SAIC® EPDM 245

SABIC EPDM 245 waa muraayad mooney hooseeya, ethylene hooseeya iyo heerka nuxurka dhexdhexaadka ah ee ENB oo ay soo saartay xalalka polymerization iyadoo la isticmaalayo kicinta metallocene. Waa polymer amorphous leh qaybinta miisaanka kelli dhexdhexaad ah. Waxaa loo isticmaali karaa sidii balaastiiste polymeric ah oo lagu daro polymers kale oo viscosity sare leh. Darajadan waxaa lagu heli karaa baalyo la shiilay.
SABIC EPDM 245 waxa loo isticmaali karaa: Qaybaha biriiga, shaabadaynta saxda ah, gaskets, xaashida xumbo ka samaysan, xidhidhiyeyaasha korantada, agabyada kale ee la qaabeeyey
  • 245

  • SABIC

  • SAIC EPDM 245

Helitaanka:
Tirada:

qiyamka hantida caadiga ah:

HANTIDA qiyamka caadiga ah UNITS HABKA IMTIXAANKA
HANTIDA POLYMERKA


Muunsanaanta Mooney


ML 1+4, 125 °C (1) 25
MU
ASTMD 1646
Waxyaabaha Ethylene 40
wt.%
ASTMD 3900
Waxa ku jira Ethylidene Norbornene (ENB) 4.5
wt.% ASTMD 6047

Tilmaamaha:

SABIC EPDM 245 waxaa loogu talagalay: habsocod heer sare ah oo keenaysa isku darka gaaban iyo waqtiyada qaabeynta, sifooyinka heerkul hoose oo wanaagsan, dabacsanaan heerkul hoose oo wanaagsan iyo dejin cadaadis, heerka daawaynta degdega ah iyo xaalad daawo sare leh. KAYDKA IYO MAAREYNTA:

SABIC EPDM 245 waa in lagu kaydiyaa baakaddeedii asalka ahayd heerkulka deegaanka ee xaaladaha qalalan; Soo-gaadhista kulaylka, iftiinka ultraviolet iyo iftiinka qorraxda tooska ah waa in laga fogaado. Marka la eego xaaladaha kaydinta ku habboon, alaabtu waxay ku xasilloon tahay 24 bilood laga bilaabo taariikhda la soo saaray. SABIC ma kordhin doonto dammaanad qaadkeeda marka xaaladaha kaydinta ay ku filnaan waayaan taas oo u horseedi karta xumaanta tayada sida adkaynta walxaha ama isbeddelka midabka taas oo keeni karta wax qabad aan ku filnayn.

AFEEF:

 Iibin kasta oo ay SABIC, la-hawlgalayaasheeda iyo la-hawlgalayaasheeda (mid walba 'iibiyaha'), waxaa lagu sameeyay si gaar ah iyada oo la raacayo shuruudaha caadiga ah ee iibka (la heli karo haddii la codsado) haddii aan si kale loogu heshiin oo qoraal ah oo loo saxiixo magaca iibiyaha. Iyadoo xogta ku jirta halkan lagu bixiyo si niyad sami ah, Iibiyuhu ma Sameeyo dammaanad, CAD AMA DARAN, oo ay ku jiraan baayacmushtar iyo la'aanta hantida caqliga LOOGU TALAGALAY ISTICMAALKA AMA UJEEDADA ALAHAAN ARJIGA KASTA. Macaamiil kastaa waa inuu go'aamiyaa ku habboonaanta agabka iibiyaha ee isticmaalka gaarka ah ee macaamilka iyada oo loo marayo baaritaan iyo falanqayn ku habboon. Ma jiro bayaan ka soo baxay iibiyaha oo ku saabsan isticmaalka suurtogalka ah ee badeecad kasta, adeeg ama naqshad kasta oo loogu talagalay, ama waa in la micneeyaa, si loo bixiyo shati kasta oo hoos timaada shati kasta ama xuquuqda kale ee hantida garaadka.

Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.