SABIC® EPDM 245

I-SABIC EPDM 245 iyi-mooney viscosity ephansi, i-ethylene ephansi kanye nebanga lokuqukethwe le-ENB eliphakathi elikhiqizwe i-polymerization yesisombululo kusetshenziswa i-metallocene catalyst. Kuyi-polymer e-amorphous enokusabalalisa kwesisindo samangqamuzana aphakathi. Ingasetshenziswa njenge-plasticizer ye-polymeric ehlanganiswe namanye ama-polymers aphezulu we-viscosity. Leli banga litholakala ngamabhala atholakalayo.
I-SABIC EPDM 245 ingasetshenziselwa: izingxenye zamabhuleki, ama-precision seal, ama-gaskets, amashidi egwebu abunjiwe, izixhumi zikagesi, ezinye izindatshana ezibunjiwe
  • 245

  • SABIC

  • SABIC EPDM 245

Ukutholakala:
Ubuningi:

IZIMALI EZIJWAYELEKILE ZEMPAHLA:

IZIMPAHLA IZIMALI EZIJWAYELEKILE AMANYE IZINDLELA ZOKUHLOLA
IMPAHLA YEPOLYMER


I-Money viscosity


I-ML 1+4, 125 °C (1) 25
MU
I-ASTMD 1646
Okuqukethwe kwe-Ethylene 40
wt.%
I-ASTMD 3900
I-Ethylidene Norbornene (ENB) Okuqukethwe 4.5
wt.% I-ASTMD 6047

IZIMPAWU:

I-SABIC EPDM 245 iklanyelwe: ukucutshungulwa okuhle kakhulu okuholela ekuxubeni okufushane kanye nezikhathi zokubumba, izici ezinhle zokushisa eziphansi, ukuguquguquka okuhle kwezinga lokushisa eliphansi kanye nesethi yokucindezela, izinga lokwelapha ngokushesha kanye nesimo sokwelapha esiphezulu. UKUGCINA NOKUPHATHA:

I-SABIC EPDM 245 kufanele igcinwe ekupakishweni kwayo kwasekuqaleni ezingeni lokushisa elizungezile ezimeni ezomile; ukuchayeka ekushiseni, ukukhanya kwe-ultraviolet nokukhanya kwelanga okuqondile kufanele kugwenywe. Ngaphansi kwezimo ezifanele zokugcinwa, umkhiqizo uzinzile izinyanga ezingama-24 kusukela ngosuku owenziwe ngalo. I-SABIC ngeke yandise iwaranti yayo uma izimo zokulondoloza zinganele okungase kuholele ekuwohlokeni kwekhwalithi njengokuqina kwezinto ezibonakalayo noma ukushintsha kombala okungase kubangele ukusebenza kahle komkhiqizo.

UMUZI wokuzihlangula:

 Noma yikuphi ukudayiswa kwe-SABIC, izinkampani ezingaphansi kwayo kanye nezinkampani ezingaphansi kwayo ('umdayisi'), kwenziwa ngokukhethekile ngaphansi kwemibandela yokuthengisa evamile yomthengisi (etholakala uma kunesicelo) ngaphandle uma kuvunyelwene ngenye indlela ngokubhaliwe futhi kwasayinwa egameni lomthengisi. Nakuba ulwazi oluqukethwe lapha lunikezwe ngokwethembeka, umdayisi akenzi ISIQINISEKISO, OKUCAMILEYO NOMA OKUSHIWO, KUHLANGANISA UKUTHENGISA KANYE NOKUNGEPHULI KWEMPAHLA EHLAKANIPHILE, FUTHI AKATHATHI ISIBOPHO, ESIQONDILE NOMA OKUNGABI NAKHO, NGENHLONIPHO, NGENHLONIPHO, NGENXA YOKUHLONIPHA UKUSETSHENZISWA OKUHLOSIWE NOMA INHLOSO YALE MIKHIQIZO KUNOMA YILUPHI ISICELO. Ikhasimende ngalinye kufanele linqume ukufaneleka kwezinto zomdayisi ukuze zisetshenziswe ngokukhethekile yikhasimende ngokuhlolwa nokuhlaziya okufanele. Asikho isitatimende somthengisi esimayelana nokusetshenziswa okungenzeka kwanoma yimuphi umkhiqizo, isevisi noma umklamo esihloselwe, noma okufanele sihunyushwe, ukunikeza noma iyiphi ilayisensi ngaphansi kwanoma yiliphi ilungelo lobunikazi noma elinye ilungelo lempahla yengqondo.

Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai