Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
tertium genus monomerorum et contentum: ENB, 4.5%
Ethylene content: 62%
viscositas Mooney: ML (1+4) 125°C 98
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obsitum
Tertium monomerorum genus et contentum: ENB, 9%
Ethylene content: 60%
Mooney viscositas: ML (1+4) 125°C 92
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
Monomatis tertii generis et contenti: ENB, 8.5%
Ethylene content: 60%
Mooney viscositas: ML (1+4) 125°C 84 ML (1+4) 150℃ 81
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
tertium genus monomerorum et contentum: ENB, 8.5%
Ethylene content: 60%
viscositas Mooney: ML (1+4) 125°C 109
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
tertium genus monomerorum et contentum: ENB, 5.7%
contentum Ethylene: 70%
contentum olei: L%
viscositas Mooney: ML (1+4) 125°C 53
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti