I-Universal Type High Melting Point Tackifying Phenolic Resin
Ukubukeka: okuphuzi okukhanyayo kuya ku-granular
okuphuzi Iphuzu lokuthambisa lomhlaba wonke: 105-110°C
Umlotha (600°C): ≤0.5%
Ukupakisha: iphepha le-kraft elinezingqimba ezintathu eliyinhlanganisela yephepha noma isikhwama sokupakisha se-PE, isisindo senetha jikelele 25kg/40kg (singenziwa)
Ukusebenza ngokwezifiso: I-Cooper I-Rubber ihola unyaka wonke.
umphakeli wekhwalithi ephezulu ye-phenolic resins e-China, neminyaka yobungcweti bemboni. Sihlinzeka ngezinhlobonhlobo ze-Universal Type High Melting Point Tackifying Phenolic Resins, eklanyelwe ukuhlangabezana nezidingo zezinhlelo zokusebenza ezihlukahlukene zezimboni. Ngamanani entengo ancintisanayo nokusebenza okuphezulu, imikhiqizo yethu yakhelwe ukuletha ukunamathela okuhle kakhulu, ukuzinza, nokuqina kwezidingo zakho zokukhiqiza. Xhumana nathi manje ukuze uthole ukuthi izixazululo zethu zingakusekela kanjani ukukhula kwebhizinisi lakho!