Telefon: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
NUSIWO WOWƆ
Èle afisia: Aƒeme » Nusiwo Wowɔ » Nuwɔwɔ ƒe Rubber » VMQ Silicone ƒe dɔwɔwɔ » Silicone rababa si ƒe aɖatsi ƒe ŋusẽ lolo (fumed Silica) (HCR)

agbatsɔtsɔ

Mamã na:
facebook dzi mamã ƒe dzesi
twitter dzi mamã ƒe dzesi
fliwo mama ƒe dzesi
wechat mama ƒe dzesi
linkedin mama ƒe dzesi
pinterest mama ƒe dzesi
whatsapp mamã ƒe dzesi
sharethis mamã ƒe dzesi

Silicone rababa si ƒe aɖatsi sesẽ ŋutɔ (fumed Silica) (HCR) .

Dɔwɔwɔ: Ʋu ƒe akpa aɖewo kple kakɛ vovovo bubu siwo ƒe ŋusẽ deŋgɔ tɔxɛ
Nu veviwo: aɖatsi ŋusẽ gã, dɔwɔwɔ nyuie, to nyateƒetoto ofRoHS, REACH, kple LFGB.
 
GA-31×0 Silicone Rubber with High Tear Strength (Fumed Silica) nye elastomer deŋgɔ si wowɔ na dɔwɔƒe siwo hiã be woawɔ dɔ nyuie wu eye wòanɔ anyi eteƒe nadidi. Esi Shanghai Herchy Rubber Co., Ltd. nye silicone rababa deŋgɔ wɔla kple edzrala xɔŋkɔ ta la, eɖoe kplikpaa be yeatsɔ nusiwo sɔ ɖe míaƒe xexeame katã ƒe asisiwo ƒe dzidzenu sesẽwo nu la ana. Míaƒe GA-31×0 silicone rababa naa aɖatsi ƒe ŋusẽ gã, si doa ŋusẽ silica si me dzudzɔ le, si wɔe be wòsɔ nyuie na dɔwɔwɔ siwo bia be woanɔ te ɖe nɔnɔme sesẽwo nu le nuteɖeamedzi kple nɔnɔme sesẽwo me.

Míetrɔ asi le wò hiahiã tɔxɛwo nu, eye míenaa egbɔkpɔnu siwo wowɔ ɖe ɖoɖo nu be míakpɔ egbɔ be wowɔ dɔ nyuie wu na dɔwɔƒe vovovo siwo dometɔ aɖewoe nye ʋuwo, yamenutomeyimɔ̃wo, kple elektrikdɔwo. Ka ɖe míaƒe nunya dzi be míana silicone rababa siwo nɔa anyi didina, siwo wɔa dɔ nyuie, siwo naa asixɔxɔ si nɔa anyi didi.
  • GA-31×0 ƒe ƒuƒoƒo

  • Herchy ƒe ame

Nusiwo Li:
Agbɔsɔsɔ:

GA-31 × 0 Silicone Rubber kple Aɖatsi Ŋusẽ Kɔkɔ (Fumed Silica) - Adzɔnuwo ƒe Numeɖeɖe


Wotrɔ asi le GA-31×0 Silicone rababa ŋu na dɔwɔwɔ siwo wɔa dɔ nyuie. Eƒe nɔnɔme deŋgɔ si te ŋu nɔa te ɖe aɖatsi nu eye wònɔa anyi didina, si wɔe be wòsɔ nyuie na dɔwɔƒe vovovowo. Shanghai Herchy Rubber Co., Ltd., si nye silicone elastomers wɔƒe xɔŋkɔ aɖee wɔa atike sia. Wotsɔa silica si me dzo le do ŋusẽ GA-31×0 ƒe hatsotso la be wòana eƒe aɖatsi ƒe ŋusẽ nadzi ɖe edzi, si wɔnɛ be ewɔa dɔ ɣeyiɣi didi le nɔnɔme sesẽwo me.


Woate ŋu akpɔ atike sia le sesẽme vovovo atɔ̃ me, tso 30 Shore A va ɖo 70 Shore A. Esia naa woate ŋu azãe le mɔ vovovowo nu hena dɔ vovovowo wɔwɔ, tso nutrenu siwo te ŋu trɔna dzi va ɖo akpa siwo sesẽ wu dzi. GA-31×0 ƒe hatsotsoawo hã ƒo adegbe le didime ƒe nɔnɔme nyuiwo ŋu, si wɔnɛ be nusi wotsɔ wɔe la te ŋu kekena le nuteɖeamedzi me evɔ megblẽa eƒe ŋusẽ me o.


Le kpekpeme ƒe didime tso 1.08 g/cm³ va ɖo 1.20 g/cm³, GA-31×0 silicone rababa ƒe kpekpeme le bɔbɔe eye wònɔa anyi didina. Enaa ŋusẽ si nɔa eŋu ɣesiaɣi be wòate ŋu aʋuʋui, si wɔnɛ be wòte ŋu kpɔa mɔ̃wo ƒe nuteɖeamedzi vovovowo gbɔ. Esia na wònye nusi sɔ na ʋuwo, yamenutomeyimɔ̃wo, kple elektrik-mɔ̃wo, afisiwo wòanɔ anyi eteƒe nadidi kple alesi wòate ŋu atrɔ ɖe nɔnɔmewo ŋu le vevie le.


Silicone rababa la ƒe dzedzeme le keklẽm, si wɔnɛ be woate ŋu alé ŋku ɖe eŋu bɔbɔe eye woatsɔe ade nusiwo me kɔ alo esiwo me kɔ afã kple afã me. Ete ŋu nɔa te ɖe nutome ƒe nɔnɔme sesẽwo nu nyuie hã, si wɔe be wòsɔ na gota alo dɔwɔƒewo zazã.


GA-31×0 ƒe hatsotso nye nusiwo ŋu kakaɖedzi le eye wònɔa anyi didina ƒe tiatia na dɔ ɖesiaɖe si bia aɖatsi ƒe ŋusẽ gã kple dɔwɔwɔ nyuie ŋutɔ.


Dodokpɔ: 1% le atike si daa gbe le ame ŋu (50% ƒe atike si wotsɔ DBPMH wɔe le silicone gum me), 175° x5minx15MPa


Nusiwo wowɔ ƒe nɔnɔmewo
Nu si wowɔ GA-3130 ƒe agbalẽa
GA-3140 ƒe agbalẽ GA-3150 ƒe agbalẽa GA-3160 ƒe agbalẽa GA-3170 ƒe agbalẽa
Dzedzeme Nusi me kɔ nyuie
Williamplasticity ƒe dɔwɔwɔ
140
180
210
240
280
Sesẽme (ƑutaA) .
30
40
50
60
70
Eƒe kpekpeme(g/cm3) . 1.08
1.11
1.14
1.17
1.20
Ŋusẽ si wotsɔna ƒoa nu (MPa) .

8
8
9
9
9
Elongation(%) ƒe didime . 900
750
750
650
600
Aɖatsi ƒe ŋusẽ (kN/m) . 30
35
45
45
40


Tabla sia na GA-31×0 series silicone rubber nuwɔna ƒe nɔnɔme veviwo. Vovototo ɖesiaɖe le nusiwo kplɔ wo nɔewo ɖo me naa mɔ̃ɖaŋununya ƒe nɔnɔme vovovowo be wòasɔ ɖe dɔwɔwɔ ƒe hiahiã vovovowo nu. Eɖanye be èhiã be wòate ŋu atrɔ ɖe nɔnɔmewo ŋu, wòanɔ anyi eteƒe nadidi, alo aɖatsi o, GA-31×0 silicone rababa nye egbɔkpɔnu si ŋu kakaɖedzi le.


Silicone rababa si ƒe aɖatsi sesẽ ŋutɔ


GA-31 × 0 Silicone Rubber kple Aɖatsi Ŋusẽ Kɔkɔ (Fumed Silica) Nɔnɔmewo


Wotrɔ asi le GA-31×0 silicone rubber series ŋu be wòana dɔwɔwɔ deŋgɔ si nɔa anyi didina na dɔwɔƒewo ƒe dɔwɔwɔ vovovowo. Nu deŋgɔ sia ƒe nɔnɔme veviwo le ete, si sɔ nyuie na dɔwɔƒe siwo bia nu geɖe abe ʋu ƒe akpa aɖewo, yamenutomeyimɔ̃wo, elektrikŋusẽ ƒe xɔxlɔ̃, kple bubuwo ene.


Aɖatsi ƒe Ŋusẽ Kɔkɔe hena Enɔanyi

GA-31×0 silicone rababa naa aɖatsiwo te ŋu nɔa te ɖe enu etɔxɛe, si wɔe be wònye tiatia nyuitɔ kekeake na akpa siwo hiã be woado dzi le mɔ̃ɖaŋununya ƒe nuteɖeamedzi sesẽwo me. Eƒe aɖatsi ƒe ŋusẽ si de ŋgɔ wu na wòsɔ nyuie na nutrenu siwo ŋu ŋusẽ le ŋutɔ, ʋu ƒe akpa aɖewo, gasketwo, kple dɔwɔƒewo ƒe rababa siwo wodona le nɔnɔme sesẽwo me.


Dɔwɔwɔ ƒe Ŋutete Nyuitɔ Kekeake

Wotrɔ asi le silicone rababa sia ŋu wòte ŋu trɔa asi le eŋu wòɖe dzesi ŋutɔ, si wɔnɛ be woate ŋu atrɔ asi le eŋu ahawɔ eƒe nɔnɔme bɔbɔe. Eɖanye rababa ƒe akpa siwo wowɔ ɖe ɖoɖo nu alo hatsotso gãwo wɔm nèle o, GA-31×0 ƒe dɔwɔwɔ bɔbɔe kpena ɖe ame ŋu be ewɔwɔ ƒe ɣeyiɣi kple gazazã dzi ɖena kpɔtɔna, si wɔe be wònye tiatia si wodi wu na adzɔnuwo wɔwɔ le agbɔsɔsɔ gã me le dɔwɔƒewo abe ʋuwo, yamenutomeyimɔ̃wo, kple atikewɔwɔ ene.


Dukɔwo Dome Dzidzenuwo Dzi Wɔwɔ

GA-31×0 silicone rababa si wɔ ɖeka kple xexeame katã ƒe dzidzenuwo abe RoHS, REACH, kple LFGB ene bliboe, eye wòkpɔa egbɔ be yewɔ ɖe nutome ƒe sewo kple dedienɔnɔ ŋuti ɖaseɖigbalẽwo dzi. Esia na wòsɔ na ʋuwo ƒe nutrenuwo, atikewɔnuwo ƒe akpa aɖewo, kple dɔwɔƒe bubu siwo wɔa se nu ŋutɔ siwo hiã nusiwo ŋu woɖo kpee.


Nusiwo Woate Ŋu Azã le Mɔ Vovovowo Me Le Dɔwɔwɔ Geɖewo Me

GA-31×0 silicone rubber nye esi woate ŋu azã le mɔ vovovowo nu ŋutɔ eye wozãnɛ geɖe le dɔwɔƒewo abe ʋuwo wɔwɔ, yamenutomeyimɔ̃wo, elektrɔnikmɔ̃wo, kple atikewɔnuwo ene me. Eƒe dɔwɔwɔ nyuie ƒe nɔnɔmewo, siwo dometɔ aɖewoe nye dzoxɔxɔ ƒe liƒo, atikewo ƒe tsitretsitsi, kple asitɔtrɔ le nɔnɔmewo ŋu, na wòsɔ nyuie na nutrenu, gasket, nusiwo xea mɔ na dzoxɔxɔ, kple nu vevi bubuwo le nɔnɔme sesẽwo me.


Sesẽme Tiatia Siwo Woate Ŋu Atrɔ Asi Le

Woate ŋu atrɔ asi le GA-31×0 silicone rababa ŋu le sesẽme ƒe tiatia vovovowo me tso 30 va ɖo 70 Shore A, eye woate ŋu atrɔ asi le eŋu wòasɔ ɖe wò dɔwɔwɔ ƒe nudidi tɔxɛwo nu. Eɖanye be èhiã rababa si te ŋu trɔna bɔbɔe alo elastomer si sesẽ wu o, GA-31×0 naa egbɔkpɔnu si woate ŋu atrɔ asi le na dɔwɔƒe vovovowo abe ʋuwo kple elektrik-mɔ̃wo ene.


Didime Kple Trɔtrɔ Ðe Nɔnɔmewo Ŋu Tɔxɛ

Le didime ƒe nɔnɔme wɔdɔɖeamedziwo ta la, GA-31×0 silicone rababa ate ŋu akeke vaseɖe 900% evɔ magblẽ ŋusẽ me o. Esia na wòsɔ nyuie na akpa siwo hiã be woate ŋu atrɔ ɖe nɔnɔmewo ŋu ahanɔ te ɖe nɔnɔme sesẽwo nu, abe nutrenu ƒe asigɛwo, gasketwo, kple akpa siwo hiã be woado dzi le mɔ̃wo ƒe teteɖeanyi me le nɔnɔme siwo bia be woate ŋu atrɔ ɖe nɔnɔmewo ŋu ŋutɔ me.


Ete ŋu nɔa te ɖe nɔnɔme sesẽwo nu

GA-31×0 silicone rababa wɔa dɔ nyuie le nɔnɔme sesẽwo me, siwo dometɔ aɖewoe nye dzoxɔxɔ gã kple UV keklẽ, ozone, kple atikewo ƒe dodo. Enyo ŋutɔ na dɔ siwo me dɔwɔwɔ si nɔa anyi didi le vevie le, abe gota nutrenu, ʋu ƒe akpa aɖewo, kple yamenutome ƒe akpa aɖewo ene.


Dzedzeme si me kɔ nyuie hena Kakaɖedzi le eƒe nyonyome ŋu

GA-31×0 silicone rubber ƒe dzedzeme si me kɔ nyuie la wɔnɛ be woate ŋu alé ŋku ɖe eŋu bɔbɔe le ewɔwɔ me, si kpena ɖe ame ŋu be woakpɔ egbɔ be akpa ɖesiaɖe ɖo nyonyomedzikpɔkpɔ ƒe dzidzenu kɔkɔtɔwo gbɔ. Nuwɔwɔ le gaglãgbe alea na wòɖea vi ŋutɔ le dɔwɔƒewo abe elektrɔnikmɔ̃wo kple atikewɔnuwo ene afisiwo nuwɔwɔ pɛpɛpɛ kple nuwɔwɔ ɖekae nye nu vevitɔ le.


Nyabiase Kple Ŋuɖoɖo Siwo Wobia Enuenu

Q1: Dɔwɔƒe kawoe zãa GA-31 × 0 Silicone Rubber kple Aɖatsi ƒe Ŋusẽ Kɔkɔ?
A1: GA-31 × 0 sɔ nyuie na ʋu, yamenutome, elektrɔnikmɔ̃wo, atikewɔnuwo, kple dɔwɔƒewo.


Q2: Ðe woate ŋu atrɔ asi le GA-31 × 0 Silicone Rubber ŋu ​​na dɔ tɔxɛ aɖewo wɔwɔa?
A2: Ẽ, míenaa silicone rababa solutions siwo wowɔ ɖe ɖoɖo nu le sesẽme, wɔwɔme, kple amadede me na dɔwɔƒe vovovowo.


Q3: Aleke GA-31×0 Silicone Rubber wɔa dɔ le dzoxɔxɔ si gbɔ eme me?
A3: GA-31 × 0 silicone rababa naa dzoxɔxɔ ƒe liƒo gã, si sɔ nyuie na dzoxɔxɔ gã nutrenu kple gaskets.


Q4: Ðaseɖigbalẽ kawoe GA-31×0 Silicone Rubber ɖo?
A4: GA-31×0 silicone rababa wɔ ɖeka kple RoHS, REACH, kple LFGB, si naa kakaɖedzi be dzidzenu siwo me gblẽa nu le nutome ŋu o.


Q5: Viɖe vevi kawoe le GA-31×0 Silicone Rubber zazã me?
A5: GA-31 × 0 naa aɖatsi ƒe ŋusẽ gã, asitɔtrɔ le nɔnɔmewo ŋu nyuie ŋutɔ, kple atikewo ƒe tsitretsitsi ɖedzesi aɖe na dɔwɔƒewo zazã.


Q6: Ðe GA-31 × 0 Silicone Rubber sɔ na ʋu ƒe nutrenu dɔwo?
A6: Ẽ, esɔ nyuie na ʋu ƒe nutrenuwo, gaskets, kple rababa ƒe akpa siwo wɔa dɔ nyuie le ʋuwo wɔwɔ me.


Q7: Aleke gbegbee GA-31×0 Silicone Rubber te ŋu nɔa te ɖe atikewo kple UV keklẽ nu?
A7: GA-31 × 0 naa atikewo ƒe tsitretsitsi sesẽ kple UV liƒo, si wɔe be wòsɔ nyuie na gota kple ʋu ƒe rababa ƒe akpawo.


Q8: Ðe woate ŋu azã GA-31×0 Silicone Rubber le atikewɔnuwo mea?
A8: Ẽ, GA-31 × 0 ɖoa dedienɔnɔ ƒe ɖaseɖigbalẽwo gbɔ eye wòsɔ nyuie na atikewɔnuwo ƒe akpa aɖewo kple atikewɔwɔ-grade rababa dɔwo.

Si do ŋgᴐ: 
Esi kplᴐe ɖo: 

NYAGBLƆÐI KABAWO

MÍAƑE NUWO ƑE NUWO

NYATAKAKA SIWO WOÐO BE WOAÐO BE WOAÐE KPƆKPƆ

Tsɔ kpe ɖe eŋu: No.33, Mɔdodo 159, Taiye Mɔ dzi, Fengxian Nutome, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nutata ƒe Gomenɔamesi     2023 Shanghai Herchy Rubber Co., Ltd. Nyatakakadzraɖoƒe ƒe Nɔnɔmetata |   Ameŋunyatakakawo Ŋuti Ðoɖo | Kpekpeɖeŋu To Leadong ƒe agbalẽ.