Ŋusẽ Kɔkɔe Dzoxɔxɔ Tsitretsitsi Hose Ethylene Propylene Rubber-EPR
Dzedzeme kple nɔnɔme: ɣi (siwo me kɔ alo esiwo me kɔ) granules
Ƒomevi kple nusiwo le eme le monomer etɔ̃lia me: ENB,4%
Ethylene ƒe agbɔsɔsɔ: 68.5%
Menni ƒe ʋeʋẽ: ML(1+4)125°C 45
Agbɔsɔsɔ kple eƒe nɔnɔme: 25kg/kotoku
Nudɔdɔ ƒe agbɔsɔsɔ suetɔ: 25kg
Nubabla: Aɖaka me