɔmpɔnɛnt dɛn, ɔ kɔnstrɔkshɔn matirial dɛn, dis prɔdak de gi spɛshal pefɔmɛns akɔdin to bɔku bɔku yus dɛn.


Tεst: 1% pan di kכring ejen (50% paste fכ DBPMH insay silikon gכm), 175° x 5min x 15MPa.


Paramita Tebul


Prodakt paramita dɛn
Sɔntin GA-3230 we dɛn kɔl
GA-3240 we dɛn kɔl GA-3250 we dɛn kɔl GA-3260 we dɛn kɔl GA-3270 we dɛn kɔl GA-3280 we dɛn kɔl
Aw a luk Translucent we de mek pɔsin fil fayn
Wiliamplastisiti
140
180
210
240
280
310
Di hadnɛs (ShoreA) .
30
40
50
60
70
80
Densiti(g/cm3) . 1.08
1.11
1.14
1.17
1.20
1.22
Tεnsilεrεngth (MPa) .

9
9.5
11
10.5
10.5
9
Elongation(%) we de go bifo. 900
700
650
600
450
350
Di trɛnk we pɔsin kin kray (kN/m) . 18
22
25
30
30
30

Wit di GA-32×0 Jɛnɛral Pɔpɔz Silikɔn Rɔba siriɔs, yu gɛt rilibul, kɔstɔmayz sɔlvishɔn fɔ difrɛn industrial aplikeshɔn dɛn. If yu de luk fɔ silikon rɔba fɔ mek, ay tear trɛnk silikon rɔba, ɔ fleksibul rɔba matirial fɔ sial, wi prɔdak dɛn de gi di bɛst pefɔmɛns na di makit.


Kɔntakt wi tide fɔ tɔk bɔt wetin yu nid fɔ du fɔ yu prɔjek, ɛn wi go tayla di pafɛkt HCR silikon rɔba fɔ fit yu nid dɛn.


Jɛnɛral Pɔpɔshɔn Silikɔn Rɔba siriɔs

GA-32×0 Jɛnɛral Pɔpɔshɔn Silikɔn Rɔba Ficha dɛn


GA-32×0 Jɛnɛral Pɔpɔshɔn Silikɔn Rɔba, we gɛt fumed silika, na wan versatile matirial we fayn fɔ bɔku bɔku industrial aplikeshɔn dɛn. I de gi spɛshal pefɔmɛns ɛn di industri dɛn we nid ɛlastom dɛn we de te ɛn we kin chenj, de trɔst am. Dis dɔŋ ya na di men tin dɛn we de mek GA-32×0 na pɔsin we pɔsin kin abop pan.


Aplikeshɔn dɛn we yu kin yuz fɔ du bɔku tin

Dɛn kin yuz GA-32×0 fɔ mek difrɛn silikon rɔba prɔdak dɛn lɛk sil, gasket, ɛn kɔtin dɛn we de protɛkt. I de wok mɔ na industri dɛn lɛk ɔtomotiv, ilɛktroniks, ɛn kɔshɔma guds manufakchurin, we mek am pɔpul choice fɔ jenɛral-pɔpɔs aplikeshɔn.


Fast Curing Spid we yu de yuz

Dis silikon rɔba de sho di tɛm we i de mɛn kwik kwik wan, we de ɛp fɔ mek di prodakshɔn wok fayn ɛn i de ridyus di tɛm we i de wok. If yu de prodyuz silikon pat fɔ ɔtomotiv sil ɔ ilɛktrik insuleshɔn, GA-32×0 de gi kwik kɔring fɔ mit ay-dimand manufakchurin schedule.


Di Strɔng we gɛt ay Tensile

GA-32×0 de gi eksepshɔnal tɛnsiɛl trɛnk, we de mek shɔ se i de wok fɔ lɔng tɛm insay diman aplikeshɔn dɛn. Dis prɔpati de mek i fayn fɔ pat dɛn we gɛt mɛkanikal strɛs, lɛk sil, gasket, ɛn kɔva we de protɛkt.


Eksɛlɛnt Prɔsɛsin Pɔfɔmɛnshɔn

Di izi we aw dɛn de prosɛs de mek GA-32×0 fayn fɔ difrɛn mold dizayn dɛn. I ɔdasayz flɔ kwaliti dɛn de mek shɔ se kɔnsistɛns rizɔlt ɛn ay-kwaliti prodak, pafɛkt fɔ ɔl tu di kɔstɔm ɛn mas prodakshɔn prɔses.


Fɔ fala di Intanɛshɔnal Stɛndad dɛn

GA-32×0 silikon rɔba mit impɔtant intanashɔnal rigyuletɔri standad dɛn lɛk RoHS, REACH, ɛn LFGB sɛtifiket dɛn. Dɛn sɛtifiket dɛn ya de mek shɔ se di matirial sef fɔ yuz fɔ it-grɛd aplikeshɔn, mɛrɛsin divays, ɛn prɔdak dɛn we nid fɔ fala strikt lɔ.


Ɛnjɔy di Tɛar Strɔng

GA-32×0 de sho wɔndaful tear trɛnk, we de mek shɔ se i de te ivin ɔnda harsh kɔndishɔn. I fayn mɔ fɔ di industrial sil ɛn ɔda prɔdak dɛn we nid fɔ bia we dɛn de west ɛn te ɔltɛm.


Gud Lɔw ɛn Ay Tɛmpratura Resistɛns

GA-32×0 na hεli rεsistεnt to tεmprachכ ekstrim, mεnten in strכkchכral integriti akrays wan big rεnj כf tεmprachכ. Dis mek am fayn fɔ yuz insay aplikeshɔn dɛn lɛk motoka pat, ɛrospɛs, ɛn ilɛktroniks, usay ay ɛn lɔw tɛmpracha stebiliti rili impɔtant.


Grɛd dɛn we yu kin kɔstɔmayz fɔ sɔm patikyula nid dɛn

Wit difrɛn hadnɛs gred dɛn, GA-32×0 kin tayla to yu spɛshal nid dɛn. Ilɛksɛf yu de luk fɔ sɔft ɛlastɔma fɔ sil ɔ fɔ gɛt strɔng gred fɔ gasket, yu kin kɔstɔmayz dis silikon rɔba fɔ mit yu ɛksaktɔl spɛsifikɛshɔn dɛn.


Shanghai Herchy Rubber Co., Ltd. na wan big manifakta ɛn saplay fɔ silikon rɔba ɛn ɔda elastomer prɔdak dɛn. Wit fɔ pe atɛnshɔn pan ay kwaliti matirial dɛn, wi de sav industri dɛn lɛk ɔtomotiv, ɛrospɛs, mɛdikal, ɛn kɔshɔma guds. Wi tim we gɛt ɛkspiriɛns de mek shɔ se ɛni prɔdak mit di ay standad fɔ kwaliti ɛn pefɔmɛns, ɛn ɛp wi klaynt dɛn fɔ rich dɛn gol dɛn wit sɔlvishɔn dɛn we dɛn kin abop pan. If yu de luk fɔ silikon kɔmpawnd, kɔstɔm fɔmyulashɔn, ɔ wan patikyula gred fɔ rɔba, wi de gi yu fleksibul ɛn tayla sɔlvishɔn fɔ yu biznɛs nid.


Na Shanghai Herchy Rubber Co., Ltd., wi de wok tranga wan fɔ gi ɛksɛlɛns ɛn inovashɔn, fɔ mek shɔ se ɔl wi prɔdak dɛn, inklud GA-32×0, mit yu ɛksaktɔl rikwaymɛnt dɛn ɛn ɛp fɔ drɛb yu biznɛs fɔ go bifo.

Bifo: 
Nɛks: 

KWƐK LINK DƐN

WI PRODƆKT DƐN

INFƆMƐSHƆN FƆ KƆNTƐKT

Ad: No.33, Len 159, Taiye Rod, Fengxian Distrikt, Shanghai
Tɛl / WatsAp / Skype: +86 15221953351
Kopirayt     2023 Shanghai Herchy Rɔba Kɔmni, Ltd. Sitemap fɔ di sayt |   Prayvesi Polisi | Sɔpɔt Bay Leadong we de na di wɔl.