SABIC® EPDM 245

ʻO SABIC EPDM 245 kahi haʻahaʻa haʻahaʻa mooney viscosity, haʻahaʻa ethylene a me medium ENB content grade i hana ʻia e ka polymerization solution me ka hoʻohana ʻana i ka metallocene catalyst. He polimer amorphous me ka puunaue kaumaha molekala. Hiki ke hoʻohana ʻia e like me ka plasticizer polymeric i hui pū me nā polymers viscosity kiʻekiʻe. Loaʻa kēia māka i nā bale friable.
Hiki ke hoʻohana ʻia ka SABIC EPDM 245 no: nā ʻāpana haʻihaʻi, nā sila kikoʻī, nā gaskets, nā ʻūhā i hoʻoheheʻe ʻia, nā mea hoʻohui uila, nā ʻatikala i hoʻoheheʻe ʻia
  • 245

  • SABIC

  • SABIC EPDM 245

Loaʻa:
Nui:

NUI WAIWAI MAU:

NA WAIWAI NA WAIWAI MAU NA UNIT NA HANA HO'O
NA WAIWAI POLYMER


Mooney viscosity


ML 1+4, 125 °C (1) 25
MU
ASTMD 1646
Ethylene maʻiʻo 40
wt.%
ASTMD 3900
Ethylidene Norbornene (ENB). 4.5
wt.% ASTMD 6047

ANOAI:

Hoʻolālā ʻia ʻo SABIC EPDM 245 no: hiki ke hoʻoponopono maikaʻi i ka hopena o ka hui ʻana a me ka manawa hoʻoheheʻe ʻia, nā waiwai haʻahaʻa haʻahaʻa haʻahaʻa maikaʻi, maikaʻi haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa a me ka hoʻonohonoho paʻa ʻana, wikiwiki ka lāʻau lapaʻau a me ke kūlana hoʻōla kiʻekiʻe. Hoʻopaʻa a me ka lawelawe ʻana:

Pono e mālama ʻia ʻo SABIC EPDM 245 i loko o kāna ʻeke kumu ma ka mahana ambient i nā kūlana maloʻo; ʻO ka ʻike ʻana i ka wela, ke kukui ultraviolet a me ka mālamalama o ka lā pono e pale ʻia. Ma lalo o nā kūlana mālama kūpono, paʻa ka huahana no 24 mau mahina mai ka lā i hana ʻia ai. ʻAʻole e hoʻolōʻihi ʻo SABIC i kāna palapala hōʻoia inā ʻaʻole lawa nā kūlana mālama e alakaʻi i ka pōʻino o ka maikaʻi e like me ka paʻakikī o nā mea a i ʻole ka hoʻololi ʻana i ka waihoʻoluʻu e hiki ke hopena i ka hana ʻole o ka huahana.

HOOLAHA:

 ʻO ke kūʻai aku ʻana e SABIC, kāna mau lālā a me nā mea pili (ʻo kēlā me kēia 'mea kūʻai aku'), e kūʻai wale ʻia ma lalo o nā kūlana kūʻai maʻamau o ka mea kūʻai aku (loaʻa ma ke noi ʻana) ke ʻole i ʻae ʻia ma ke kākau ʻana a kau inoa ʻia ma ka inoa o ka mea kūʻai aku. ʻOiai ua hāʻawi ʻia ka ʻike i loko o kēia me ka manaʻo maikaʻi, ʻaʻohe mea kūʻai aku i palapala hōʻoia, i hōʻike ʻia a i ʻole i hoʻohālikelike ʻia, e komo pū me ke kālepa a me ka hōʻino ʻole ʻana i ka waiwai noʻonoʻo, ʻaʻole i manaʻo i kekahi kuleana, pololei a i ʻole pololei ʻole, e pili ana i ka hana no ka hana, kūpono. KE KUMU O KEIA MAU HANA MA KEKAHI PILI. Pono kēlā me kēia mea kūʻai aku e hoʻoholo i ke kūpono o nā mea kūʻai aku no ka hoʻohana pono ʻana o ka mea kūʻai aku ma o ka hoʻāʻo ʻana a me ka nānā ʻana. ʻAʻohe ʻōlelo a ka mea kūʻai aku e pili ana i ka hoʻohana ʻana i kekahi huahana, lawelawe a hoʻolālā paha i manaʻo ʻia, a i ʻole e manaʻo ʻia, e hāʻawi i kekahi laikini ma lalo o kekahi patent a i ʻole nā ​​​​kuleana waiwai naʻauao.

Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.