I-GA-31×0 Irabha ye-Silicone yenzelwe izinhlelo zokusebenza ezisebenza kahle kakhulu. Ifaka ukumelana nezinyembezi okuthuthukisiwe kanye nokuqina, okuyenza ifaneleke ezinhlobonhlobo zezimboni. Lo mkhiqizo ukhiqizwa i-Shanghai Herchy Rubber Co., Ltd., umkhiqizi ohamba phambili wama-silicone elastomers. Uchungechunge lwe-GA-31×0 luqiniswa nge-silica evuthayo ukuze kuthuthukiswe amandla alo okudabula, kuqinisekiswe ukusebenza okuhlala isikhathi eside ezindaweni ezinzima.
Umkhiqizo utholakala ngamaleveli obulukhuni amahlanu ahlukene, kusukela ku-30 Shore A kuya ku-70 Shore A. Lokhu kunikeza ukuguquguquka kwezinhlelo zokusebenza ezihlukahlukene, kusukela kuma-flexible seals kuya ezingxenyeni eziqinile. Uchungechunge lwe-GA-31 × 0 luphinde luziqhayisa ngezakhiwo ezinhle kakhulu zokwelula, ezivumela izinto ukuthi zinwebe ngaphansi kwengcindezi ngaphandle kokuyekethisa amandla ako.
Ngebanga lokuminyana elisuka ku-1.08 g/cm³ ukuya ku-1.20 g/cm³, irabha ye-silicone ye-GA-31×0 ayisindi futhi ihlala isikhathi eside. Inikeza amandla okuqina angaguquguquki, iqinisekisa ukuthi ingakwazi ukubhekana nokucindezeleka komshini okuhlukahlukene. Lokhu kuyenza ibe into efanelekile yezimoto, i-aerospace, nezingxenye zikagesi, lapho ukuqina nokuvumelana nezimo kubalulekile.
Irabha ye-silicone iyashintshashintsha ngokubukeka, ivumela ukuhlolwa nokuhlanganiswa kwemikhiqizo ecacile noma ecace kancane. Iphinde inikeze ukumelana okuhle kakhulu nezimo zemvelo ezinzima, okuyenza ifaneleke izicelo zangaphandle noma zezimboni.
Uchungechunge lwe-GA-31×0 luyisinqumo esithembekile nesihlala isikhathi eside sanoma iyiphi iphrojekthi edinga amandla aphezulu okudabula nokusebenza okuhle kakhulu.
Isivivinyo: 1% we-ejenti yokwelapha (50% unamathisele we-DBPMH ku-silicone gum), 175° x5minx15MPa
| Imingcele yomkhiqizo | |||||
| Umkhiqizo | GA-3130 |
GA-3140 | GA-3150 | GA-3160 | GA-3170 |
| Ukubukeka | I-Translucent | ||||
| Williamplasticity |
140 |
180 |
210 |
240 |
280 |
| Ukuqina (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Ukuminyana(g/cm3) | 1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
| Amandla e-Tensile (MPa) |
8 |
8 |
9 |
9 |
9 |
| Ubude(%) | 900 |
750 |
750 |
650 |
600 |
| Amandla wezinyembezi (kN/m) | 30 |
35 |
45 |
45 |
40 |
Leli thebula linikeza imininingwane ebalulekile yochungechunge lwemikhiqizo yerabha ye-silicone ye-GA-31 × 0. Okuhlukile ngakunye phakathi kochungechunge kunikeza izakhiwo ezihlukile zokusebenzisa ukuze zivumelane nezidingo ezahlukahlukene zohlelo lokusebenza. Kungakhathaliseki ukuthi udinga ukuguquguquka, ukuqina, noma ukumelana okuphezulu kwezinyembezi, i-GA-31 × 0 irabha ye-silicone iyisixazululo esithembekile.

Uchungechunge lwerabha ye-silicone ye-GA-31 × 0 yakhelwe ukuletha ukuqina kokusebenza okuphezulu kwezinhlelo eziningi zokusebenza zezimboni. Ngezansi izici ezibalulekile zalokhu okubalulekile okuthuthukisiwe, okulungele imikhakha efunwa kakhulu njengezingxenye zezimoto, i-aerospace, insulation kagesi, nokunye.
I-GA-31 × 0 irabha ye-silicone inikezela ukumelana nezinyembezi okukhethekile, okuyenza ibe yinketho efanelekile yezingxenye ezidinga ukubekezelela ukucindezeleka okuphezulu kwemishini. Amandla ayo aphakeme okudabula ayenza ifaneleke kakhulu kuma-seal anamandla, izingxenye zezimoto, ama-gaskets, nemikhiqizo yenjoloba yezimboni echayeka ezimeni ezinzima.
Le rabha ye-silicone iklanywe ngokukwazi ukusetshenzwa kahle, ivumela ukubumba nokubunjwa kalula. Kungakhathaliseki ukuthi ukhiqiza izingxenye zenjoloba zangokwezifiso noma amaqoqo amakhulu, ukusebenziseka kalula kwe-GA-31×0 kusiza ukunciphisa isikhathi sokukhiqiza nezindleko, kukwenze kube ukukhetha okuncanyelwayo kokukhiqizwa kwevolumu ephezulu ezimbonini ezifana nezezimoto, i-aerospace, nezokwelapha.
Ithobelana ngokugcwele namazinga omhlaba afana ne-RoHS, REACH, ne-LFGB, i-GA-31×0 irabha ye-silicone iqinisekisa ukuthi ihlangabezana nemithetho yemvelo kanye nezitifiketi zokuphepha. Lokhu kuyenza ifanelekele izigxivizo zezimoto, izingxenye zedivayisi yezokwelapha, nezinye izimboni ezithobelayo kakhulu ezidinga izinto eziqinisekisiwe.
Irabha ye-silicone ye-GA-31×0 iguquguquka kakhulu futhi isetshenziswa kabanzi ezimbonini ezifana nokukhiqiza izimoto, i-aerospace, electronics, kanye nemishini yezokwelapha. Izici zayo zokusebenza okuphezulu, okuhlanganisa ukuzinza kwe-thermal, ukumelana namakhemikhali, kanye nokuguquguquka, kuyenza ifaneleke kuma-seal, ama-gaskets, ama-insulators, nezinye izinto ezibucayi ezindaweni ezidinga kakhulu.
Itholakala kuhlu olubanzi lwezinketho zokuqina kusuka ku-30 kuya ku-70 Shore A, i-GA-31×0 irabha ye-silicone ingahle ihambisane nezidingo zakho zohlelo lokusebenza. Kungakhathaliseki ukuthi udinga inhlanganisela yerabha eguquguqukayo noma i-elastomer eqinile, i-GA-31×0 inikeza isixazululo ongase usenze ngokwezifiso ezimbonini ezihlukahlukene ezifana nokufakwa kwezimoto nokufakwa kukagesi.
Ngezakhiwo ezihlaba umxhwele zokwelula, irabha ye-silicone ye-GA-31 × 0 inganwebeka ifike ku-900% ngaphandle kokuyekethisa amandla. Lokhu kuyenza ilungele izingxenye ezidinga ukuguquguquka nokuqina, njengezindandatho zokuvala, ama-gaskets, nezingxenye ezidinga ukubekezelela ubunzima bemishini ezindaweni ezidinga ukunwebeka okuphezulu.
I-GA-31×0 irabha ye-silicone yenza kahle ngaphansi kwezimo ezimbi kakhulu, okuhlanganisa izinga lokushisa eliphezulu nokuchayeka emisebeni ye-UV, i-ozone, namakhemikhali. Ilungele izinhlelo zokusebenza lapho ukusebenza okuhlala isikhathi eside kubalulekile, njengezigxivizo zangaphandle, izingxenye zezimoto, nezingxenye ze-aerospace.
Ukubonakala okuguquguqukayo kwerabha ye-silicone ye-GA-31×0 kuvumela ukuhlola okubonakalayo kalula ngesikhathi sokukhiqiza, kusiza ukuqinisekisa ukuthi yonke ingxenye ihlangabezana nezindinganiso eziphakeme zokulawula ikhwalithi. Lokhu kubeka izinto ngale kukwenza kusebenziseke ikakhulukazi ezimbonini ezifana ne-elekthronikhi nemishini yezokwelapha lapho ukunemba nokungaguquguquki kubalulekile.
I-Q1: Yiziphi izimboni ezisebenzisa i-GA-31 × 0 I-Silicone Rubber nge-High Tear Strength?
I-A1: I-GA-31×0 ilungele izimoto, i-aerospace, i-electronics, imishini yezokwelapha, nezinhlelo zokusebenza zezimboni.
I-Q2: Ingabe i-GA-31 × 0 I-Silicone Rubber ingenziwa ngezifiso izinhlelo zokusebenza ezithile?
I-A2: Yebo, sinikeza izixazululo zenjoloba ze-silicone ezenziwe ngokwezifiso ngobulukhuni, ukwakheka, nombala wezimboni ezihlukahlukene.
Q3: Isebenza kanjani i-GA-31 × 0 Silicone Rubber emazingeni okushisa aphezulu?
I-A3: Irabha ye-silicone ye-GA-31 × 0 inikeza ukuzinza okuphezulu kokushisa, ilungele izimpawu zokushisa okuphezulu nama-gaskets.
I-Q4: Yiziphi izitifiketi i-GA-31 × 0 Silicone Rubber ehlangana nazo?
I-A4: Irabha ye-silicone ye-GA-31 × 0 ihambisana ne-RoHS, REACH, ne-LFGB, iqinisekisa izindinganiso ezinobungani bemvelo.
I-Q5: Yiziphi izinzuzo ezibalulekile zokusebenzisa i-GA-31 × 0 I-Silicone Rubber?
I-A5: I-GA-31×0 inikeza amandla aphezulu okudabula, ukuguquguquka okuhle kakhulu, nokumelana namakhemikhali okuvelele ukusetshenziswa kwezimboni.
I-Q6: Ingabe i-GA-31 × 0 I-Silicone Rubber ifaneleka ekufakweni uphawu kwezimoto?
I-A6: Yebo, ilungele ama-seal ezimoto, ama-gaskets, nezingxenye zenjoloba ezisebenza kahle ekukhiqizeni izimoto.
I-Q7: Ikwazi ukumelana ne-GA-31 × 0 Irabha yeSilicone kumakhemikhali nasemisebeni ye-UV?
I-A7: I-GA-31 × 0 inikeza ukumelana kwamakhemikhali okuqinile nokuzinza kwe-UV, okuyenza ilungele izingxenye zenjoloba zangaphandle nezezimoto.
I-Q8: Ingabe i-GA-31 × 0 I-Silicone Rubber ingasetshenziswa kumadivayisi wezokwelapha?
I-A8: Yebo, i-GA-31×0 ihlangabezana nezitifiketi zokuphepha futhi ilungele izingxenye zedivayisi yezokwelapha kanye nezicelo zenjoloba ezisezingeni lezokwelapha.