Heat Resistant Hoses Ethylene Propylene Diene Monomer-EPDM
Kulay: Itim(nako-customize)
hitsura:Mga bloke o strip (nako-customize)
Uri ng Vulcanization:Sulfur
Mooney lagkit ML(1+4)100℃:55-65
Hardness:60±5 Shore A
Tensile strength:min.10 Mpa
Elongation at break:min.300%
MOQ:
ration date: 1 month Expiration