Nooca Caalamiga ah ee Meesha dhalaalaysa ee Sare ee Xakamaynta Resin phenolic
Muuqashada: huruud fudud ilaa jaalaha granular dhibic
jilciya Global: 105-110 ° C
Ash (600 ° C): ≤0.5%
Baakad: saddex-lakab ka kooban warqad kraft ama baakadaha PE, miisaanka net universal 25kg / 40kg (waa la beddeli karaa)
ansaxnimada: Sida caadiga ah 1 sano
Co., Herchy Ltd. wax ka qabashada resins phenolic gudaha Shiinaha, oo leh sanado khibrad warshadeed ah. Waxaan bixinaa noocyo kala duwan oo caalami ah oo ah Nooca Caalamiga ah ee Dhalalinta Sare Tackifying Resins Phenolic, loogu talagalay in lagu daboolo baahiyaha codsiyada warshadaha kala duwan. Iyada oo leh qiime tartan iyo wax qabad sare, alaabadayada waxaa loo habeeyay si ay u bixiyaan ku dheggan, xasilloonida, iyo adkeysiga baahiyahaaga wax soo saarka. Nala soo xidhiidh hadda si aad u ogaato sida xalalkeennu u taageeri karo kobaca ganacsigaaga!