626
Sabic
Sabic EPDM 626
Nnweta: | |
---|---|
Ọnụ ọgụgụ: | |
Ngwongwo nke Ngwongwo:
Olu | Ụkpụrụ omume | Nkeji iri | Ụzọ ule |
Ngwongwo polymer | |||
Vioney Vivances | |||
ML 1 + 4, 125 Celsius C (1) | 67 |
Mu |
ASTMD 1646 |
Ọdịnaya Etylene | 69 |
wt.% |
ASTMD 3900 |
Odide Otheylido (ENB) | 2.8 |
wt.% | ASTMD 6047 |
Njirimara:
Ezubere EPDM 626 maka: Njirimara nke anụ ahụ ka mma, ịgwakọta ma na-ejikwa mil, ma belata, belata ọgwụgwọ oge ntoju na ogige.
Nchekwa na ijikwa: Sabic Epdm 626 kwesịrị ịchekwa na mbukota mbụ na amịrị na ọnọdụ akọrọ; Flutbility nke pellets nwere ike imetụta ya site na nrụgide ma ọ bụ okpomọkụ dị elu; Ekpughere ọkụ na ọkụ, ọkụ ultraviolet na ìhè anyanwụ kwesịrị izere. N'okpuru ọnọdụ nchekwa kwesịrị ekwesị, ngwaahịa ahụ kwụsiri ike maka ọnwa 24 site na ụbọchị nrụpụta. Sabic agaghị agbasa akwụkwọ ikike ya mgbe ọnọdụ nchekwa ezughi oke nke nwere ike ibute ogo dị ka Pellet siri ike nke nwere ike ibute arụmọrụ ngwaahịa ezughi oke.
Gbanyụọ ire ọ bụla na-ere ahịa, ihe enyemaka na ndị mmekọ ya (ọ bụla na-ere ahịa ere (ọ dị n'okpuru ọkọlọtọ nke ire ere (ọ gwụla ma ekwenyeghị na ederede na-ere ahịa. Ọ bụ ezie na enyere ozi ahụ dị ka ezigbo akwụkwọ ozi, onye na-ere ahịa anaghị ekwe ọrụ, gosipụta ma ọ bụ na-adịghị mma, yana ahụike maka iji ya mee ihe ma ọ bụ nzube nke ngwaahịa ndị a na ngwa ọ bụla. Onye ahịa ọ bụla ga-ekpebi ikike nke ndị na-ere ahịa maka iji ihe ndị ahịa na nyocha kwesịrị ekwesị. Enweghị nkwupụta site na onye na-ere ahịa banyere iji ngwaahịa ọ bụla, ezubere, ma ọ bụ nke a ga-eme, iji nye ikike ọ bụla ma ọ bụ ihe ọgụgụ isi ọ bụla.
Ngwongwo nke Ngwongwo:
Olu | Ụkpụrụ omume | Nkeji iri | Ụzọ ule |
Ngwongwo polymer | |||
Vioney Vivances | |||
ML 1 + 4, 125 Celsius C (1) | 67 |
Mu |
ASTMD 1646 |
Ọdịnaya Etylene | 69 |
wt.% |
ASTMD 3900 |
Odide Otheylido (ENB) | 2.8 |
wt.% | ASTMD 6047 |
Njirimara:
Ezubere EPDM 626 maka: Njirimara nke anụ ahụ ka mma, ịgwakọta ma na-ejikwa mil, ma belata, belata ọgwụgwọ oge ntoju na ogige.
Nchekwa na ijikwa: Sabic Epdm 626 kwesịrị ịchekwa na mbukota mbụ na amịrị na ọnọdụ akọrọ; Flutbility nke pellets nwere ike imetụta ya site na nrụgide ma ọ bụ okpomọkụ dị elu; Ekpughere ọkụ na ọkụ, ọkụ ultraviolet na ìhè anyanwụ kwesịrị izere. N'okpuru ọnọdụ nchekwa kwesịrị ekwesị, ngwaahịa ahụ kwụsiri ike maka ọnwa 24 site na ụbọchị nrụpụta. Sabic agaghị agbasa akwụkwọ ikike ya mgbe ọnọdụ nchekwa ezughi oke nke nwere ike ibute ogo dị ka Pellet siri ike nke nwere ike ibute arụmọrụ ngwaahịa ezughi oke.
Gbanyụọ ire ọ bụla na-ere ahịa, ihe enyemaka na ndị mmekọ ya (ọ bụla na-ere ahịa ere (ọ dị n'okpuru ọkọlọtọ nke ire ere (ọ gwụla ma ekwenyeghị na ederede na-ere ahịa. Ọ bụ ezie na enyere ozi ahụ dị ka ezigbo akwụkwọ ozi, onye na-ere ahịa anaghị ekwe ọrụ, gosipụta ma ọ bụ na-adịghị mma, yana ahụike maka iji ya mee ihe ma ọ bụ nzube nke ngwaahịa ndị a na ngwa ọ bụla. Onye ahịa ọ bụla ga-ekpebi ikike nke ndị na-ere ahịa maka iji ihe ndị ahịa na nyocha kwesịrị ekwesị. Enweghị nkwupụta site na onye na-ere ahịa banyere iji ngwaahịa ọ bụla, ezubere, ma ọ bụ nke a ga-eme, iji nye ikike ọ bụla ma ọ bụ ihe ọgụgụ isi ọ bụla.