Ma hoses Osagwira Kutentha Ethylene Propylene Diene Monomer-EPDM
Mtundu: Wakuda (customizable)
maonekedwe:Ma blocks kapena mizere (customizable)
mtundu wa Vulcanization:Sulfur
Mooney viscosity ML(1+4)100℃:55-65
Kulimba:60±5 M'mphepete mwa nyanja A
Mphamvu yolimba:min.10 Mpa
Elongation panthawi yopuma:min.300 Mpa
deti:
tsiku limodzi: MOQ imodzi Expi