A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 1.9%
Ethylene awm zat: 57.8%
Mooney viscosity: ML (1+4) 125°C 44
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 2.0%
Ethylene awm zat: 62%
Mooney viscosity: ML(1+4)125°C 53
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 7%
Ethylene awm zat: 52%
Mooney viscosity: ML (1+4) 100°C 45
Size: 25kg/bag
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 3.9%
Ethylene awm zat: 68.5%
Oil charge: 20%
Mooney viscosity: ML(1+4)125°C 41
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a awm dan: granule dum (transparent emaw translucent emaw)
Third monomer chi leh a awm zat: ENB,4%
Ethylene awm zat: 68.5%
Menni viscosity: ML(1+4)125°C 45
Size leh specification: 25kg/bag
Order tlem ber: 25kg
Packing: Boxed
A lan dan leh a dinhmun: var (transparent emaw translucent emaw) blocky
Third monomer chi leh a awm zat: ENB, 7.7%
Ethylene awm zat: 52.5%
Mooney viscosity: ML(1+4)125°C 65
Size: 25kg/bag
MOQ: 25kg
Packing: boxed