GA-32 × 0 General cholinga silikoni rabala (fumed silika) (HCR)

Ntchito: oyenera kupanga mitundu yonse ya m'chimake, kitchenware, kachikwama, wotchi ndi zinthu zina ochiritsira.
Zofunika kwambiri: kuchiritsa mwachangu, mphamvu yayikulu, kusinthika kwabwino, kupititsa kutsimikizika kwa RoHS, REACH, ndi LFGB.
 
Shanghai Herchy Rubber Co., Ltd ndiwopanga zinthu zapamwamba kwambiri za mphira wa silikoni. Timakhala okhazikika popereka njira zingapo zopangira mphira za silicone zomwe zimasinthidwa kuti zikwaniritse zosowa zanu. Ndiukadaulo wapamwamba wopanga komanso gulu la akatswiri, timapereka zida zapamwamba za silikoni zomwe zimakhala zolimba, zosinthika, komanso zomwe zimakwaniritsa miyezo yapamwamba kwambiri yamakampani. Titumizireni zomwe mukufuna lero, ndipo tidzakupatsani yankho labwino pakugwiritsa ntchito kwanu.
  • GA-32 × 0

  • Herchy

Zida:
kupezeka:
Kuchuluka:

GA-32 × 0 General Purpose Silicone Rubber (Fumed Silica) Kufotokozera Kwazinthu


GA-32 × 0 General Purpose Silicone Rubber, yopangidwa ndi Shanghai Herchy Rubber Co., Ltd, idapangidwa kuti ikwaniritse zosowa zamakampani osiyanasiyana. Ndi magiredi osiyanasiyana, kuphatikiza GA-3230 mpaka GA-3280, imapereka magwiridwe antchito osiyanasiyana pamapulogalamu osiyanasiyana. Rabara ya silikoni yochita bwino kwambiri iyi ndi yabwino kusindikiza, kuyika gasket, komanso kutchinjiriza m'mafakitale osiyanasiyana monga zamagalimoto, zamagetsi, ndi zomangamanga.


Rabara ya silica silikoni yofukiza iyi imawonetsa kusinthasintha kwabwino komanso kulimba, ndikupangitsa kuti ikhale yoyenera madera onse otentha komanso otsika. Amapereka mphamvu zolimba zolimba, kutalika, komanso kukana misozi, kuwonetsetsa kuti zimagwira ntchito kwanthawi yayitali ngakhale pazovuta. Amagwiritsidwa ntchito kwambiri pamapulogalamu omwe amafunikira kusinthasintha komanso mphamvu, monga zosindikizira za silicone, ma gaskets a silicone, ndi zida za elastomeric.


Rabara ya silikoni yowoneka bwino imapezeka m'magawo osiyanasiyana olimba, kuyambira 30 Shore A mpaka 80 Shore A, kukupatsani mwayi wosankha giredi yoyenera kwambiri pazosowa zanu. Ndi kachulukidwe kosiyanasiyana komanso kulimba kwamphamvu, mndandanda wa GA-32 × 0 ukhoza kusinthidwa kuti ugwiritse ntchito zosiyanasiyana zamafakitale ndi zamalonda.


Mndandanda wa GA-32 × 0 ndi wosunthika kwambiri, ndikupangitsa kukhala chisankho chabwino pamayankho a rabara a silicone. Kaya mukufuna mphira wa silikoni wosinthika wazigawo zamagalimoto, zamagetsi, kapena zomangira, chogulitsirachi chimapereka magwiridwe antchito apamwamba pamagwiritsidwe osiyanasiyana.


Mayeso: 1% ya mankhwala ochiritsira (50% phala la DBPMH mu chingamu cha silicone), 175 ° x 5min x 15MPa.


Table ya Parameter


Zogulitsa katundu
Zogulitsa GA-3230
GA-3240 GA-3250 GA-3260 GA-3270 GA-3280
Maonekedwe Zowoneka bwino
Williamplasticity
140
180
210
240
280
310
Kuuma (ShoreA)
30
40
50
60
70
80
Kachulukidwe (g/cm3) 1.08
1.11
1.14
1.17
1.20
1.22
Tensilestrength (MPa)

9
9.5
11
10.5
10.5
9
Kutalikira (%) 900
700
650
600
450
350
Mphamvu ya misozi (kN/m) 18
22
25
30
30
30

Ndi mndandanda wa GA-32 × 0 General Purpose Silicone Rubber, mumapeza mayankho odalirika, osinthika makonda pazogwiritsa ntchito zosiyanasiyana zamafakitale. Kaya mukuyang'ana labala ya silikoni yopangira, labala ya silikoni yong'ambika kwambiri, kapena zida zosunthika zomata, zogulitsa zathu zimapereka magwiridwe antchito abwino kwambiri pamsika.


Lumikizanani nafe lero kuti mukambirane zomwe mukufuna polojekiti yanu, ndipo tidzasintha mphira wabwino wa silikoni wa HCR kuti agwirizane ndi zosowa zanu.


General Purpose Silicone Rubber Series

GA-32 × 0 General Purpose Silicone Rubber Features


GA-32 × 0 General Purpose Silicone Rubber, yomwe ili ndi silika ya fumed, ndi chinthu chosunthika chomwe chili choyenera pakugwiritsa ntchito mafakitale osiyanasiyana. Zimapereka magwiridwe antchito apamwamba ndipo zimadaliridwa ndi mafakitale omwe amafunikira ma elastomer olimba komanso osinthika. Pansipa pali zinthu zazikulu zomwe zimapangitsa GA-32 × 0 kukhala chisankho chodalirika.


Zosiyanasiyana Mapulogalamu

GA-32 × 0 amagwiritsidwa ntchito popanga zinthu zosiyanasiyana za mphira za silikoni monga zosindikizira, ma gaskets, ndi zokutira zoteteza. Ndiwothandiza makamaka m'mafakitale monga opanga magalimoto, zamagetsi, ndi zinthu zogula, zomwe zimapangitsa kukhala chisankho chodziwika bwino pamagwiritsidwe ntchito wamba.


Kuthamanga Kwachangu Kwambiri

Rabara ya silicone iyi imawonetsa nthawi yochiritsa mwachangu, kupititsa patsogolo kupanga komanso kuchepetsa nthawi yopuma. Kaya mukupanga zida za silikoni zosindikizira zamagalimoto kapena zotsekera zamagetsi, GA-32 × 0 imapereka machiritso mwachangu kuti akwaniritse madongosolo opanga omwe amafuna kwambiri.


Kuthamanga Kwambiri Kwambiri

GA-32 × 0 imapereka mphamvu yokhazikika yokhazikika, kuwonetsetsa kuti ikugwira ntchito kwanthawi yayitali pamapulogalamu ovuta. Katunduyu amapangitsa kuti ikhale yabwino kwa magawo omwe amakumana ndi zovuta zamakina, monga zosindikizira, ma gaskets, ndi zophimba zoteteza.


Kuchita Kwabwino Kwambiri Kwambiri

Kusavuta kwa kukonza kumapangitsa GA-32 × 0 kukhala yoyenera pamitundu yosiyanasiyana ya nkhungu. Mawonekedwe ake oyenda bwino amatsimikizira zotsatira zosasinthika ndi zinthu zapamwamba kwambiri, zoyenera pazochita zonse komanso kupanga zambiri.


Kutsata Miyezo Yadziko Lonse

GA-32 × 0 mphira wa silikoni umakwaniritsa zofunikira zoyendetsera mayiko monga RoHS, REACH, ndi LFGB certification. Zitsimikizozi zimatsimikizira kuti zinthuzo ndi zotetezeka kuti zigwiritsidwe ntchito pazakudya, zida zamankhwala, ndi zinthu zomwe zimafunikira kutsatiridwa mosamalitsa.


Mphamvu Yowonjezera ya Misozi

GA-32 × 0 imawonetsa mphamvu zong'ambika modabwitsa, kuwonetsetsa kulimba ngakhale pamavuto. Ndizoyenera makamaka zisindikizo za mafakitale ndi zinthu zina zomwe zimafunika kupirira nthawi zonse zowonongeka.


Kukaniza Kwabwino Kwambiri komanso Kutentha Kwambiri

GA-32 × 0 imalimbana kwambiri ndi kutentha kwambiri, kusunga umphumphu wake pamatenthedwe osiyanasiyana. Izi zimapangitsa kuti zikhale zoyenera kugwiritsidwa ntchito ngati zida zamagalimoto, zakuthambo, ndi zamagetsi, komwe kukhazikika kwapamwamba komanso kotsika ndikofunikira.


Magiredi Omwe Mungasinthire Pazofuna Zachindunji

Ndi mitundu yosiyanasiyana ya kuuma, GA-32 × 0 ikhoza kukhala yogwirizana ndi zosowa zanu. Kaya mukuyang'ana elastomer yofewa yosindikizira kapena giredi yolimba ya ma gaskets, labala ya silikoni iyi imatha kusinthidwa kuti ikwaniritse zomwe mukufuna.


Shanghai Herchy Rubber Co., Ltd. ndiwopanga komanso ogulitsa mphira wa silikoni ndi zinthu zina za elastomer. Poyang'ana kwambiri zida zapamwamba, timagwira ntchito m'mafakitale monga zamagalimoto, zamlengalenga, zamankhwala, ndi zinthu zogula. Gulu lathu lodziwa zambiri limatsimikizira kuti mankhwala aliwonse amakwaniritsa miyezo yapamwamba kwambiri ya khalidwe ndi ntchito, kuthandiza makasitomala athu kukwaniritsa zolinga zawo ndi mayankho odalirika. Kaya mukuyang'ana zosakaniza za silikoni, zopangira makonda, kapena gulu linalake la mphira, timapereka mayankho osinthika komanso ogwirizana ndi zosowa zanu zabizinesi.


Ku Shanghai Herchy Rubber Co., Ltd., tadzipereka kupereka zabwino komanso zatsopano, kuwonetsetsa kuti zinthu zathu zonse, kuphatikiza GA-32 × 0, zikukwaniritsa zomwe mukufuna ndikuthandizira kuyendetsa bizinesi yanu patsogolo.

Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.