Akwai nau'ikan roba da yawa a kasuwa, kamar roba na halitta, roba styrene-butadiene, butyl roba, roba nitrile, butadiene roba da roba sake yin fa'ida da sauransu. Kwanaki wani abokin ciniki ya zo ya tambayi dalilin da ya sa ake samar da kayan roba tare da launin shudi, wanda ke faruwa ta hanyar kuskuren zabi na roba ko tsarin da bai dace ba, injiniyoyinmu sun kasance don gabatar da abokan ciniki, janar na fesa blue yana faruwa ne saboda yawan acid, akwai lokuta da yawa.
1, plasticizer: plasticizer da aka kara a cikin samar da sake yin fa'ida kayayyakin roba an oxidized kafin hadawa, don haka a cikin vulcanized roba zai fesa blue; babban man kamshi mai laushi na hydrocarbon (kamar mai laushi na roba, da sauransu) an ƙara da yawa kuma mai sauƙin sa kayan roba suna fesa shuɗi.
2, Carbon baki: a cikin samar da carbon baƙar fata carbon baki a cikin manyan kwayoyin halitta na aromatic hydrocarbons ba a cika kone, sayan irin wannan carbon baki kara da roba roba kayayyakin zai zama da sauki fesa blue.
3, antioxidant: a cikin samar da kayan roba don ƙarawa da amfani da maganin antioxidant daidai gwargwado da launi na kayan roba, antioxidant ƙara launi da yawa da duhu zai haifar da kayan roba don fesa shuɗi, don haka adadin antioxidant da ya dace.
4, zafin vulcanization: saboda samfuran roba don ƙara kayan ƙara shuɗi mai sauƙi, ban da yanayin haɗuwa ya yi yawa, mai sauƙin sa samfuran vulcanized su fesa shuɗi.
5, roba hadawa m: a Bugu da kari na karin kayan hadawa saboda m hadawa na roba a hade tare da maida hankali na wani karin kayan aiki da yawa zai sa saman kayayyakin roba fesa blue.
Guji samfuran roba suna fesa bakan gizo: dabarar carbon baki don zama mai ma'ana da; vulcanization tsarin ya zama dan kadan wuce kima, kokarin ƙara m maiko, guduro, stearic acid, da dai sauransu.