626
SABIC
SABIC EPDM 626. Enkola y’okukozesa enkola ya SABIC
| Ebiriwo: | |
|---|---|
| Omuwendo: | |
EMIRIMU GY’EBINTU EBY’ENJAWULO:
| EBY'BWANANNYINI | EMIRIMU EGY’ENJAWULO | UNITS | ENGERI Y’OKUKEBERA |
| EBINTU EBIKWATA KU POLYMER | |||
| Obuzito bwa Mooney | |||
| ML 1+4, 125 °C (1) . | 67 |
MU |
ASTMD 1646. Enkola ya ASTMD |
| Ebirimu Ethylene | 69 |
wt.% |
ASTMD 3900. Enkola ya ASTMD |
| Ebirimu Ethylidene Norbornene (ENB) Ebirimu | 2.8 |
wt.% | ASTMD 6047 |
OBUBONERO:
SABIC EPDM 626 ekoleddwa :okubeera n’ebintu ebirungi eby’omubiri, okulongoosa mu kutabula n’okukwata ekyuma, okulongoosa mu kalenda, okukuuma obulungi amafuta, okukendeeza ku bimuli ebiwonya mu bikozesebwa.
OKUTEEKA N’OKUKWATA: SABIC EPDM 626 erina okuterekebwa mu paakingi yaayo eyasooka ku bbugumu eriri mu mbeera enkalu; okukulukuta kw’obukuta kuyinza okukwatibwako obubi puleesa oba ebbugumu eringi; okubeera mu bbugumu, ekitangaala kya ultraviolet n’omusana obutereevu kulina okwewalibwa. Mu mbeera entuufu ey’okutereka, ekintu kino kibeera kinywevu okumala emyezi 24 okuva ku lunaku lwe kyakolebwa. SABIC tejja kwongera ku ggaranti yaayo ng’embeera y’okutereka temala ekiyinza okuvaako omutindo okwonooneka ng’okukaluba kwa pellet oba okukyusa langi ekiyinza okuvaamu omulimu gw’ebintu obutakola bulungi.
OKWEGAANA Okutunda kwonna okukolebwa SABIC, amakampuni gaayo n'abakwatibwako (buli emu 'mutunzi'), kukolebwa wansi w'obukwakkulizo obw'omutindo obw'okutunda obw'omutunzi (obufunibwa nga osabye) okuggyako nga bakkiriziganyizza mu buwandiike era nga kussiddwaako omukono ku lw'omutunzi. Wadde ng’amawulire agali wano gaweereddwa mu mutima mulungi, OMUTUNDI TAKOZESA WARANTI, EY’OKULAGULA OBA ETEGEEZEBWA, OMULI OKUTUUNDIBWA N’OBUTATyoboola EBINTU BY’OBUTUNDU, WAADDE TAKITWALA BUVUNAANYIZIBWA BYONNNA, OBUTUNDU OBA OBUTITEEREVU, KU BY’OKUTUNDA KU NKOZESA, OBUVUNANYIZIBWA OBA OKUSAANIRA OKUKOLA OBA EKIGENDERERWA KYA BINTU BINO MU KUKOZESA KWONNA. Buli kasitoma alina okuzuula oba ebikozesebwa omutunzi bisaanira okukozesebwa kasitoma mu ngeri ey’enjawulo ng’ayita mu kugezesa n’okwekenneenya okutuufu. Tewali kiwandiiko kya mutunzi ekikwata ku nkozesa esoboka ey’ekintu kyonna, empeereza oba dizayini kigendereddwa, oba kisaana kutambulizibwa, kuwa layisinsi yonna wansi wa patent yonna oba eddembe eddala ery’obuntu.