245
SABIC na ɔkyerɛwee
SABIC EPDM 245 na ɛwɔ hɔ
| Availability: | |
|---|---|
| Quantity: | |
AGYADEƐ HO NKYERƐKYERƐMU:
| AGYAPADEƐ | NKYERƐKYERƐMU A ƐTƆ SO | NKYEKYƐMU | AKWAN A WƆFA SO YƐ SƆHWƐ |
| POLYMER NSƐM A ƐYƐ NSƐM | |||
| Mooney a ɛyɛ den | |||
| ML 1+4, 125 °C (1) . | 25 |
MU |
ASTMD 1646 na ɛwɔ hɔ |
| Ethylene a Ɛwɔ Mu | 40 |
wt.% . |
ASTMD 3900 na ɛwɔ hɔ |
| Ethylidene Norbornene (ENB) Nneɛma a ɛwɔ mu | 4.5 |
wt.% . | ASTMD 6047 na ɛwɔ hɔ |
ESU:
SABIC EPDM 245 yɛ nea wɔayɛ ama : processability a ɛkyɛn so a ɛde afrafra ne molding bere tiaa ba, ɔhyew a ɛba fam su pa, ɔhyew a ɛba fam yiye a ɛyɛ mmerɛw ne compression set, ntɛmntɛm ayaresa rate ne high cure tebea. NKYERƐKYERƐMU NE NEA WƆDE DI DWUMA:
Ɛsɛ sɛ wɔde SABIC EPDM 245 sie nea wɔde ahyɛ mu mfiase no mu wɔ baabi a ɛhɔ yɛ hyew wɔ tebea a ɛyɛ kusuu mu; ɛsɛ sɛ wɔkwati ɔhyew, ultraviolet hann ne owia hann tẽẽ a wɔde bɛhyɛ mu. Wɔ tebea horow a ɛfata a wɔde sie mu no, ade no gyina hɔ pintinn asram 24 fi da a wɔyɛɛ no. SABIC rentrɛw ne warranty mu bere a tebea a wɔde sie no nyɛ nea ɛfata a ebetumi ama nneɛma asɛe te sɛ nneɛma a ɛyɛ den anaa kɔla a ɛbɛsakra a ebetumi ama nneɛma no anyɛ adwuma yiye..
NKYERƐKYERƐMU:
Adetɔn biara a SABIC, ne nnwumakuw nketewa ne wɔn a wɔka ho (biara yɛ 'ɔtɔnfo'), yɛ adetɔn biara wɔ adetɔnfo no adetɔn ho nhyehyɛe a wɔahyɛ da ayɛ no mu nkutoo (a wobetumi anya bere a wɔabisa) gye sɛ wɔakyerɛw apene so sɛ wɔkyerɛw na wɔde wɔn nsa ahyɛ ase wɔ adetɔnfo no ananmu. Bere a wɔde adwempa na ɛde nsɛm a ɛwɔ ha no ama no, ƆDONDENFO NO MMA MMƆDENBƆ BIARA, WƆADA MU ANAA WƆAKYERƐW, A ADWUMA A WƆDE DI DWUMA NE AKWANKYERƐ NE WƆMMA MMƆDENBƆ KA HO, NA MMƆ ASOBƆ BIARA, TƐNEE ANAA ƐNKYERƐKYERƐMU, A ƐFA ADWUMA, AKWANKYERƐ HO ANAA ƐFATA SƐ WƆDE DI DWUMA ANAA BOTAE A WƆDE BƐDI DWUMA ANAA ATIRIMKA A WƆDE BƐDI DWUMA WƆ AKWANKYERƐ BIARA MU. Ɛsɛ sɛ adetɔfoɔ biara nam sɔhwɛ ne nhwehwɛmu a ɛfata so kyerɛ sɛ nneɛma a wɔtɔn no fata ma adetɔfoɔ no dwumadie pɔtee. Asɛm biara a nea ɔtɔn no kae a ɛfa sɛnea wobetumi de ade, adwuma anaa adwini biara adi dwuma ho no atirimpɔw, anaasɛ ɛsɛ sɛ wɔkyerɛ ase, sɛ ɛbɛma tumi krataa biara wɔ tumi krataa anaa adwene mu agyapade hokwan foforo biara ase.