e Zamakampani a Rubber ndi Chiyani?
Maonekedwe ndi mawonekedwe: zoyera (zowonekera kapena zowonekera) zotsekera
Mtundu wachitatu wa monomer ndi zomwe zili: ENB, 1.9%
Ethylene zili: 57.8%
Mooney viscosity: ML (1+4) 125°C 44
Kukula: 25kg/block
MOQ: 25kg
Kupaka: bokosi