Amansan no su a ɛkorɔn a ɛma nsu a ɛyɛ hyew Tackifying Phenolic Resin
Sɛnea ɛte: hann kɔkɔɔ kosi kɔkɔɔ granular
Wiase nyinaa softening point: 105-110 ° C
Ash (600 ° C): ≤0.5%
Packing: abiɛsa-layer composite kraft krataa anaa PE packaging bag, amansan net mu duru 25kg / 40kg (betumi ayɛ customized)
Validity: Mpɛn pii no 1 afe
Shanghai Herchy Rubber Co., Ltd yɛ kan manufacturer ne nea ɔde tackifying phenolic resins a ɛkorɔn ma wɔ China, a ɔde mfe pii ayɛ adwuma ho nimdeɛ. Yɛde Universal Type High Melting Point Tackifying Phenolic Resins ahorow pii ma, a wɔayɛ sɛnea ɛbɛyɛ a wobedi mfiridwuma mu nneɛma ahorow ahwehwɛde ho dwuma. Ɛnam akansi bo ne adwumayɛ a ɛkorɔn nti, wɔayɛ yɛn nneɛma no sɛnea ɛbɛyɛ a ɛbɛma abatade a ɛkyɛn so, agyina pintinn, na ayɛ den ama w’ahiade a ɛfa nneɛma a wɔyɛ ho. Di yɛn nkitaho mprempren na woahu sɛnea yɛn ano aduru betumi aboa w’adwuma nkɔso!