Tɛlɛfon: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
NNƐM A WƆYƐ
Wowɔ ha: Fie » Nneɛma a wɔyɛ » Nneɛma a Wɔde Yɛ Nneɛma » VMQ Silicone a wɔde yɛ adwuma » GA-30×3 Silicone Rɔba (Silica a ɛyɛ wusiw) a ɛwɔ ahoɔden a ɛkorɔn (HCR)

loading a wɔde ahyɛ mu

Kyɛ ma:
facebook a wɔde kyɛ nsɛmma nhoma
twitter so a wɔde kyɛ ade
line kyɛfa button
wechat kyɛfa button
linkedin kyɛfa button
pinterest a wɔde kyekyɛ nneɛma
whatsapp kyɛfa button
kyɛ saa kyɛfa button yi

GA-30×3 Silicone Rɔba (Silica a ɛyɛ wusiw) a ɛwɔ ahoɔden a ɛkorɔn (HCR) .

Dwumadi: nsɔano a ɛkorɔn, mats, agumadi cushions ne nneɛma afoforo a ɛkorɔn resilience.
Nneɛma atitiriw: ahoɔden a ɛkorɔn, processab小ty a eye kyɛn so,twam RoHS,REACH, ne LFGB no nokwaredi.
 
Shanghai Herchy Rubber Co., Ltd. yɛ wo ahotoso manufacturer ne supplier a ɛkorɔn rɔba compounds, titiriw wɔ GA-30 × 3 Silicone Rubber (fumed Silica) a High Resilience (HCR) yɛ mu. Yɛn adwumakuw no ayɛ krado sɛ yɛde nneɛma soronko a wɔayɛ ama w’ahiade pɔtee ne w’ahwehwɛde ahorow bɛma. Yɛde yɛn hoahoa yɛn ho wɔ yɛn tumi a yɛde ano aduru a wɔahyɛ da ayɛ ama a yɛwɔ ahofama sɛ yɛbɛyɛ nea ɛkorɔn ne adwumayɛ a ɛda nsow. Di yɛn nkitaho nnɛ na fi wo adwuma a edi hɔ no ase na nya yɛn rɔba ano aduru a ɛkorɔn no mu osuahu wɔ bo a ɛyɛ den so.
  • GA-30×3 na ɛwɔ hɔ

  • Herchy a ɔyɛ ɔbarima

Nea Ɛwɔ Hɔ:
Dodow:

Yɛn GA-30×3 Silicone Rubber (fumed Silica) a ɛwɔ ahoɔden a ɛkorɔn (HCR) a yɛde reba .


Wɔ Shanghai Herchy Rubber Co., Ltd., yɛde GA-30 × 3 Silicone Rubber (fumed Silica) a High Resilience (HCR), elastomer a ɛyɛ adwuma yiye a wɔayɛ sɛnea ɛbɛyɛ a wobedi nnwuma ahorow ahiade a ɛyɛ den ho dwuma ma. Saa rɔba yi ye ma nneɛma a ɛhwehwɛ sɛ wɔde mfiri yɛ adwuma a ɛkorɔn na ɛtra hɔ kyɛ, wɔ mmeae a ɛyɛ hu mpo.


Yɛn GA-30×3 Silicone Rubber no yɛ nea wɔde silica a ɛyɛ wusiw ayɛ no sɛnea ɛbɛyɛ a n’ahoɔden ne n’ahoɔden a ɛyɛ den no ayɛ kɛse, na ɛma ɛyɛ nea wotumi paw no pii ma nsɔano, gaskets, ne nneɛma a wɔde siw ano. Sɛ́ ebia wowɔ kar, ahunmu, anaa anyinam ahoɔden adwuma mu no, saa silicone rɔba yi betumi ama woayɛ adwuma a wuhia.


Aduru no wɔ ahorow pii, na wɔayɛ emu biara sɛnea ɛbɛyɛ a ebedu ahwehwɛde pɔtee bi a egyina sɛnea ɛyɛ den, ɛyɛ den, ne nneɛma atitiriw afoforo so. Esiane sɛ saa rɔba yi tumi gyina ano kɛse na ɛtumi tetew mu yiye nti, ɛyɛ adwuma yiye wɔ tebea horow a ɛyɛ den na ɛyɛ den kɛse mpo mu. Ɛsan nso tumi gyina ɔhyew a ɛba fam ne nea ɛkɔ soro nyinaa ano, na ɛhwɛ hu sɛ ɛkɔ so yɛ nea wotumi de ho to so wɔ ɔhyew a ɛtrɛw mu.


Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175° x 5min x 15MPa.


Nneɛma a wɔyɛ no parameters
Adwadeɛ GA-3033 na ɛwɔ hɔ
GA-3043 na ɛwɔ hɔ GA-3053 na ɛwɔ hɔ GA-3063 na ɛwɔ hɔ GA-3073 na ɛwɔ hɔ
Mmaeɛ Ɛyɛ nea ɛyɛ translucent
Williamplasticity a wɔde yɛ nneɛma
140
180
200
230
260
Nneɛma a ɛyɛ den (Shor
30
40
50
60
70
Nsuo a ɛyɛ den(g/cm3) . 1.08
1.10
1.13
1.16
1.18
Ahoɔden a wɔde twe ade (MPa) .

5.5
9
9
9
8.5
Ntrɛwmu(%) . 550
500
400
300
200
Ahoɔden a ɛtetew mu (kN/m) . 12
20
20
20
20
Rebound(%) a ɛsan ba.
60
55
55
50
50

Silicone Rɔba a Ɛyɛ Den a Ɛkorɔn


GA-30 × 3 Silicone Rɔba a ɛwɔ ahoɔden a ɛkorɔn (HCR) - Nneɛma atitiriw


Wɔ Shanghai Herchy Rubber Co., Ltd., yɛyɛ titiriw wɔ silicone rɔba nneɛma a ɛkorɔn te sɛ GA-30 × 3 Silicone Rubber a fumed silica, engineered ma ɛkorɔn resilience ne adwumayɛ a ɛda nsow. Saa elastomer yi ye ma nnwuma a ɛhwehwɛ sɛ wɔde nsɔano ano aduru a ɛkɔ anim, ɛtra hɔ kyɛ, ne mfiri a ɛkyɛn so.


High Resilience ma Nsakrae a Ɛtra Hɔ Bere Tenten

GA-30×3 Silicone Rubber yɛ nea wɔayɛ ama rebound a ɛkorɔn, a ɛma ahoɔden a ɛkorɔn ne nsakrae wɔ tebea horow a ɛyɛ nnam mu. Ɛyɛ mfaso titiriw wɔ sealing components, vibration dampeners, ne high-end gaskets, baabi a elasticity ne ahoɔden ho hia.


Mfiridwuma mu Ahoɔden a Ɛkyɛn So

Esiane sɛ saa silicone rɔba yi tumi twetwe ade kɛse na ɛko tia nusu a ɛyɛ nwonwa nti, ɛma ɛtra hɔ kyɛ. Sɛnea ɛyɛ den no ma ɛyɛ nea ɛfata ma nnwuma te sɛ kar, ahunmu, ne ɛlɛtrɔnik mfiri, baabi a ɛsɛ sɛ nneɛma gyina tebea horow a emu yɛ den ano.


Wide Ɔhyew a Ɛko Tia

GA-30×3 Silicone Rubber ma ahoɔden soronko a ɛyɛ den wɔ ɔhyew a ɛtrɛw mu, fi -40°C kosi 200°C. Eyi ma ɛyɛ nea eye ma dwumadie a ɛhwehwɛ sɛ wɔyɛ adwuma daa wɔ ɔhyew a ɛsakrasakra mu, te sɛ kar nsɔano ne nhama a wɔde siw nsu ano mu.


Nneɛma a Wɔde Di Dwuma a Ɛda Nsow

Yɛn silicone rɔba no yɛ nea wotumi de di dwuma wɔ akwan horow so kɛse wɔ sɛnea wotumi yɛ ho adwuma no mu. Sɛ́ ɛyɛ nea wɔde yɛ molding, extrusion, anaa compression no, GA-30×3 boa akwan horow a wɔfa so yɛ nneɛma, na ɛhwɛ hu sɛ wubetumi ayɛ afã horow a ɛyɛ pɛpɛɛpɛ a ɛnyɛ den.


Wiase Nyinaa Adansedi a Wɔde Di Dwuma

Shanghai Herchy Rubber Co., Ltd. hwɛ hu sɛ GA-30×3 Silicone Rubber di nnwuma gyinapɛn te sɛ RoHS, REACH, ne LFGB adansedi ahorow so. Eyi ma ɛyɛ nea ahobammɔ wom na wotumi de ho to so a wɔpaw ma dwumadie a ɛho hia wɔ aduane, aduruyɛ, ne ɛlɛtrɔnik mfiridwuma mu a ɛhia sɛ wɔdi mmara so katee.


Onyin ne Nneɛma a Atwa Yɛn Ho Ahyia a Ɛyɛ Den a Wɔko tia

Wɔayɛ saa ade yi sɛnea ɛbɛyɛ a ɛbɛko atia onyin, UV hann, ozone, ne oxidation, na ɛma ɛyɛ den kɛse bere a bere kɔ so no. Sɛ́ ebia wɔde di dwuma wɔ abɔnten anaasɛ nea ɛhyɛ kɛse mu no, GA-30×3 Silicone Rubber kura ne su ahorow mu na ɛma adwumayɛ a wotumi de ho to so bere tenten.


Nneɛma a Wɔde Di Dwuma Wɔ Nnwuma Ahorow Nyinaa Mu

GA-30×3 Silicone Rubber yɛ papa ma dwumadie ahodoɔ, a nea ɛka ho ne nneɛma a ɛkorɔn a wɔde kata so, vibration pads, gaskets, ne shock absorbers. Wɔde di dwuma kɛse wɔ nnwuma te sɛ kar, ahunmu, anyinam ahoɔden, ne nnuruyɛ mfiri a wɔyɛ mu.


Nneɛma a Wɔyɛ a Ɛnyɛ Nneɛma a Atwa Yɛn Ho Ahyia

Yɛde nneɛma a ɛbɛkɔ so atra hɔ daa di kan wɔ yɛn nneɛma a yɛyɛ mu. Wɔde akwan a ɛnyɛ nea ɛmma nneɛma a atwa yɛn ho ahyia na ɛyɛ GA-30×3 Silicone Rubber, na ɛtew nneɛma a atwa yɛn ho ahyia so a ɛmma adwumayɛ nsɛe. Eyi ne yɛn bo a yɛasi sɛ yɛde nneɛma a ɛyɛ papa na ɛnyɛ nea ɛmma nneɛma a atwa yɛn ho ahyia nyinaa bɛkɔ no hyia.


Customizable Hardness ma Ahiade Pɔtee

Ɛwɔ hardness levels ahorow mu, efi 30 kosi 70 Shore A, GA-30×3 betumi ayɛ nea ɛfata ma ɛne w’ahiade pɔtee no ahyia. Sɛ́ ebia wuhia ade a ɛyɛ mmerɛw na ama woatumi ayɛ nsakrae anaasɛ rɔba a ɛyɛ den na ama ayɛ den no, wobetumi ayɛ saa ade yi ma ɛne w’adwuma no ahiade ahorow ahyia.


Esiane sɛ GA-30×3 Silicone Rubber with High Resilience (HCR) tumi gyina ano kɛse, mfiridwuma mu ahoɔden, na ɛyɛ adwuma pii nti, ɛyɛ nea eye ma nnwuma a wɔrehwehwɛ rɔba ano aduru a ɛkɔ anim. Di yɛn ho nkɔmmɔ na hwehwɛ sɛnea yɛn rɔba nneɛma a wɔayɛ no sɛnea wɔpɛ no betumi adi w’ahiade pɔtee ho dwuma.


Nsɛmmisa ne Mmuae a Wɔtaa Bisa


Q1: Dɛn na wɔde GA-30×3 Silicone Rubber di dwuma?
A1: GA-30 × 3 Silicone Rubber yɛ nea eye ma nsɔano, gaskets, wosow dampeners, ne adwumayɛ a ɛkorɔn elastomer applications.


Q2: So GA-30 × 3 Silicone Rubber yɛ nea wotumi sesa ma ahiade pɔtee bi?
A2: Yiw, yɛde customization options ma hardness ne agyapade afoforo ma ɛne wo project ahwehwɛde ahorow hyia.


Q3: Nnwuma bɛn na wonya mfaso fi GA-30×3 Silicone Rubber mu?
A3: Wɔtaa de di dwuma wɔ kar, ahunmu, aduruyɛ, ne ɛlɛtrɔnik mfiridwuma mu de yɛ nneɛma a ɛyɛ den.


Q4: So GA-30×3 Silicone Rubber di nnwuma gyinapɛn ahorow so?
A4: Yiw, ɛne adansedi ahorow te sɛ RoHS, REACH, ne LFGB hyia, na ɛhwɛ hu sɛ wɔde bedi dwuma a ahobammɔ wom, wotumi de ho to so wɔ nnwuma ahorow mu.


Q5: Ɔhyew bɛn na GA-30×3 Silicone Rubber betumi agyina ano?
A5: GA-30 × 3 Silicone Rubber kura ne dwumadi mu wɔ ɔhyew a ɛtrɛw, a eye ma nneɛma a atwa yɛn ho ahyia a emu yɛ den.


Q6: Ɔkwan bɛn so na GA-30×3 Silicone Rubber gyina onyin ne UV a ɛda adi no ano?
A6: Sɛnea ɛko tia onyin, UV, ne ozone a ɛkorɔn no ma ɛtra hɔ kyɛ na ɛyɛ adwuma wɔ tebea horow a emu yɛ den mu.


Q7: So wobetumi de GA-30×3 Silicone Rubber adi dwuma wɔ abɔnten so nneɛma mu?
A7: Yiw, UV ne ozone a ɛko tia ade no ma ɛfata sɛ wɔde di dwuma wɔ abɔnten ne nea ɛhyɛ kɛse.


Q8: So GA-30×3 Silicone Rubber nsɛe nneɛma a atwa yɛn ho ahyia?
A8: Yiw, wɔde akwan a ɛnyɛ nea ɛmma nneɛma a atwa yɛn ho ahyia na ɛyɛ, a ɛboa elastomer ano aduru a ɛtra hɔ daa, a ɛyɛ papa.

Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.