Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
a ɛto so abiɛsa monomer su ne emu nsɛm: ENB, 8.5%
ethylene a ɛwɔ mu: 60%
Mooney viscosity: ML (1+4) 125°C 84 ml(1+4)150 °C 81
size: 25kg/block
: 25kg:
moq
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
a ɛto so abiɛsa monomer no su ne emu nsɛm: ENB, 5.7%
Ethylene a ɛwɔ mu: 70%
ngo a ɛwɔ mu: 50%
Mooney Viscosity: ML(1+4)125°C 53
Size: 25kg/block
moq: 25kg
Packing: Boxed: Boxed: Boxed: