855
SABIC
SABIC® EPDM 855. Enkola y’okukozesa enkola ya SABIC®
| Ebiriwo: | |
|---|---|
| Omuwendo: | |
EBINTU EBIKOLA OKUKOLA:
SABIC EPDM 855 esobola okukozesebwa ku: ebiziyiza embeera y’obudde mu mmotoka, hoosi z’amazzi aganyogoza n’empewo mu mmotoka, gaasikiti z’amakolero ne O-rings, gaasikiti z’ebyuma eby’okwoza.
EMIRIMU GY’EBINTU EBY’ENJAWULO:
| EBY'BWANANNYINI | EMIRIMU EGY’ENJAWULO | UNITS | ENGERI Y’OKUKEBERA |
| EBINTU EBIKWATA KU POLYMER | |||
| Obuzito bwa Mooney | |||
| ML 1+4, 125 °C (1) . | 80 |
MU |
ASTMD 1646. Enkola ya ASTMD |
| Ebirimu Ethylene | 55 |
wt.% |
ASTMD 3900. Enkola ya ASTMD |
| Ebirimu Ethylidene Norbornene (ENB) Ebirimu | 5.2 |
wt.% | ASTMD 6047 |
OBUBONERO:
SABIC EPDM 855 ekoleddwa ku : okufulumya mu ngeri ennyangu era ey’amangu, okulongoosa okutabula, okukwata ekyuma n’ebintu ebirabika, okulongoosa okukuuma amafuta n’okuwonya okufuumuuka mu bikozesebwa, eby’obugagga ebirungi ennyo eby’ebbugumu eri wansi n’okuteekebwa mu kunyigirizibwa n’okuwonya amangu.
OKUTEEKA N'OKUKWATA:
SABIC EPDM 855 erina okuterekebwa mu paakingi yaayo eyasooka ku bbugumu eriri mu mbeera enkalu; okubeera mu bbugumu, ekitangaala kya ultraviolet n’omusana obutereevu kulina okwewalibwa. Mu mbeera entuufu ey’okutereka, ekintu kino kibeera kinywevu okumala emyezi 24 okuva ku lunaku lwe kyakolebwa. SABIC tejja kwongera ku ggaranti yaayo ng’embeera y’okutereka temala ekiyinza okuvaako omutindo okwonooneka ng’okukaluba kw’ebintu oba okukyusa langi ekiyinza okuvaamu okukola ebintu mu ngeri emala.
OKWEGAANA:
Okutunda kwonna okukolebwa SABIC, amakampuni gaayo n'abakwatibwako (buli emu 'omutunzi'), kukolebwa wansi w'obukwakkulizo bw'okutunda obw'omutindo gw'omutunzi (obufunibwa nga osabye) okuggyako nga bakkiriziganyizza mu buwandiike era nga kussiddwaako omukono ku lw'omutunzi. Wadde ng’amawulire agali wano gaweereddwa mu mutima mulungi, OMUTUNDI TAKOZESA WARANTI, EY’OKULAGULA OBA ETEGEEZEBWA, NGA MULI OKUTUNDA N’OBUTATyoboola BY’OBUTUNDU BY’OBUTUNDU, WAADDE TAKWATA BUVUNAANYIZIBWA Byonna, OBUTUNDU OBA OBUTITEEREVU, KU BY’OKUTUNDA KU NKOZESA, OBUVUNANYIZIBWA OBA OKUSAANIRA OKUKOLA OBA EKIGENDERERWA KYA BINTU BINO MU KUKOZESA KWONNA. Buli kasitoma alina okuzuula oba ebikozesebwa omutunzi bisaanira okukozesebwa kasitoma mu ngeri ey’enjawulo ng’ayita mu kugezesa n’okwekenneenya okutuufu. Tewali kiwandiiko kya mutunzi ekikwata ku nkozesa esoboka ey’ekintu kyonna, empeereza oba dizayini kigendereddwa, oba kisaana kutambulizibwa, kuwa layisinsi yonna wansi wa patent yonna oba eddembe eddala ery’obuntu.