Ubwoko Bwisi Bwose bwo Gushonga Ingingo Gukuramo Fenolike
Kugaragara: Umuhondo woroshye kugeza umuhondo granular
Ingingo yoroshya Isi: 105-110 ° C
Ivu (600 ° C): ≤0.5%
Gupakira: impapuro eshatu zikorana impapuro zipapuro cyangwa igikapu cyo gupakira PE, uburemere bwumutungo rusange 25kg / 40kg (birashobora guhindurwa)
Agaciro: Mubisanzwe umwaka 1
Shanghai Herchy Rubber Co., Ltd numushinga wambere kandi utanga ibicuruzwa byujuje ubuziranenge mubushinwa. Dutanga ubwoko butandukanye bwubwoko Bwose bwo Gushonga Ingingo Yokoresha Ibisigarira bya Fenolike, byashizweho kugirango bihuze ibyifuzo byinganda zitandukanye. Hamwe nibiciro byapiganwa nibikorwa byiza, ibicuruzwa byacu byashizweho kugirango bitange neza, bihamye, kandi biramba kubyo ukeneye gukora. Twandikire nonaha kugirango tumenye uburyo ibisubizo byacu bishobora gutera inkunga ubucuruzi bwawe!