Ra'ayoyi: 0     Mawallafi: Lokacin Buga Editan Yanar Gizo: 2023-08-13 Asalin: Shafin

Tambaya

Rubber yana da kyawawan kaddarorin damping, ana amfani da su sosai wajen kera raguwar girgiza girgiza ko keɓe samfuran damping na girgiza. Tare da saurin haɓakar kimiyya da fasaha na zamani da ci gaban zamantakewa, da kuma hankalin mutane game da haɗarin girgizar ƙasa, samfuran girgizar roba suna ƙara faɗuwar amfani, buƙatun aikin sa suna ƙara girma.


Compressor vibration damping kushin da aka sanya a kasa na kwampreso, goyon bayan da kwampreso ta key sassa, general bukatun ga sabis rayuwa na game da shekaru 10 da kuma a cikin rayuwar da bukatun na tsawo na kushin, taurin, size canji ne karami, saboda da kwampreso rataye a waje, don haka roba kushin na roba bukatun ne high, da kuma bukatar da taurin da zazzabi canje-canje ne low zafin jiki na kushin.


Ayyukan matashin roba kai tsaye yana rinjayar tasirin damping vibration damping da amo, ta yadda, jijjiga damping matashin roba babu makawa iska kwandishan kwampreso 'kore da muhalli abokantaka wani muhimmin bangare na '. Bisa ga aikin da roba buga kushin ne da yin amfani da roba ta high elasticity da kuma high danko saita a daya, yadda ya kamata maida inji makamashi cikin motsi makamashi na kwayoyin motsi, tare da roba kwayoyin nakasu da kuma maido da inji makamashi amfani, kuma zai rage vibration da amo. Vibration-damping roba matashin aiki na dogon lokaci a cikin waje, ana buƙatar samun kwanciyar hankali mai girma, juriya na yanayi da taurin tare da canjin zafin jiki ba a bayyane halaye ba.


Chloroprene roba (CR) yana da kyakkyawan juriya na yanayi, da kyakkyawan aiki da maras tsada. Yawancin ƙasashen da suka ci gaba suna ba da fifiko ga amfani da shi azaman kwampreso vibration damping matashin matashin matashin kai, kamar ƙayyadaddun kushin jijiya na masana'antar kwampreta ta Japan (daidai da ƙa'idodin fasaha na cikin gida), wanda ke ba da amfani da robar chloroprene. Makasudin wannan bincike da haɓakawa shine don zaɓar ƙimar da ta dace na roba neoprene da wakili mai laushi, da bincika kayan aikin injin sa, kayan tsufa da kwanciyar hankali.


1. Sakamakon nau'ikan nau'ikan CR daban-daban akan aikin kayan aikin roba


Shock absorbing gammaye a kan tsufa juriya da ƙananan zafin jiki na buƙatun, kuma dole ne la'akari da farashin, zaɓi na DCR2131, CR3221 da CR2321 nau'ikan maki uku. Hakanan tare da roba, CR2321 rubber a karkashin al'ada na jiki da na inji sun fi kyau, amma juriya na tsufa ya ɗan yi muni, bai dace da ƙayyadaddun fasaha ba; Ayyukan roba na DCR2131 don isa ga alamun da ake buƙata, amma tsarin haɗawa ba shi da kyau, roba yana da taushi sosai, bakin ciki ta wurin da wahala, mai sauƙin kai ga yanayin haɗuwa mara daidaituwa. Saboda ƙananan danko na hadawar roba Mooney, roba a cikin vulcanization yana da wuya a cire iska, yana haifar da kumfa saman samfurin, yana shafar ƙimar cancantar samfurin; da kuma CR3221 masu nuna alamun aikin roba don saduwa da buƙatun ƙayyadaddun fasaha.


2. Tasirin masu laushi daban-daban akan aikin kayan aikin roba


Saboda da kwampreso a kan vibration damping matashi taurin musamman, zai zama ƙananan tauri (Shore A40 digiri), don haka da bukatun na softener ne mafi wuya da adadin ne kuma in mun gwada da girma, tare da tsarin yana da babban tasiri a kan yi na roba da kuma samfurin. A lokaci guda don yin la'akari da farashi da tushen, zaɓi wakilin DOTP, mai mai aromatics, mai laushi mai waken soya mai epoxy a cikin CR3221 kayan roba don gwaje-gwajen kwatankwacin, saboda amfani da aromatics mai roba kayan taurin abu mai ƙarfi, a cikin dabarar mai na aromatics da aka yi amfani da su a cikin 39, sakamakon amfani da DOTP ko aromatics na man fetur na iya saduwa da buƙatun roba na fasaha na iya haɗuwa da buƙatun mai. na DOTP roba abu ba sauki don tsayawa rollers, sauki hadawa, da kuma sakamakon da yin amfani da DOTP ko aromatics man curing aikin roba iya saduwa da bukatun na fasaha bayani dalla-dalla. Yana da sauƙi don haɗuwa, kuma la'akari da injin kwampreso zuwa takaddun shaida na RosH 'Ƙuntatawar amfani da wasu abubuwa masu haɗari a cikin umarnin kayan lantarki da lantarki' da kuma takardar shaidar REACH ' akan rajista, kimantawa, izini da ƙuntatawa na tsarin sinadarai ' bukatun muhalli, don haka DOTP shine mafi kyawun zaɓi!


SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.