Kɔla: tuntum den
: 65±5 Mpoano A
menni viscosity: ML(1+10)121°C 30-50
Size Specification: Can be more customized (Sheet)
vulcanization Condition: 175l*10min secondary Vulcanization
:
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4%
Ethylene a ɛwɔ mu: 72%
Ngo a ɛwɔ mu: 100%
Mooney Viscosity: ML(1+4)125°C 41
Size: 25kg/block
MOQ: 25kg
Packing: Boxed: Boxed
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 8.5%
Ethylene Nsɛm: 60%
Mooney Viscosity: ML(1+4)125°C 109
Size: 25kg/block
MOQ: 25kg
Packing: Boxed: Boxed
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4.5%
ethylene a ɛwɔ mu: 62%
Mooney Viscosity: ML(1+4)125°C 98
Size: 25kg/block
MOQ: 25kg
Packing: Boxed: Boxed