Go šoma gabotse ga Hose ya Matla a Godimo Fluoroelastomer .
Mmala: Black
Vulcanization System: Bisphenol Tsamaiso
Thata: 70±5 Shore A
Mooney Viscosity: ML(1+10)121 50-70
Boholo Specification: E ka ba ho feta customised (letlakala)
vulcanization Maemo: 175 7 10min Bobeli Vulcanization:
5001 4H) bonyane qetellong (