GA-8153P
Herchy
| Loaʻa: | |
|---|---|
| Nui: | |
ʻO GA-8153P kahi mea hana kiʻekiʻe kiʻekiʻe o ka seramika silicone rubber i hoʻolālā ʻia no nā noi koi. He kūpono ia no nā ʻoihana kahi e pono ai ka lōʻihi a me ke kū'ē i nā wela kiʻekiʻe. Hōʻike kēia ʻōpala silicone i nā waiwai mechanical maikaʻi loa a kūpono hoʻi no ka hana ʻana i nā mea e pono ai ke kūpaʻa lōʻihi ma lalo o ke kaumaha.
Loaʻa ka huahana i ke kala keʻokeʻo, hāʻawi i kahi hiʻohiʻona maʻemaʻe a ʻoihana. ʻO kona ikaika tensile maikaʻi e hōʻoiaʻiʻo i ke kūpaʻa kū'ē i ke kaumaha kino. He kūpono ia no nā noi kahi e pono ai ka maʻalahi a me ka ikaika. Me ka Shore A paʻakikī o 55, hāʻawi ʻo GA-8153P i kahi hui kaulike o ka maʻalahi a me ka lōʻihi.
Me ka ikaika dielectric kiʻekiʻe o 26 kV / m, ʻo GA-8153P ka mea kūpono no ka insulation uila i nā huahana ʻoihana like ʻole. Hāʻawi ka mea i kahi mea hoʻohaʻahaʻa haʻahaʻa a me ka resistivity leo kiʻekiʻe, e kūpono ana ia no nā noi e koi ana i ka emi o ka ikehu a me ka conductivity uila.
ʻO ka ikaika o ka waimaka maikaʻi a me nā waiwai elongation e hōʻoia i ka hoʻomau ʻana o ka mea ma hope o ka hoʻohana nui ʻana. Hoʻohana nui ʻia ia no nā sila, gaskets, a me nā ʻāpana ʻoihana ʻē aʻe e koi ana i nā mea hana kiʻekiʻe.
Hoʻomaopopo pū ʻia ʻo GA-8153P no ka haʻahaʻa haʻahaʻa o ka uahi i ka wā o ka puhi ʻana. He mea koʻikoʻi kēia hiʻohiʻona i nā noi kahi e hopohopo ai ka palekana ahi. Me kona kūpaʻa kiʻekiʻe i ka ʻaʻahu a me nā waiwai wela maikaʻi loa, hilinaʻi kēia silicone rubber i nā wahi hana paʻakikī.
Ho'āʻo: ʻo ka lakio A/B o ka ʻōnaehana hoʻōla platinum he 1:1, 130°C x 5min x 15MPa.
| Nā palena huahana | ||
| Huahana | GA-8153P |
GA-8173P |
| Ka nana aku | Keʻokeʻo |
|
| Williamplasticity |
220 |
280 |
| Paʻakikī (ShoreA) |
55 |
70 |
| Māmā (g/cm3) | 1.38 |
1.47 |
| Ka ikaika uʻi (MPa) |
7 |
7.5 |
| Elongation(%) | 300 |
270 |
| Kaha waimaka (kN/m) | 18 |
22 |
| Kū'ē Volume (Ω.cm) | 1×1015 | 1×1015 |
| Ka ikaika dielectric (kV/m) | 26 |
26 |
| Dielectric mau ma 100 HZ | 3.33 |
|
| Ka helu hoʻopau ma 100 HZ |
0.01238 |
|
| Uhi Uhi ('ā) |
22.35 |
18.66 |
| ʻAʻohe ʻāʻī |
45.10 |
40.17 |

Hoʻolālā ʻia ʻo GA-8153P Ceramic Silicone Rubber (HCR) no nā noi hana kiʻekiʻe, e hāʻawi ana i ka lōʻihi a me ka versatility. He mea maikaʻi loa kēia kāpili silicone holomua no nā ʻoihana e koi ana i nā mea paʻa a hilinaʻi hoʻi, e like me ka ʻoihana kaʻa, uila, a me ke ahi. Aia ma lalo nā hiʻohiʻona nui e hoʻokaʻawale iā GA-8153P:
Hāʻawi ʻo GA-8153P i ka ikaika tensile maikaʻi, e pale aku i ke kaumaha kino a me ka ʻaʻahu. He mea kūpono kēia silicone rubber kiʻekiʻe no nā noi i nā ʻāpana kaʻa, nā sila, a me nā gaskets, e hōʻoia ana i ka hana lōʻihi a me ka hilinaʻi.
ʻO kekahi o nā pōmaikaʻi koʻikoʻi o GA-8153P ʻo ia ka haʻahaʻa haʻahaʻa o ka uahi ke ʻike ʻia i ke ahi. He mea kūpono loa ia no nā noi kahi i ʻoi aku ka nui o ka palekana ahi, e like me nā kaula pale ahi, nā ʻāpana uila, a me nā ʻāpana kaʻa.
Hāʻawi ʻo GA-8153P i kahi ʻano like ʻole o ka seramika e hoʻonui ai i kona kūpaʻa wela. He mea kūpono kēia no ka hoʻohana ʻana i nā wahi me nā wela kiʻekiʻe, e like me nā ʻoihana kaʻa, ʻoihana, a me nā ʻoihana uila. ʻO kona kūpaʻa wela maikaʻi e hōʻoia i ka hana hilinaʻi i nā kūlana koi.
Me ka ikaika dielectric o 26 kV/m, hāʻawi ʻo GA-8153P i ka insulation uila koʻikoʻi. ʻO kēia ke koho maikaʻi loa no nā noi i ka uila, ka insulation uila, a me nā ʻāpana uila automotive, kahi koʻikoʻi ka ikaika dielectric kiʻekiʻe no ka palekana a me ka hana.
ʻO ka ikaika waimaka maikaʻi o GA-8153P e hōʻoia i ka paʻa mau ʻana ma lalo o ke koʻikoʻi mechanical mau. He mea maikaʻi loa kēia no nā noi e koi ana i nā sila lōʻihi, nā gaskets, a me nā ʻāpana e hoʻomanawanui i ka neʻe pinepine a i ʻole nā kūlana paʻakikī.
ʻO GA-8153P ka lapalapa ahi, e lilo ia i koho palekana no ka hoʻohana ʻana i nā noi koʻikoʻi ahi. Inā ma ka ʻoihana kaʻa, aerospace, a i ʻole nā ʻoihana uila, kōkua kēia silicone rubber e hōʻoia i ka hoʻokō ʻana i nā kūlana palekana ahi, e hāʻawi ana i ka maluhia o ka noʻonoʻo no nā mea hana.
Hōʻike kēia mea i ka elongation kupaianaha (a hiki i 300%), e hōʻoiaʻiʻo i ka maʻalahi i nā noi kahi e koi ʻia ai ke kikoo a me ke kulou. ʻO ka maʻalahi ka mea kūpono no ka hana ʻana i nā sila a me nā gaskets, ʻoi aku hoʻi i nā wahi i pili i ka neʻe ʻana a i ʻole deformation.
Hoʻopili piha ʻo GA-8153P i nā kūlana kaiapuni e like me RoHS a me REACH. Mālama kēia i ka hoʻokō ʻana i nā koi hoʻoponopono no nā ʻoihana e pili ana i ka hoʻomau a me ka palekana, e kūpono ana i nā noi ikehu ʻōmaʻomaʻo, me nā ʻāpana automotive no nā kaʻa uila.
Hana kēia mau hiʻohiʻona i ka GA-8153P Ceramic Silicone Rubber i mea koho maikaʻi loa no ka nui o nā noi, me nā ʻāpana kaʻa uila ʻōmaʻomaʻo, nā kaula pale ahi, a me nā ʻāpana insulation uila. Ma ka hāʻawi ʻana i ka ikaika, palekana, a me ka maʻalahi, hāʻawi ia i ka hana ʻoi aku ka maikaʻi no nā ʻoihana e koi ana i nā mea kiʻekiʻe, nā mea paʻa. Inā makemake ʻoe i nā hoʻonā maʻamau no nā noi hana kiʻekiʻe a i ʻole e ʻimi ana i nā mea hilinaʻi no kāu mau pono hana, hāʻawi ʻo GA-8153P i ka maikaʻi a me ka hilinaʻi āu e hilinaʻi ai.
Q1: He aha nā noi nui o GA-8153P Ceramic Silicone Rubber?
A1: Hoʻohana nui ʻia ʻo GA-8153P i nā kaʻa kaʻa, nā uwea pale ahi, a me ka insulation uila.
Q2: Hiki iā GA-8153P ke kū i nā kaiapuni wela kiʻekiʻe?
A2: ʻAe, ua hoʻolālā ʻia ʻo GA-8153P no nā noi wela kiʻekiʻe a hāʻawi i ka pale wela maikaʻi loa.
Q3: Hāʻawi anei ʻo GA-8153P i ka hoʻokaʻawale uila no nā mea koʻikoʻi?
A3: ʻOiaʻiʻo, hāʻawi ia i nā waiwai insulation uila no nā noi like ʻole.
Q4: Hiki iaʻu ke kiʻi i ka GA-8153P Ceramic Silicone Rubber no kaʻu mau pono kikoʻī?
A4: ʻAe, hāʻawi mākou i nā hana maʻamau o GA-8153P e kūpono i kāu mau koi papahana.
Q5: Ua kūpono anei ʻo GA-8153P Ceramic Silicone Rubber me nā kūlana honua?
A5: ʻAe, hoʻokō ia i nā kūlana RoHS, REACH, a me LFGB, e hōʻoiaʻiʻo ana i ka hoʻohana palekana i nā ʻoihana like ʻole.
Q6: Pehea ka pale ahi o GA-8153P Silicone Rubber i hoʻohālikelike ʻia me nā huahana ʻē aʻe?
A6: Loaʻa i ka GA-8153P ke kūpaʻa ahi ʻoi aku ka maikaʻi no nā kaula ahi a me nā mea ʻāpana.
Q7: Ua kūpono ʻo GA-8153P no ka hoʻohana ʻana i nā gaskets a me nā sila?
A7: ʻAe, ʻo kona ikaika haʻalulu kiʻekiʻe a me ka maʻalahi e lilo ia i koho kūpono no nā gaskets a me nā sila.
Q8: Hiki iā GA-8153P ke hoʻohana i nā noi ikehu ʻōmaʻomaʻo, e like me nā kaʻa uila?
A8: ʻAe, ʻo GA-8153P kahi mea hilinaʻi no ka hana ʻana i nā ʻāpana i hoʻohana ʻia i nā kaʻa uila a me nā ʻōnaehana ikehu ʻōmaʻomaʻo.