Tae: Brown (ka taea te whakarite)
Pūnaha Vulcanization: bisphenol system
Te ihirangi Fluorine: 65%
Mooney viscosity: ML (1 + 10) 121 ° C 20-40
Rahi: Ka taea te whakarite ake (pepa)
Nga tikanga Vulcanization: 175 ° C * 10min Te vulcanization tuarua: 200 ° Q * 4hmen te paerewa: 202 ° Q *
4hmen.
Tae: pango
Pakeke: 65±5 SHORE A
Menni viscosity: ML(1+10)121℃ 30-50
Rahi whakatakotoranga: ka taea te whakarite ake (pepa)
Te ahua o te whakangao: 175℃ * 10min te vulcanization tuarua: 200 ℃ * 4h (2mm waahanga whakamatautau paerewa)
Te rahinga ota 50kg:
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 4%
Ethylene content: 72%
Te hinu hinu: 100%
Mooney viscosity: ML(1 + 4) 125 ° C 41
Rahi: 25kg / poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) paraka
Tuatoru momo monomer me te ihirangi: ENB, 8.5%
Ethylene ihirangi: 60%
Mooney viscosity: ML(1+4)125°C 109
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa, maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 4.5%
Ethylene ihirangi: 62%
Mooney viscosity: ML(1+4)125°C 98
Rahi: 25kg/poraka
MOQ: 25kg