Mmala: Mmala (o ka tloaeleha)
ponahalo: Li-blocks kapa li-strip (customizable)
Mofuta oa vulcanization:Sulfur
Mooney viscosity ML(1+4)100℃:65-75
Hardness:60±5 Shore A
Tensile strength:min.10 Mpa
Elongation at break:min.300 Mpa date
:
one Expi month: one Expie month:
Mmala: Mmala (o ka tloaeleha)
chebahalo: Li-blocks kapa li-strip (customizable)
Mofuta oa vulcanization:Sulfur
Mooney viscosity ML(1+4)100℃:75-85
Hardness:60±5 Shore A
Tensile strength:min.10 Mpa
Elongation at break:min.300 Mpa date
:
one Expi month: one Expie month: