Ua hoʻolālā ʻia ʻo GA-31×0 Silicone rubber no nā noi hana kiʻekiʻe. Hōʻike ia i ke kūpaʻa waimaka kiʻekiʻe a me ka lōʻihi, e kūpono ana ia no kahi ākea o nā ʻoihana. Hana ʻia kēia huahana e Shanghai Herchy Rubber Co., Ltd., kahi mea hana nui o nā elastomers silicone. Hoʻoikaika ʻia ka moʻo GA-31×0 me ka silica fumed e hoʻonui i kona ikaika waimaka, e hōʻoia ana i ka hana lōʻihi i nā kaiapuni koi.
Loaʻa ka huahana i ʻelima mau pae paʻakikī, mai 30 Shore A a hiki i 70 Shore A. Hāʻawi kēia i ka versatility no nā noi like ʻole, mai nā sila maʻalahi a hiki i nā mea ʻoi aku ka paʻakikī. Hāʻawi ka GA-31 × 0 i nā waiwai elongation maikaʻi loa, e ʻae ana i ka mea e hoʻolōʻihi i lalo o ke koʻikoʻi me ka ʻole o kona ikaika.
Me kahi ākea ākea mai 1.08 g/cm³ a hiki i ka 1.20 g/cm³, ʻo GA-31×0 silicone rubber ka māmā a me ka lōʻihi. Hāʻawi ia i ka ikaika tensile mau, e hōʻoiaʻiʻo ana hiki iā ia ke mālama i nā ʻano koʻikoʻi mechanical. Hana ia i mea kūpono no ka automotive, aerospace, a me nā ʻāpana uila, kahi mea koʻikoʻi ka lōʻihi a me ka maʻalahi.
He translucent ka ʻili silicone i ka nānā ʻana, e ʻae i ka nānā maʻalahi a me ka hoʻohui ʻana i nā huahana a i ʻole semi-clear. Hāʻawi ia i ke kū'ē maikaʻi loa i nā kūlana kūlohelohe koʻikoʻi, e kūpono ana i nā noi waho a i ʻole nā hana ʻoihana.
ʻO ka moʻo GA-31×0 he mea hilinaʻi a paʻa hoʻi ke koho waiwai no kēlā me kēia papahana e koi ana i ka ikaika waimaka kiʻekiʻe a me ka hana maikaʻi loa.
Ho'āʻo: 1% o ka lāʻau lapaʻau (50% paʻi o DBPMH i ka silicone gum), 175° x5minx15MPa
| Nā palena huahana | |||||
| Huahana | GA-3130 |
GA-3140 | GA-3150 | GA-3160 | GA-3170 |
| Ka nana aku | Alohilohi | ||||
| Williamplasticity |
140 |
180 |
210 |
240 |
280 |
| Paʻakikī (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Māmā (g/cm3) | 1.08 |
1.11 |
1.14 |
1.17 |
1.20 |
| Ka ikaika uʻi (MPa) |
8 |
8 |
9 |
9 |
9 |
| Elongation(%) | 900 |
750 |
750 |
650 |
600 |
| Kaha waimaka (kN/m) | 30 |
35 |
45 |
45 |
40 |
Hāʻawi kēia papa ʻaina i nā kikoʻī koʻikoʻi o nā huahana silicone rubber series GA-31×0. Hāʻawi kēlā me kēia ʻano like ʻole i loko o ka moʻo i nā ʻano mechanical like ʻole e kūpono i nā pono noi. Inā makemake ʻoe i ka maʻalahi, ka lōʻihi, a i ʻole ke kūpaʻa waimaka kiʻekiʻe, ʻo GA-31×0 silicone rubber kahi hopena hilinaʻi.

ʻO ka GA-31 × 0 silicone rubber series ua hana ʻia e hoʻopuka i ka lōʻihi o ka hana kiʻekiʻe no kahi ākea o nā noi ʻoihana. Aia ma lalo iho nā hiʻohiʻona nui o kēia mea holomua, kūpono no nā ʻāpana koi e like me nā ʻāpana automotive, aerospace, insulation uila, a me nā mea hou aku.
Hāʻawi ʻo GA-31×0 silicone rubber i ke kūpaʻa waimaka maikaʻi loa, e hana ana i ke koho kūpono loa no nā mea pono e hoʻomanawanui i ke koʻikoʻi mechanical. ʻO kona ikaika haʻalulu maikaʻi e kūpono ia no nā sila ikaika kiʻekiʻe, nā ʻāpana kaʻa, nā gaskets, a me nā huahana lāʻau ʻenehana i ʻike ʻia i nā kūlana paʻakikī.
Hoʻolālā ʻia kēia ʻōpala silicone me ke kaʻina hana koʻikoʻi, e ʻae ai i ka hoʻoheheʻe maʻalahi a me ke ʻano. Inā ʻoe e hana ana i nā ʻāpana kopa maʻamau a i ʻole nā pūʻulu nui, ʻo ka maʻalahi o ka hana ʻana o GA-31×0 e kōkua i ka hōʻemi ʻana i ka manawa hana a me nā kumukūʻai, e hoʻolilo iā ia i koho koho no ka hana kiʻekiʻe i nā ʻoihana e like me ka automotive, aerospace, a me nā lāʻau lapaʻau.
Hoʻokō piha i nā kūlana honua e like me RoHS, REACH, a me LFGB, ʻo ka GA-31 × 0 silicone rubber e hōʻoia i ka hoʻokō ʻana i nā lula kaiapuni a me nā palapala hōʻoia palekana. He mea kūpono kēia no nā sila kaʻa, nā ʻāpana lāʻau lapaʻau, a me nā ʻoihana hoʻokō kiʻekiʻe e koi ana i nā mea i hōʻoia ʻia.
ʻO GA-31×0 silicone rubber ka mea maʻalahi a hoʻohana nui ʻia i nā ʻoihana e like me ka hana ʻana o ka automotive, aerospace, electronics, a me nā mea lapaʻau. ʻO kāna mau hiʻohiʻona hana kiʻekiʻe, e komo pū ana me ke kūpaʻa wela, ka pale ʻana i ke kemika, a me ka maʻalahi, e kūpono ia no nā sila, gaskets, insulators, a me nā mea koʻikoʻi ʻē aʻe i nā wahi koi.
Loaʻa i loko o kahi ākea o nā koho paʻakikī mai 30 a 70 Shore A, GA-31 × 0 silicone rubber hiki ke hoʻohālikelike ʻia i kāu koi noi kikoʻī. Inā makemake ʻoe i kahi pūhui kaila maʻalahi a i ʻole ka elastomer ʻoi aku ka paʻakikī, hāʻawi ʻo GA-31 × 0 i kahi hopena maʻamau no nā ʻoihana like ʻole e like me ka automotive a me ka insulation uila.
Me nā waiwai elongation maikaʻi loa, hiki i ka rubber silicone GA-31 × 0 ke kau aku a hiki i 900% me ka ʻole o ka hoʻololi ʻana i ka ikaika. He mea kūpono kēia no nā ʻāpana e pono ai ka maʻalahi a me ke kūpaʻa, e like me ke apo sealing, gaskets, a me nā ʻāpana e pono ai ke hoʻomanawanui i ke koʻikoʻi mechanical i nā wahi e koi ai i ka elasticity kiʻekiʻe.
Hana maikaʻi ʻo GA-31×0 silicone rubber ma lalo o nā kūlana koʻikoʻi, me nā wela kiʻekiʻe a me ka ʻike ʻana i ka radiation UV, ka ozone, a me nā kemika. He kūpono ia no nā noi kahi mea koʻikoʻi ka hana lōʻihi, e like me nā sila waho, nā ʻāpana kaʻa, a me nā ʻāpana aerospace.
ʻO ka hiʻohiʻona translucent o GA-31 × 0 silicone rubber hiki ke nānā maʻalahi i ka wā o ka hana ʻana, e kōkua ana i ka hoʻokō ʻana o kēlā me kēia ʻāpana i nā kūlana mana kiʻekiʻe loa. Hoʻohana pono kēia ʻike i nā ʻoihana e like me ka uila a me nā mea lapaʻau kahi mea nui o ka pololei a me ka kūlike.
Q1: He aha nā ʻoihana e hoʻohana ana i ka GA-31 × 0 Silicone Rubber me ka ikaika waimaka kiʻekiʻe?
A1: ʻO GA-31×0 ka mea kūpono no ka kaʻa, aerospace, uila, nā mea lapaʻau, a me nā noi ʻoihana.
Q2: Hiki iā GA-31×0 Silicone Rubber ke hoʻopilikino ʻia no nā noi kikoʻī?
A2: ʻAe, hāʻawi mākou i nā hoʻonā silicone rubber maʻamau i ka paʻakikī, ka hana ʻana, a me ke kala no nā ʻoihana like ʻole.
Q3: Pehea e hana ai ʻo GA-31×0 Silicone Rubber i nā mahana wela?
A3: GA-31×0 silicone rubber hāʻawi i ke kūpaʻa wela kiʻekiʻe, kūpono no nā sila wela a me nā gaskets.
Q4: He aha nā palapala hōʻoia e hui ai ʻo GA-31×0 Silicone Rubber?
A4: ʻO GA-31×0 silicone rubber e hoʻokō me RoHS, REACH, a me LFGB, e hōʻoiaʻiʻo ana i nā kūlana pili i ke kaiapuni.
Q5: He aha nā pōmaikaʻi nui o ka hoʻohana ʻana iā GA-31×0 Silicone Rubber?
A5: Hāʻawi ʻo GA-31×0 i ka ikaika waimaka kiʻekiʻe, hiki ke hoʻololi maikaʻi, a me ke kūpaʻa kemika koʻikoʻi no ka hoʻohana ʻana i ka ʻoihana.
Q6: Ua kūpono anei ʻo GA-31×0 Silicone Rubber no nā noi hoʻopaʻa kaʻa?
A6: ʻAe, kūpono ia no nā sila kaʻa kaʻa, gaskets, a me nā ʻāpana pahu hana kiʻekiʻe i ka hana kaʻa.
Q7: Pehea ka pale ʻana o GA-31 × 0 Silicone Rubber i nā kemika a me ka radiation UV?
A7: Hāʻawi ʻo GA-31×0 i ke kūpaʻa kemika ikaika a me ka paʻa ʻana o UV, i mea kūpono no nā ʻāpana o waho a me nā kaʻa.
Q8: Hiki ke hoʻohana ʻia ʻo GA-31×0 Silicone Rubber i nā lāʻau lapaʻau?
A8: ʻAe, hui ʻo GA-31×0 i nā palapala hōʻoia palekana a he kūpono ia no nā ʻāpana lāʻau lapaʻau a me nā noi lāʻau lapaʻau.