Uri hano: Murugo » Amakuru » Amakuru » Ingaruka za okiside ya zinc na magnesium oxyde kumiterere ya peroxide yanduye HNBR

Ingaruka ya okiside ya zinc na magnesium oxyde kumiterere ya peroxide yanduye HNBR

Reba: 0     Umwanditsi: Muhinduzi wurubuga Gutangaza Igihe: 2023-08-15 Inkomoko: Urubuga

Baza

Nka kimwe mu bikoresho bya mbere byakoreshwaga mu nganda za reberi, uruhare rwa okiside ya zinc yagiye ihinduka hamwe n’iterambere rya tekinoroji.

Kuva muburyo bwambere bwo gusiga amabara, imbaraga zongerera imbaraga sisitemu ya volcanisation irashobora kugabanya igihe cyibirunga cyumukozi ukora, chloroprene reberi na carboxy reberi muri agent ya volcanizing, imiterere yimikorere yibicuruzwa bya reberi bikoreshwa mumashanyarazi yumuriro wuzuza, nibindi, nkuburyo bwa sisitemu yibirunga byumukozi ukora, okiside ya zinc iracyari ubwoko bwibintu byiza cyane. Okiside ya Magnesium irashobora kandi gukoreshwa nkigikorwa gikora muguterera amabuye ya reberi, ariko kubera ibikorwa byo hasi hamwe nimiterere yumubiri wibikoresho bya reberi ni bibi, bityo okiside ya magnesium ikoreshwa cyane nkibikoresho byangiza umubiri hamwe na stabilisateur yubushyuhe muri reberi irimo halogene.

 

Peroxide vulcanisation ni peroxide na reberi mugikorwa cya volcanisation ibaho kubuntu bwiyongera kubuntu kugirango habeho ingufu zingana cc.

Ugereranije na sulfure y'umuhondo wa sulfuru, ifite ibyiza byo kurwanya ubushyuhe bwiza, gukora compression nziza ihoraho ihindagurika, ntibyoroshye gutera ubukonje, no guhuza byoroshye, nibindi. Mu myaka yashize, yakoreshejwe cyane mubicuruzwa bya reberi mugihe cy'ubushyuhe bwinshi. Duhereye ku buryo bwo guhuza, sisitemu ya voloxisation ya peroxide ntishobora gukoreshwa na okiside yicyuma, ariko mubikorwa nyirizina byakozwe, abantu baracyongeramo ibice 5 bya okiside yicyuma muri formula, hamwe nuburyo bwihariye bwo gukoresha ingaruka zibitekerezo bitandukanye. Ubushakashatsi bwerekana ko okiside ya nano zinc, okiside ya magnesium, calcium oxyde na aside idahagije ishobora gukoreshwa nkumukozi mushya uhuza imiyoboro muri peroxide vulcanized hydrogenated nitrile butadiene reberi (HNBR), ishobora kugabanya igihe cy’ibirunga no kunoza ubwinshi bw’imiterere ya reberi.

 

1. Ingaruka ya okiside ya zinc cyangwa magnesium oxyde kumiterere yibikoresho bya reberi

Ugereranije nicyitegererezo cyambaye ubusa, kongeramo okiside ya zinc cyangwa magnesium oxyde rubber M yariyongereye, kandi zinc oxyde reberi ML iri hejuru, ibi biterwa na okiside ya zinc ifite ubuso bunini kandi bigira ingaruka zikomeye, muri materique ya reberi ntabwo byoroshye gutatanya, byoroshye guhuriza hamwe, agglomeration, itera reberi ML yiyongera, amazi meza. Kwiyongera kwa okiside yicyuma kandi byongera MH-ML yikomatanya, byerekana ko okiside yicyuma ishobora guteza imbere guhuza, kuzamura urwego rwibirunga, ariko kandi ikagabanya T10 ariko ikagira ingaruka nke kuri T90. Byongeye kandi, MH-ML ya zinc oxyde ya zinc yari hejuru kurenza iyindi mvaruganda ya magnesium kuri dosiye imwe, ibyo bikaba byerekana ko okiside ya zinc igira ingaruka zikomeye kumirunga kuruta okiside ya magnesium muri sisitemu ya voloxisation ya peroxide.

 

Hamwe no kwiyongera kwa okiside ya zinc na magnesium oxyde, imbaraga zingutu za reberi ya volcanized yabanje kwiyongera hanyuma ikagabanuka, 100% ihoraho yo kuramba ihindagurika muri rusange imyumvire yo kwiyongera, mugihe kurambura kumeneka no kurira imbaraga bigenda bigabanuka, kandi muri dosiye imwe ya zinc oxyde reber material ihora irambuye hejuru ya magnesium oxyde ya MH okiside ya zinc ni ibice 10 bya 100% bihoraho byo kuramba kwa reberi yibirunga ni inzira igabanuka, ishobora guterwa no gukwirakwiza nabi kwa okiside. Ariko, mugihe igipimo cya oxyde ya zinc cyari ibice 10, guhangayikishwa 100% guhoraho kwa reberi yibirunga byerekanaga ko bigenda bigabanuka, ibyo bikaba bishobora guterwa no gukwirakwiza nabi kwa okiside ya zinc. Muri make, kongeramo okiside yicyuma birashobora kunoza ubwuzuzanye bwa rebero ya HNBR munsi ya sisitemu ya peroxide vulcanisation, kandi urwego rwo guhuza ibice bya zinc oxyde irimo reberi iruta iy'umwuka wa magnesium munsi ya dosiye imwe, ariko iyo dosiye ya okiside ya zinc ari ibice 10 byo gutatana guhoraho. Kuva ku mbonerahamwe ya 2, birashobora kandi kugaragara ko kongeramo okiside yicyuma bishobora guteza imbere ubukana, ariko hamwe na dosiye yayo ntibihinduka cyane, kandi ingaruka ku giciro cyo kwisubiraho ntabwo ari ingirakamaro, aho dosiye ya zinc oxyde itagira ingaruka zikomeye kuri DIN abrasion, magnesium oxyde volcanized adrasive abrasion hamwe na dosiye ikomeza kwiyongera, ariko nanone murwego rwo hasi rwerekana. ifite abrasion nziza cyane.

 

Gusaza kwa HNBR ni ubwoko bwumunyururu uhuza ubwoko, bugaragarira mukugabanuka kuramba no kwiyongera kwingufu nimbaraga nyuma yo gusaza. Ibi byerekana ko reaction ihuza ibikorwa ikomeza mugihe cyo gusaza, ibyo bikaba byongera ubucucike bwambukiranya imipaka, kandi imbaraga zingana za reberi zose ziyongera nyuma yo gusaza, byerekana ko HNBR ifite imiterere yubushyuhe bwo hejuru cyane. Mubyongeyeho, kongeramo okiside ya zinc na magnesium oxyde byateje imbere cyane

Byongeye kandi, kongeramo okiside ya zinc na okiside ya magnesium birashobora kuzamura cyane umuvuduko wimpinduka zo kuramba kwinshi nyuma yo guhangana nubushyuhe, kandi umuvuduko wimpinduka zo kurambura kwinshi kwibikoresho bya reberi uragabanuka hamwe no kwiyongera kwa dosiye yibikoresho, byerekana ubukana buhebuje bwubushyuhe bwo hejuru, ibyo bikaba bishobora guterwa nuko okiside yicyuma ubwayo ishobora kuba ihujwe nubushuhe bwibintu byangiza umubiri. ya ogisijeni, no kunoza imikorere yubushyuhe bwo hejuru bwibikoresho bya reberi. Muri icyo gihe, kongeramo okiside ya zinc irashobora kugabanya cyane ihindagurika ryimiterere ihoraho ya reberi, ariko hamwe na dosiye yayo ntabwo ihinduka cyane; magnesium oxyde kuri compression ihoraho ihindagurika ryingaruka ntabwo ari ngombwa cyane. Kubwibyo, kongeramo urugero rukwiye rwa oxyde yicyuma muri sisitemu ya peroxide volcanisation ifasha kunoza ubushyuhe bwa reberi.

 

Iyo igipimo cya okiside ya zinc ari ibice 5, umurongo wa TG-DTG wibikoresho bya reberi ya HNBR, nko kubora ubushyuhe bwumuriro wibikoresho bya reberi byagaragaye ibyiciro bibiri bigaragara cyane, biterwa ahanini nitsinda ryibice bibiri bitandukanye bya HNBR ya molekuline yubushyuhe butandukanye. Icyiciro cya mbere ahanini ni butyl

Icyiciro cya mbere giterwa ahanini nubushyuhe bwumuriro wububiko bubiri muri butadiene, naho icyiciro cya kabiri giterwa no kuzenguruka igice cyumunyururu wa acrylonitrile mugihe cyo gushyushya kugirango habeho uruganda rwa chelate, rushobora gusa gufatanwa nubushyuhe bwo hejuru cyane, kuburyo hariho ibyiciro bibiri bigaragara byerekana ubushyuhe, kandi ubushyuhe ntarengwa bwo kubora bwibikoresho bya reberi byagaragaye kuri 468.49 ℃ .

 

Ubushyuhe bwambere bwangirika bwumuriro (mugihe igipimo cyigihombo kinini ari 5%) hamwe nubushuhe ntarengwa bwo kubora bwibikoresho bya reberi bifite icyerekezo kimwe, kandi kongeramo okiside yicyuma birashobora kugabanya umuvuduko mwinshi wibintu byinshi bya reberi  , aho ubushyuhe bwambere bwangirika bwumuriro wibice 5 byibikoresho bya reberi byiyongera cyane okiside ugereranije nibice bya rubber, byerekana ko ibice 5 bya zeru, byerekana ko ibice 5 bya zeru, byerekana ko ibice 5 bya zeru, ibyo bikaba byerekana ko ibice 5 bya zeru, byerekana ko ibice 5 bya zeru; ya zinc ni ibice 10, kubanza kwangirika kwubushyuhe Ariko, mugihe urugero rwa okiside ya zinc yari ibice 10, ubushyuhe bwambere bwangirika bwumuriro bwaragabanutse. Ibi birashobora guterwa na: (1) gukwirakwiza nabi kwa okiside ya zinc; . Impamvu nyayo yabyo iracyakomeza gukorwaho iperereza. Ubushyuhe bwambere bwo kubora bwumuriro wibice 5 bya magnesium oxyde ya reberi yagabanutse ugereranije nubwa reberi yambaye ubusa, kandi ubushyuhe bwo kubora bwumuriro bwibikoresho bya reberi bwashoboraga kwiyongera gusa mugihe ingano ya oxyde ya magnesium yari ibice 10. Gukoresha isesengura rya TG mu kuranga ubushyuhe bwa reberi ya silicone, ibisubizo byerekana ko ubushyuhe bwo mu kirere busaza imikorere ya reberi ya silicone hamwe nubushyuhe bwangirika bwumuriro mukirere cya ogisijeni yimihindagurikire irahinduka, ariko muri iki kizamini byombi ntabwo byandikiranye, ahubwo ni igipimo ntarengwa cyo gutakaza kwinshi hamwe nuburyo bwo guhinduka kwubushuhe bwumuriro ushushe bitewe nubushyuhe butandukanye bwumuriro hamwe nubushyuhe butandukanye bitewe nubushyuhe bwumuriro ushushe hamwe nubushuhe butandukanye bwumuriro. isesengura rya TG uko ibintu bimeze (nk'ikirere cya gaze). Ibi birashobora guterwa nuburyo butandukanye muburyo bwo kubora bwumuriro wubwoko butandukanye bwa reberi hamwe nuburyo butandukanye bwo gusesengura TG (urugero: ikirere cya gaze), niba rero isesengura rya TG rikoreshwa mugusuzuma ubukana bwumuyaga ushushe wa reberi, imiterere nyayo nibizamini bigomba gusuzumwa neza.

 

2. okiside ya zinc / magnesium oxyde no gukoresha ibifatika kumuriro no kurwanya gusaza kwikirere no kwikuramo ingaruka zihoraho.

Iyo igipimo cya okiside ya zinc / magnesium oxyde ari 7/3, habaho ingaruka zifatika kumikorere yubushyuhe bwo gusaza bwimikorere ya adhesive, kandi ibifatika bigira imbaraga nziza zo guhangana nubushyuhe, mugihe iyongerwaho rya okiside ya magnesium igira ingaruka mbi kumyuka ihoraho ihindagurika ryimiterere.

 

Umwanzuro

. guhora uhangayitse kubera gutatana nabi, ariko amazi yibikoresho bya reberi arangirika, ibyo bikaba bidafite ingaruka nke kubiciro byagarutse no kurwanya abrasion. Kurwanya Abrasion nta ngaruka nke bifite.

.

Ingano yo kurwanya ubushyuhe iriyongera, mugihe hiyongereyeho okiside ya zinc irashobora kunoza ihindagurika rihoraho rya rebero, mugihe oxyde ya magnesium ntacyo igira kuri yo.

.

.


LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.