Kyakkyawan Tsari Babban Ƙarfi Mai Ƙarfi Fluoroelastomer
Launi: Baƙar fata
tsarin vulcanization: tsarin bisphenol
Hardness: 70 ± 5 SHORE A
Mooney danko: ML (1 + 10) 121 ℃ 50-70
Size ƙayyadaddun: na iya zama mafi musamman (sheet)
Vulcanization yanayi: 175 ℃ * 10min Sakandare vulcanization: misali 2400 ℃ (
matsakaicin adadin) 50kg