Humilis densitas Sigilla Ethylene Propylene Diene Monomer-EPDM
Color: Black(customizable)
appearance:Blocks or stripes (customizable)
Vulcanization type:peroxide
Mooney viscosity ML(1+4) 100℃:65-75
Hardness:60±5 Litus
tensile strength:min.10 Mpa
Elongation at break:min.300%
MOQ: 150kg
Expiration date: Three months