Ponahalo le boemo: bosoeu (bo bonaletsang kapa bo feto-fetohang) blocky
Mofuta oa boraro oa monomer le litaba: ENB, 2.0%
Likahare tsa ethylene: 62%
Mooney viscosity: ML (1+4) 125 ° C 53
Boholo: 25kg / thibela
MOQ: 25kg
Ho paka: lebokose
Ponahalo le boemo: bosoeu (bo bonaletsang kapa bo hlakileng) granular
Mofuta oa boraro oa monomer le litaba: ENB, 4%
Likahare tsa ethylene: 68.5%
Mooney viscosity: ML (1+4) 125 °C 70
Boholo: 25kg / mokotla
MOQ: 25kg
Ho paka: lebokose
Ponahalo le boemo: bosoeu (bo bonaletsang kapa bo feto-fetohang) blocky
Mofuta oa boraro oa monomer le litaba: ENB, 7%
Likahare tsa ethylene: 52%
Mooney viscosity: ML (1+4) 100 ° C 45
Boholo: 25kg / mokotla
MOQ: 25kg
Ho paka: lebokose