Heat Resistant Hoses Ethylene Propylene Diene Monomer-EPDM
Tae: Pango(ka taea te whakarite)
te ahua: Poraka, takai ranei (ka taea te whakarite)
Momo whakangao: Sulfur
Mooney viscosity ML(1+4)100℃:55-65
Te pakeke:60±5 Shore A
Te kaha Tensile:min.10 Mpa
Te whakaroa i te wehenga:min.300%
MoQ: 1000% MOQ
: Min.