GA-30×3
Hercsekele
| Boteng: | |
|---|---|
| Bongata: | |
Ho Shanghai Herchy Rubber Co., Ltd., re fana ka GA-30 × 3 Silicone Rubber (Silica e tukang) e nang le High Resilience (HCR), elastomer e sebetsang hantle e etselitsoeng ho fihlela litlhoko tse boima tsa liindasteri tse fapaneng. Rabara ena e loketse lisebelisoa tse hlokang thepa e phahameng ea mochine le ho tšoarella, esita le libakeng tse feteletseng.
GA-30 × 3 Silicone Rubber ea rona e entsoe ka silika e tukang ho matlafatsa matla a eona le ho tiea, ho e etsa khetho e fapaneng bakeng sa litiiso, likhase le lisebelisoa tsa ho kenya letsoho. Hore na o indastering ea likoloi, ea sefofane kapa ea motlakase, rabara ena ea silicone e ka fana ka ts'ebetso eo u e hlokang.
Sehlahisoa se fumaneha ka mefuta e 'maloa, e' ngoe le e 'ngoe e etselitsoe ho fihlela litlhoko tse ikhethileng tse ipapisitseng le boima, boima le lisebelisoa tse ling tsa bohlokoa. Ka ho tiea ha eona ho phahameng le matla a babatsehang a ho tabola, rabara ena e sebetsa hantle esita le tlas'a maemo a matla le a phahameng a khatello ea kelello. E boetse e khona ho mamella mocheso o tlase le o phahameng, ho netefatsa hore e lula e tšepahala ho pholletsa le mefuta e mengata ea mocheso.
Teko: 1% ea moemeli oa phekolo (50% peista ea DBPMH ka silicone gum), 175 ° x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | |||||
| Sehlahisoa | GA-3033 |
GA-3043 | GA-3053 | GA-3063 | GA-3073 |
| Ponahalo | Translucent | ||||
| Williamplasticity |
140 |
180 |
200 |
230 |
260 |
| Ho thatafala (LebopoA) |
30 |
40 |
50 |
60 |
70 |
| Boima ba 'mele(g/cm3) | 1.08 |
1.10 |
1.13 |
1.16 |
1.18 |
| Tensile Matla (MPa) |
5.5 |
9 |
9 |
9 |
8.5 |
| Elongation(%) | 550 |
500 |
400 |
300 |
200 |
| Matla a ho lla (kN/m) | 12 |
20 |
20 |
20 |
20 |
| Rebound(%) |
60 |
55 |
55 |
50 |
50 |

Ho Shanghai Herchy Rubber Co., Ltd., re ipabola ka ho fana ka lihlahisoa tsa rabara tsa silicone tsa boleng bo holimo joalo ka GA-30 × 3 Silicone Rubber e nang le silika e tukang, e etselitsoeng ho mamella maemo a holimo le ts'ebetso e ikhethang. Elastomer ena e loketse liindasteri tse hlokang tharollo e tsoetseng pele ea ho tiisa, ho tšoarella, le thepa e ntle ea mochini.
GA-30 × 3 Silicone Rubber e entsoe bakeng sa rebound e phahameng, e fana ka botsitso bo phahameng le ho feto-fetoha ha maemo tlas'a maemo a matla. E bohlokoa haholo ho likarolo tsa ho tiisa, li-dampeners tsa vibration, le li-gaskets tse phahameng, moo elasticity le matla li leng bohlokoa.
Ka matla a phahameng a tsitsipano le khanyetso e khahlang ea meokho, rabara ena ea silicone e netefatsa ho tšoarella ha nako e telele. Sebopeho sa eona se matla se etsa hore e be e loketseng indastering e kang ea likoloi, sefofane le lisebelisoa tsa elektroniki, moo thepa e tlamehang ho mamella maemo a thata.
GA-30×3 Silicone Rubber e fana ka botsitso bo ikhethang ho pholletsa le mocheso o pharaletseng, ho tloha ho -40°C ho isa ho 200°C. Sena se etsa hore e be khetho e nepahetseng bakeng sa lits'ebetso tse hlokang ts'ebetso e ts'oanang tlas'a mocheso o feto-fetohang, joalo ka litiiso tsa likoloi le lisebelisoa tsa cable.
Rabara ea rona ea silicone e sebetsa ka mokhoa o fapaneng haholo mabapi le ts'ebetso. Ebang ke ea ho bopa, extrusion, kapa compression, GA-30×3 e ts'ehetsa mekhoa e mengata ea tlhahiso, ho netefatsa hore o ka etsa likarolo tse nepahetseng habonolo.
Shanghai Herchy Rubber Co., Ltd. e netefatsa hore GA-30×3 Silicone Rubber e lumellana le maemo a indasteri a kang RoHS, REACH, le LFGB certification. Sena se etsa hore e be khetho e bolokehileng le e ts'epahalang bakeng sa lits'ebetso tsa bohlokoa indastering ea lijo, ea bongaka le ea lisebelisoa tsa elektroniki tse hlokang ho ba le taolo e tiileng ea taolo.
Sehlahisoa sena se etselitsoe ho hanela botsofali, leseli la UV, ozone le oxidation, e leng se etsang hore se tšoarelle nako e telele. Ebang e sebelisoa lits'ebetsong tsa kantle kapa tse apereng haholo, GA-30×3 Silicone Rubber e boloka thepa ea eona mme e fana ka ts'ebetso e tšepahalang ka nako e telele.
GA-30 × 3 Silicone Rubber e loketse mefuta e fapaneng ea lisebelisoa, ho kenyelletsa likarolo tsa ho tiisa tse phahameng, li-vibration pads, li-gaskets le li-absorbers tse tšosang. E sebelisoa haholo liindastering tse kang tsa likoloi, sefofane, motlakase le lisebelisoa tsa bongaka.
Re etelletsa pele ho tšoarella lits'ebetsong tsa rona tsa tlhahiso. GA-30 × 3 Silicone Rubber e hlahisoa ka mekhoa ea eco-friendly, e fokotsang tšusumetso ea tikoloho ntle le ho senya ts'ebetso. Sena se tsamaisana le boitlamo ba rona ba ho fana ka lihlahisoa tsa boleng bo holimo le tse ikarabellang tikolohong.
E fumaneha ka mefuta e fapaneng ea maemo a thata, ho tloha ho 30 ho isa ho 70 Shore A, GA-30×3 e ka hlophisoa ho fihlela litlhoko tsa hau tse ikhethileng. Ho sa tsotellehe hore na u hloka thepa e bonolo bakeng sa ho tenyetseha kapa rabara e tiileng bakeng sa ho tšoarella, sehlahisoa sena se ka etsoa ho lumellana le litlhoko tsa morero oa hau.
Ka botsitso ba eona bo phahameng, matla a mochini, le ho feto-fetoha ha maemo, GA-30 × 3 Silicone Rubber e nang le Resilience e Phahameng (HCR) ke khetho e nepahetseng bakeng sa liindasteri tse batlang tharollo e tsoetseng pele ea rabara. Ikopanye le rona ho hlahloba hore na lihlahisoa tsa rona tsa rabara tse lokiselitsoeng li ka khotsofatsa litlhoko tsa hau joang.
Q1: GA-30 × 3 Silicone Rubber e sebelisetsoa eng?
A1: GA-30×3 Silicone Rubber e loketse litiiso, li-gaskets, li-vibration dampeners, le lisebelisoa tse phahameng tsa elastomer.
Q2: Na GA-30 × 3 Silicone Rubber e ka etsoa ka litlhoko tse khethehileng?
A2: E, re fana ka likhetho tsa ho ikhethela ho thatafala le thepa e meng ho lumellana le litlhoko tsa morero oa hau.
Q3: Ke liindasteri life tse ruang molemo ho GA-30 × 3 Silicone Rubber?
A3: E sebelisoa hangata indastering ea likoloi, ea sefofane, ea bongaka le ea lisebelisoa tsa elektroniki bakeng sa lits'ebetso tse thata.
Q4: Na GA-30 × 3 Silicone Rubber e lumellana le litekanyetso tsa indasteri?
A4: E, e kopana le litifikeiti tse kang RoHS, REACH, le LFGB, ho netefatsa ts'ebeliso e bolokehileng, e tšepahalang liindastering tse fapaneng.
Q5: Ke mocheso ofe oa mocheso o ka mamellang GA-30 × 3 Silicone Rubber?
A5: GA-30 × 3 Silicone Rubber e boloka ts'ebetso ea eona ka mocheso o pharaletseng, o loketseng maemo a feteletseng.
Q6: GA-30 × 3 Silicone Rubber e hanela botsofali le ho pepeseha ha UV joang?
A6: Ho hanyetsa ha eona ho phahameng ho tsofalang, UV, le ozone ho netefatsa ho tšoarella ha nako e telele le ho sebetsa maemong a thata.
Q7: Na GA-30 × 3 Silicone Rubber e ka sebelisoa lits'ebetsong tsa kantle?
A7: E, khanyetso ea UV le ozone ea sehlahisoa e etsa hore e tšoanelehe bakeng sa lits'ebetso tsa kantle le tse phahameng.
Q8: Na GA-30 × 3 Rabara ea Silicone e na le tikoloho?
A8: E, e entsoe ka mekhoa e metle ea tikoloho, e tšehetsang litharollo tse tsitsitseng, tsa boleng bo holimo tsa elastomer.