GA-9440 Silicone Rubber for Cable Accessories (platinum) (HCR)

Product description: platinum curing high voltageresistant silicone rubber. 
Key application: cold shrinkable cable sleeve, 4Gcommunication. 
Key features: extrusion molding, high tensile, highelongation, high tea「strength,small deformation, passthe authentication of RoHS and REACH
 
We are a reliable manufacturer of high-performance silicone rubber for cable accessories. Our GA-9440 Silicone Rubber for Cable Accessories (Platinum) (HCR) is engineered to provide excellent durability and flexibility for various cable applications. We specialize in producing high-quality silicone rubber products that meet the stringent requirements of the cable industry, offering a variety of sizes and specifications.
  • GA-9440

  • Herchy

Availability:
Quantity:

Introduction of Our GA-9440 Silicone Rubber for Cable Accessories (Platinum) (HCR) 


GA-9440 Silicone Rubber for Cable Accessories (Platinum) (HCR) is a high-performance material designed for demanding applications. This platinum-cured silicone rubber provides outstanding durability and resistance to high pressures, making it ideal for various cable applications. It offers excellent electrical insulation and superior flexibility, ensuring long-lasting performance even in extreme conditions.


This silicone rubber has a translucent appearance and is suitable for both indoor and outdoor applications. The material is engineered to maintain high performance under high temperatures and pressure, while its dielectric strength and resistance to electrical tracking provide added safety.


The GA-9440 product is available in multiple hardness and tensile strength options, making it highly customizable to meet your specific requirements. Whether you're in the automotive, electronics, or industrial sector, this silicone rubber will ensure that your cable accessories are of the highest quality.


Test: platinum curing, A:0.5%; B:0.7%; first curing·130°C x 10minutes, post curing: 200°C x 4H


Product parameters
Product GA-9442
Appearance Translucent
Williamplasticity
160
Hardness (ShoreA)
43
Density(g/cm3) 1.135
Tensile strength (MPa)

10.0
Elongation(%) 900
Tear strength (kN/m) 45
Dielectric constant at 100HZ
3.03
Dissipation factor at 100HZ
0.0029
Tracking resistance --
Dielectric Strength (kV/mm) 23
Volume Resistivity (Ω·cm) 1.0*1016

silicone rubber

GA-9440 Silicone Rubber for Cable Accessories (Platinum) (HCR) Features


Excellent Mechanical Properties

GA-9440 silicone rubber provides high tensile strength and elongation, offering enhanced performance for cable accessories. It is engineered to withstand high stress and pressure while maintaining its shape, making it ideal for cable insulation and cable accessories. This high-performance silicone rubber is trusted by numerous global companies for its reliability and versatility.


Wide Range of Applications

This platinum-cured silicone rubber is commonly used in cold shrink cable joints and 4G communication cables. Its flexibility and high electrical insulation properties make it perfect for use in telecommunications and electrical cable accessories. We supply GA-9440 to various industries, including automotive, electronics, and telecommunications, ensuring high-quality solutions for their specific needs.


High-Temperature Stability

GA-9440 silicone rubber performs exceptionally well in high-temperature environments, maintaining stability and integrity even under extreme conditions. This feature is especially beneficial for high-performance cables and electrical insulation materials. With its excellent thermal stability, our product is designed to meet the demanding requirements of modern industries.


Compliance with Global Standards

Our silicone rubber complies with international standards such as RoHS and REACH certifications. It meets environmental and safety regulations, ensuring the material is safe for use in industries like telecommunications, automotive, and electronics. We prioritize quality and safety to deliver products that align with global regulatory standards, offering peace of mind to our customers.


Customizable for Various Uses

We offer custom silicone rubber solutions, tailored to meet the specific needs of different applications, whether for cable accessories or electrical insulation. Our GA-9440 product can be adjusted for various hardness, tensile strength, and elongation requirements. With over 10 years of experience in rubber solutions, our team ensures the perfect fit for your technical specifications.


Enhanced Electrical Insulation

GA-9440 silicone rubber excels at providing high electrical insulation. This makes it an excellent choice for use in power cables, electrical systems, and other applications requiring superior insulation properties and safety standards. Our extensive product range supports the creation of high-quality, reliable electrical components for global markets.


Resistance to Aging and Ozone

The rubber’s resistance to ozone and weathering makes it an ideal material for outdoor cable applications and telecom cable systems. It maintains its integrity and function over time, even in challenging environmental conditions. With our focus on providing long-lasting solutions, GA-9440 offers reliability and performance that endures.


Low Shrinkage

GA-9440 has low shrinkage, which helps to maintain the performance of cable accessories and silicone rubber components over time. This property is particularly important in dynamic environments where minimal deformation is required. Our team at Herchy ensures that every batch of GA-9440 is optimized for performance and durability.


Frequently Asked Questions and Answers


Q1: What are the key applications of GA-9440 silicone rubber for cable accessories?
A1: GA-9440 is ideal for cable insulation, telecommunications, cold shrink cable joints, and high-performance electrical components.


Q2: Can GA-9440 silicone rubber be customized for specific cable accessory needs?
A2: Yes, we offer customizable solutions to meet your technical specifications, including hardness and tensile strength.


Q3: How does GA-9440 silicone rubber perform under high-temperature conditions?
A3: GA-9440 maintains stability and performance in extreme temperatures, making it suitable for high-temperature cable applications.


Q4: Is GA-9440 silicone rubber compliant with international safety standards?
A4: Yes, it meets RoHS, REACH, and other global safety standards, ensuring safe and reliable use in various industries.


Q5: What industries use GA-9440 silicone rubber for cable accessories?
A5: GA-9440 is widely used in telecommunications, automotive, electrical systems, and high-performance cable manufacturing.


Q6: Does GA-9440 silicone rubber offer excellent electrical insulation properties?
A6: Yes, it provides high dielectric strength, making it perfect for electrical cable insulation and power systems.


Q7: Can GA-9440 silicone rubber resist aging and ozone damage?
A7: Yes, it offers excellent resistance to aging, ozone, and weathering, ensuring long-lasting durability in outdoor applications.


Q8: How can I request a sample or order GA-9440 silicone rubber for my project?
A8: Simply contact us for a custom quote or sample to test GA-9440 for your cable accessory applications.

Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.