Tuna fluoroelastomer dinhmun leh hmalam hun leh metallurgy, automobile leh oil field rubber sealing-a a hman dan

Views: 0     Author: Site Editor A chhuah hun: 2023-08-22 A chhuahna: Hmun

Zawhna zawt rawh

1, rubber seal siamna atana metallurgy, automotive industry leh oilfield drilling mamawh te a ni


(1) metallurgical machinery: metallurgical industry, high-speed wire rod mill, small mill technology chu a thang chak hle a, a bik takin rolling speed sang tak a ni a, productivity a sang hle a, foreign hmasawn ber berte chu 120m / s thleng a ni a, mill oil film bearing speed a sang zel a, seal mamawhna nei bearing pawh a tha chho zel bawk. Seal form for double-sided seal (roll diameter seal tia hriat bawk), sealing surface pahnih a awm a, a sir khatah sealing water vapor, a sir lehlamah sealing lubricating oil, hnathawhna temperature chu a tlangpuiin 120 °C aia sang a ni a, a pianzia leh a structure chu a complexity a size mamawh a ni. Product mamawh rubber compound heat resistance tha tak, tar chak lo, water vapor leh lubricant resistance nei, process performance tha tak nei, mobility tha tak nei, complex structural product siamna atana tha.


(2) automotive industry: automotive industry leh a kaihhnawih field-ah (rubber) seal hmang tam ber a ni tawh. Tun hnaiah, user mamawh sang zawk chi hrang hrang hmachhawnin, inelna nasa zawk, khawvel puma environment regulation tihchakna nen a inzawm a, hei hian thil siamtute chu siamṭhat chhunzawm zel turin a fuih a, design ṭha zawkah siamin, performance tihchangtlun turin, emission tihtlem nan, fuel hman tlem nan rit tihtlem turin a fuih a ni. Technology lama hmasawnna avang hian high-tech, high-performance equipment leh devices te chu an lo thang zel a, an lar chho zel a, chungte chu: high-performance engine (turbocharged engine system ang chi), turbocharger, automatic transmission, fuel economy tihchangtlunna tur aerodynamic design thar, electronic fuel injection device, bakah technology thar, exhaust gas purification device ang chi te. Car rit siam la, specification a tlem tial tial a, engine room space a tawi tial tial a, temperature a sang chho zel a; engine oil (SF) level thar ber hman te, chubakah lubricant leh oil siam thatna dangte, additives, a bik takin corrosive additives tam zawk, chemical environment complex zawk, leh chutih rual chuan automotive rear crankshaft inversion of crankshafts with silicone seals with the increasingly serious damage phenomenon, and therefore the rubber seals of heat resistance, Corrosion resistance, lubricating oil additives leh oxidized oil (acid oil) performance do theihna, leh nunna leh a dangte chuan mamawh sang zawk a dah a, traditional NBR chuan a man a hniam viau nachungin, a pumpuiah performance tha tak, oil-resistant rubber anga hman lar tak, mahse chain link-a double bonds awm avang hian, heat aging, weather resistance, chemical stability a chhe hle a, mamawh tak tak a tlin theih loh avangin, a mamawh tak tak a tlin theih loh avangin rubber material bik, ACM, FKM leh HNBR te performance combination bik nen hman tur a ni.


(3) oilfield: rubber seal tan chuan oil well-a oil drilling downhole seal hi a harsa ber a, boruak mamawh ber a ni fo a, kum tam tak chhunga oil laihchhuah a nih avangin lei hnuaia crude oil chu tun hnaiah leilung tlangram atanga tuifinriat thuk tak emaw thlaler hmunah zawi zawiin a inthlak tan a, chu chuan oil wells thuk zawk, tuikhuah thuk zawkah a thuk zawk a, chu chu hmasawnna a ni of ultra-deep wells, the downhole seals must be resistant to more demanding and complex working conditions such as high and low temperatures, high pressure, the current Well hnuai lam temperature leh pressure chu a tlangpuiin 200 °C leh 100 MPa a tling tawh a ni. Sulfur oil sang tak, H2S, H20, C02-containing strong corrosive media leh hmanraw tam zawk chu drilling fluid-ah an awm a, chutah chuan anticorrosive agents, additives chi hrang hrang a awm a, rubber sealing materials hmante performance chu a tlangpui aiin a sang zawk hle a, tuna fluoroelastomers tam tak hman a ni wells downstream working conditions have a changeable environment, there may often be Unpredictable situations, such as the danger of sudden pressure drop, the working pressure of the well, elastomer seal zawng zawng hian he hlauhawmna hi an nei vek a, elastomer hi bubble lo lang awlsam tak a ni a, rubber products te chu soluble high-pressure gas ah hun engemaw chen an awm a, chu chu pressure hloh nghal ang chi, soluble gases te hi a ni ang taksaah chak taka a inzar pharh a, bubble lian tak tak a lo awm a, a puak a, heng dinhmun hriat lawk lohte hian tuikhuah chu a tlan tawh loh nan seal thlak a thlen ang a, nitin a siam chhuah hloh chu oil ton sang tam tak thleng a ni thei. Heng thil thleng tur ruahman lawk lohte hian seal thlak nan well khar a thlen thei a, chu chuan ni khatah dollar maktaduai tam tak a siam chhuah a hloh phah thei a ni. Hei hian sealing performance tihchangtlun nan rubber material chakna sang, recovery tha leh adapted tha zawk zawn a ngai a ni.


2、FKM mizia


Fluoroelastomer hi a tirah chuan aviation industry-in high-performance sealing elastomers mamawh phuhruk nan hman a ni a, chumi hnuah rang takin kawng dang, automotive, chemical leh field dangah te pawh a zau chho ta a, tunah chuan automotive industry-ah ramdang fluorine rubber hman ber a ni a, temperature sang, boruak chhe thei tak leh hriat hlawh tak takah pawh a practical performance tha tak a ni.

Fluorine rubber hian a hnuaia mi ang hian a nei a.


(1) heat resistance tha tak, temperature sang tak performance atana rubber tha ber, 230 °C-ah hun rei tak hman theih a ni a, hun rei lote chhung atan 300 °C thleng hman theih a ni a, general oil-resistant nitrile rubber hmanna temperature chu 120 °C aia tam lo, ACM 160 °C, chlorine ether a hnuaia 120 °C aia tam lo a ni thung.


(2)Oil resistance tha tak, rubber zawng zawng zingah a tha ber hian mineral oil leh lubricating oil tam zawk a do thei.


(3)Chemical media laka invenna tha tak, chuta tang chuan solvent resistance, fuel resistance, acid leh alkali resistance, vapor resistance te hi rubber zawng zawng zingah a tha ber a, mineral acid tam zawk laka invenna a ni.


(4) Meialh laka invenna tha tak, mahni in timit thei meialh laka invenna rubber;


(5) Ozone laka invenna rubber tha ber atan khaw lum leh khaw vawt laka invenna tha tak, mold leh mildew laka invenna tha tak a ni.


(6) high-temperature strength performance tha tak leh compression permanent deformation performance tha tak, high-temperature physical leh mechanical property tha zawk elastomer dang tam zawk aiin chu bâkah low-temperature performance chu a tlangpui zawk a ni a, rubber-a fluoroelastomer property tam tak chu a ṭha ber, a nih loh leh an zinga rank-a dah a ni a, a bik takin oil leh chemical laka a do theihna, fluid chi hrang za thum aia tam tihchhiat a do theihna a ni a, chu aia tlem zawk chu temperature sang chhoh vanga nghawng laka a do theihna chu a lian lo hle a ni fluoroelastomer low-temperature performance hi a tlangpui a, mahse absolute zero hnaih condition-a hman static sealing effect pawh a satisfactory a nih pawhin, fluoroelastomer hian rubber dang tam zawk a nei a, performance tha tak a nei lo, almost indispensable sealing material in high temperature leh strong corrosive environment, has been in the ever-changing automotive, chemical, office automation and semiconductor manufacturing leh industry dangte hian hmun pawimawh tak leh pawimawh tak an chang!


3、Industry pathum-a FKM application dinhmun


Automobile, metallurgy leh oil field industry-ah rubber leh plastic sealing material-te tana hnathawh dan khauh zual zelin temperature sang tak, oil resistance, chemical resistance leh complex environment-a physical leh mechanical property mamawh sang zawk, traditional nitrile rubber hian mamawh a phuhruk thei lo a, fluorine rubber rubber leh rubber chi dang combination bik nen hman a ngai a ni. Fluoroelastomer hi a performance tha tak nen heng industry hrang hrangah hian hman a ni nasa hle.FKM hi a performance tha tak nen heng industry ah te hian hman a ni nasa hle.


Khawvel pumah FKM hman a pung chho zel a, a tam zawk hi automotive industry-ah hman a ni. Chutiang chu tunlai khawvela fluoroelastomer siam chhuah hian 8000t a pel tawh a, chung zinga 60 a 70% chu automotive products hmanga siam a ni a, a bik takin oil seal chi hrang hrang (rotary, reciprocating) siamna a ni a, engine oil seal, transmission oil seal (chutiang: oil seal hma leh hnua crankshaft, gear compartment oil seal, camshaft, hub leh half-shaft oil seal, valve guide oil seal, etc.), 'chutiang bawkin transmission seal, air intake gasket compressor O-ring, fuel system seal (eg, fuel injection unit seal, fuel pump diaphragm, pump seal, injector 0-ring, accelerator pump bowl, filter seal, carburetor seal leh gasoline pump seal) te pawh a awm bawk.


Automobile engine performance tihchangtlun, engine oil grade thar (SF ang chi) hman leh lubricant tihchangtlun, corrosive additives tam zawk, engine temperature a sang chho zel a, oil seal hman pawh 30m/s thleng a sang thei a, temperature hman dan pawh a tlangpuiin 150 °C thleng a ni chemical environment a khauh zual zel a, chutih laiin automobile hnua crankshaft of the inverted crankshaft with silicone seals with the damage phenomenon chu a nasa zual zel a, fluoroelastomer seal hman hian Viton seals hman hian oil resistance a ti tha thei a, heat resistance a ti tha thei a, service life a ti rei thei bawk (50~600/0 thleng), wear 40~60% a ti tlem thei bawk.


Metallurgical industry, metallurgical high-line rolling mill shaft diameter double-sided sealing ramdang ramte hian NBR an hmang tlangpui a, a chhiatna ber chu a product hi a tar awlsam a, a chhe thei a, a dam rei thei lo a, a tlangpuiin kar 3. 5 a ni a, continuous casting machine hi metallurgical enterprise tan chuan hmanraw pawimawh ber a ni a, fan cylinder seal te hi fluorine rubber material a ni.


Oil drilling oil well seal te hian hnathawhna hmun harsa leh khirh ber ber an hmachhawn a, chu chu tui thuk tak thlenga drilling vang te, ultra-deep well development avang te, oil well downhole seal te hian hnathawh dan boruak khirh leh harsa zawk (high leh low temperature, high pressure, high sulfur petroleum, strong corrosive media H2S, H20, C02 awmna, chubakah hmanraw tam zawk chu anticorrosive-ah an inhnim a ngai a ni agents, additives chi hrang hrang drilling fluid te). Tun hma chuan oil lakchhuahna hmanruaa rubber seal hman te hi oil resistance tha tak nitrile rubber hmanga siam a ni tlangpui a, zawi zawiin fluorine rubber, silicone rubber leh HNBR rubber, etc.-ah te siam chhuah a ni a, a chang chuan tetra-propyl fluorine rubber, perfluoroethers rubber leh fluorine rubber bik dang, in downhole-a sulfur awmna crude oil nena inzawmna leh wellhead hmanrua, blowout preventer, downhole safety valve leh rubber seal-a packers te chu fluorine rubber hmannaah hman a ni nasa hle. Entirnan, fluorine rubber hi downhole leh wellhead hmanrua, sulfur awmna crude oil nena inzawm, blowout preventer leh packer te nena inzawm rubber seal-ah hman a ni fo tawh a ni.


QUICK LINKS A AWM VE ANG

CONTACT THIL AWM DAN

Add: No.33, Lane 159, Taiye kawngpui, Fengxian District, Shanghai-a awm a ni
Tel / WhatsApp / Skype: +86 15221953351 ah zawhfiah theih a ni
E-mail hmangin:  info@herchyrubber.com
A rilru a hah lutuk chuan a rilru a buai em em a.     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a ni |   Thuruk humhalh dan tur | Support By Leadong a ni.